# US 2020/0006653 A1 · Resistive random-access memory (rram) cell with recessed bottom electrode sidewalls

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0006653 A1
- Document ID: US20200006653A1
- Status: Published application
- Kind: A1
- Application number: 16/559,994
- Filed: 2019-09-04
- Published: 2020-01-02
- Earliest claimed: 2017-08-02
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Yuan-Tai Tseng; Shih-Chang Liu
- Web page: https://patentgrep.com/patent/US20200006653A1

## CPC

- H10N 70/841: {Electrodes}
- H10B 63/00: Resistance change memory devices, e.g. resistive RAM [ReRAM] devices
- H10N 70/011: {Manufacture or treatment of multistable switching devices}
- H10N 70/021: {Formation of switching materials, e.g. deposition of layers}
- H10N 70/063: {by etching of pre-deposited switching material layers, e.g. lithography}
- H10N 70/066: {by filling of openings, e.g. damascene method}
- H10N 70/068: {by processes specially adapted for achieving sub-lithographic dimensions, e.g. using spacers}
- H10N 70/24: {based on migration or redistribution of ionic species, e.g. anions, vacancies}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- H10N 70/8836: {Complex metal oxides, e.g. perovskites, spinels}
- H10B 63/30: {comprising selection components having three or more electrodes, e.g. transistors}
- H10N 70/883: {Oxides or nitrides}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

Various embodiments of the present application are directed towards an integrated circuit comprising a resistive random-access memory (RRAM) cell with recessed bottom electrode sidewalls to mitigate the effect of sidewall plasma damage. In some embodiments, the RRAM cell includes a lower electrode, a data storage element, and an upper electrode. The lower electrode includes a pair of recessed bottom electrode sidewalls respectively on opposite sides of the lower electrode. The data storage element overlies the lower electrode and includes a pair of storage sidewalls. The storage sidewalls are respectively on the opposite sides of the lower electrode, and the recessed bottom electrode sidewalls are laterally spaced from and laterally between the storage sidewalls. The upper electrode overlies the data storage element.

## Claims

### Claim 1

A method for forming an integrated circuit comprising a memory cell, the method comprising:
forming a lower conductive layer on a substrate;
forming a data storage layer overlying the lower conductive layer;
forming an upper conductive layer overlying the data storage layer;
patterning the upper conductive layer, the data storage layer, and the lower conductive layer to respectively form an upper electrode, a data storage element, and a lower electrode stacked on the substrate, wherein the patterning forms sidewall defects in storage sidewalls of the data storage element; and
performing an etch into the lower electrode to laterally recess electrode sidewalls of the lower electrode respectively relative to neighboring ones of the storage sidewalls.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the patterning comprises:
performing a second etch into the data storage layer and the lower conductive layer to respectively form the data storage element and the lower electrode, wherein the storage sidewalls are respectively aligned with the electrode sidewalls upon completion of the second etch.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the second etch is performed by a plasma etch and forms the sidewall defects in the storage sidewalls, and wherein the etch is performed by a wet etch.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the patterning further comprises:
forming a hard mask overlying a memory region of the upper conductive layer;
performing a third etch into the upper conductive layer with the hard mask in place to form the upper electrode, wherein the third etch stops on the data storage layer; and
forming spacer segments on sidewalls of the upper electrode, wherein the second etch is performed with the hard mask and the spacer segments in place.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the lower electrode comprises titanium nitride, and wherein the etch comprises applying a hydrogen peroxide solution to the lower electrode to laterally recess the electrode sidewalls.

### Claim 6 (depends on 1)

The method according to claim 1, further comprising performing a second etch into the substrate to form a via opening, wherein the forming of the lower conductive layer comprises:
depositing the lower conductive layer covering the substrate and filling the via opening; and
performing a planarization into the lower conductive layer to flatten a top surface of the lower conductive layer, wherein the flattened top surface of the lower conductive layer is spaced over a top surface of the substrate.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the lower conductive layer comprises a diffusion barrier layer and a metal layer overlying the diffusion barrier layer.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising:
performing a second etch into the substrate to form a via opening;
depositing a conductive via layer covering the substrate and filling the via opening; and
performing a planarization into a top surface of the conductive via layer until a top surface of the substrate is reached, thereby forming a via in the via opening from the conductive via layer, wherein the lower conductive layer is formed on the via.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the conductive via layer comprises a diffusion barrier layer and a metal layer overlying the diffusion barrier layer.

