# US 2020/0006581 A1 · Methods and apparatus for producing copper-indium-gallium-selenium (cigs) film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0006581 A1
- Document ID: US20200006581A1
- Status: Published application
- Kind: A1
- Application number: 16/442,776
- Filed: 2019-06-17
- Published: 2020-01-02
- Earliest claimed: 2018-06-28
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: PHILIP HSIN-HUA LI; SESHADRI RAMASWAMI
- Web page: https://patentgrep.com/patent/US20200006581A1

## CPC

- H10F 39/021: {of image sensors having active layers comprising only Group III-V materials, e.g. GaAs, AlGaAs or InP}
- H10F 77/1265: {characterised by the dopants}
- H10F 39/184: {Infrared image sensors}
- H10F 71/128: {Annealing}
- H10F 77/126: {comprising only Group I-III-VI chalcopyrite materials, e.g. CuInSe2, CuGaSe2 or CuInGaSe2 [CIGS]}
- Y02E 10/541: CuInSe2 material PV cells
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Methods and apparatus form a photon absorber layer of a photodiode with characteristics conducive to applications such as, but not limited to, image sensors and the like. The absorber layer uses a copper-indium-gallium-selenium (CIGS) material with a gallium mole fraction of approximately 35% to approximately 70% to control the absorbed wavelengths while reducing dark current. Deposition temperatures of the absorber layer are controlled to less than approximately 400 degrees Celsius to produce sub-micron grain sizes. The absorber layer is doped with antimony at a temperature of less than approximately 400 degrees Celsius to increase the absorption.

## Claims

### Claim 1

A method of forming a film layer on a substrate, comprising:
depositing the film layer using a copper-indium-gallium-selenium (CIGS) material;
controlling a deposition temperature to produce sub-micron grain size in the film layer during deposition; and
doping the film layer with antimony to increase photon energy absorption of the film layer.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
depositing the film layer using a CIGS material with a gallium mole fraction of approximately 35% to approximately 70%.

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
depositing the film layer using a CIGS material with a gallium mole fraction of approximately 57%.

### Claim 4 (depends on 3)

The method of claim 3, further comprising:
controlling the deposition temperature to less than approximately 400 degrees Celsius to produce sub-micron grain size in the film layer during deposition.

### Claim 5 (depends on 4)

The method of claim 4, further comprising:
doping the film layer with antimony at a temperature of less than approximately 400 degrees Celsius.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
controlling the deposition temperature to less than approximately 400 degrees Celsius to produce sub-micron grain size in the film layer during deposition.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
doping the film layer to approximately 1.2 mol % to approximately 5 mol % antimony.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
doping the film layer with antimony at a temperature of less than approximately 400 degrees Celsius.

### Claim 9

A method of forming a film layer of a photodiode, comprising:
depositing the film layer using a copper-indium-gallium-selenium (CIGS) material with a gallium mole fraction of approximately 35% to approximately 70%;
controlling a deposition temperature to less than approximately 400 degrees Celsius to produce sub-micron grain size in the film layer during deposition; and
doping the film layer with antimony at a temperature of less than approximately 400 degrees Celsius.

### Claim 10 (depends on 9)

The method of claim 9, further comprising:
depositing the film layer using a CIGS material with a gallium mole fraction of approximately 57%.

### Claim 11 (depends on 9)

The method of claim 9, further comprising:
doping the film layer to approximately 1.2 mol % to approximately 5 mol % antimony.

### Claim 12

An apparatus for detecting images, comprising:
a photodiode with an absorber layer having a copper-indium-gallium-selenium (CIGS) material with a sub-micron grain size.

### Claim 13 (depends on 12)

The apparatus of claim 12, wherein the CIGS material has a gallium mole fraction of approximately 35% to approximately 70%.

### Claim 14 (depends on 12)

The apparatus of claim 12, wherein the CIGS material has a gallium mole fraction of approximately 57%.

### Claim 15 (depends on 14)

The apparatus of claim 14, wherein the CIGS material is doped with antimony.

### Claim 16 (depends on 15)

The apparatus of claim 15, wherein the CIGS material is doped with approximately 1.2 mol % to approximately 5 mol % antimony.

### Claim 17 (depends on 12)

The apparatus of claim 12, wherein the CIGS material is doped with antimony.

### Claim 18 (depends on 17)

The apparatus of claim 17, wherein the CIGS material is doped with approximately 1.2 mol % to approximately 5 mol % antimony.

### Claim 19 (depends on 12)

The apparatus of claim 12, wherein the absorber layer absorbs wavelengths less than or equal to approximately 940 nm and is transparent to wavelengths greater than approximately 940 nm.

### Claim 20 (depends on 12)

The apparatus of claim 12, wherein the absorber layer has a bandgap of approximately 1.31 eV.