### Claim 10

A method comprising:
patterning a first insulating layer to form a first opening overlying and exposing a first wire that underlies the first insulating layer;
forming a first via filling the first opening;
forming a memory cell on the first via, wherein the memory cell comprises a lower electrode on the first via, a high k dielectric element overlying the lower electrode, and an upper electrode overlying the high k dielectric element, and wherein the high k dielectric element and the lower electrode respectively have a dielectric sidewall and an electrode sidewall that are formed even with each other; and
recessing the electrode sidewall laterally relative to the dielectric sidewall after the forming of the memory cell.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the forming of the memory cell comprises:
depositing a high k dielectric layer; and
plasma etching the high k dielectric layer to form the high k dielectric element, wherein the plasma etching forms defects in the high k dielectric element that extend laterally into the high k dielectric element from the dielectric sidewall by a distance, and wherein the recessing persists until the electrode sidewall is offset from the dielectric sidewall by the distance.

### Claim 12 (depends on 10)

The method according to claim 10, wherein the recessing comprises wet etching the lower electrode.

### Claim 13 (depends on 10)

The method according to claim 10, wherein the lower electrode and the via are formed from a single deposition.

### Claim 14 (depends on 10)

The method according to claim 10, further comprising:
depositing a second insulating layer covering the memory cell and the first insulating layer, and further contacting the electrode sidewall and the dielectric sidewall, wherein the high k dielectric element overhangs and contacts the second insulating layer at a bottom surface of the high k dielectric element.

### Claim 15 (depends on 14)

The method according to claim 14, further comprising:
depositing an interlayer dielectric (ILD) layer covering the second insulating layer and the memory cell, and further having a bottom surface that is recessed relative to a bottom surface of the upper electrode;
patterning the ILD layer and the second insulating layer to form a second opening overlying and exposing the memory cell;
forming a second via in the second opening; and
forming a second wire on the second via and the ILD layer.

### Claim 16

A method comprising:
forming a first via extending through a first insulating layer from a top of the first insulating layer to a first wire underlying the first insulating layer;
forming a lower conductive layer overlying the first via and the first insulating layer;
depositing a metal oxide layer on the lower conductive layer;
forming an upper electrode and a hard mask stacked on the metal oxide layer and overlying the first via;
forming a sidewall spacer on an upper electrode sidewall of the upper electrode and a hard mask sidewall of the hard mask;
plasma etching the metal oxide layer and the lower conductive layer to respectively form a metal oxide element and a lower electrode, wherein the plasma etching stops on the first insulating layer and uses the hard mask and the sidewall spacer as a mask; and
wet etching the lower electrode to offset a lower electrode sidewall of the lower electrode from a metal oxide sidewall of the metal oxide element.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the plasma etching forms a defect region in the lower electrode, wherein the defect region is along the lower electrode sidewall and adjoins a central region of the lower electrode having a lower concentration of defects than the defect region, and wherein the wet etching persists until the lower electrode sidewall is at a boundary between the central and defect regions.

### Claim 18 (depends on 16)

The method according to claim 16, wherein the plasma etching forms a defect region in the lower electrode, and wherein the method further comprises:
applying a forming voltage from the upper electrode to the lower electrode after the wet etching, wherein the applying of the forming voltage forms a plurality of conductive filaments that is in the metal oxide layer and that is completely spaced laterally from the defect region.

### Claim 19 (depends on 16)

The method according to claim 16, wherein the lower conductive layer comprises the first via, and wherein the lower conductive layer and the first via are simultaneously formed.

### Claim 20 (depends on 16)

The method according to claim 16, further comprising:
depositing a second insulating layer covering the first insulating layer, the hard mask, and the sidewall spacer, wherein the second insulating layer has an inner surface facing the metal oxide element and further has an outer surface facing away from the metal oxide element, and wherein the inner and outer surfaces wrap around a bottom corner of the metal oxide element and conform to the lower electrode sidewall and the metal oxide sidewall; and
depositing an interlayer dielectric (ILD) layer covering the second insulating layer and having a bottom surface that is recessed relative to a bottom surface of the upper electrode.