# US 2020/0006074 A1 · Methods for fabricating and etching porous silicon carbide structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0006074 A1
- Document ID: US20200006074A1
- Status: Published application
- Kind: A1
- Application number: 16/434,049
- Filed: 2019-06-06
- Published: 2020-01-02
- Earliest claimed: 2016-12-16
- Assignees: Elwha LLC
- Applicants: Elwha LLC
- Inventors: Rachel Cannara; Emma Rae Mullen; Fred Sharifi
- Web page: https://patentgrep.com/patent/US20200006074A1

## CPC

- C25D 11/32: of semiconducting materials
- H10P 50/613: {of Group IV materials}
- C25F 3/12: of semiconducting materials
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C25F: PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR

## Abstract

The present disclosure relates to methods of fabricating a porous structure, such as a porous silicon carbide structure. The methods can include a step of providing a structure to be rendered porous, and a step of providing an etching solution. The methods can also include a step of electrochemically etching the structure to produce pores through at least a region of the structure, resulting in the formation of a porous structure. The morphology of the porous structure can be controlled by one or more parameters of the electrochemical etching process, such as the strength of the etching solution and/or the applied voltage.

## Claims

### Claim 1

A method of fabricating a porous silicon carbide structure having a selected morphology, comprising:
providing a silicon carbide structure;
providing an etching solution comprising a reducing agent and an oxidizing agent;
electrochemically etching the silicon carbide structure with the etching solution to produce pores through a region of the silicon carbide structure to form a porous silicon carbide structure, wherein electrochemically etching the silicon carbide structure comprises applying a voltage to a surface of the silicon carbide structure to produce a current density through the region of the silicon carbide structure; and
controlling an etch propagation rate of the etching solution through the region of the silicon carbide structure to achieve the selected morphology, wherein the selected morphology comprises a substantially uniform porous structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the silicon carbide structure comprises a 3C, 4H, or 6H polytype of silicon carbide.

### Claim 3 (depends on 1)

The method of claim 1, wherein the silicon carbide structure comprises a silicon carbide semiconductor.

### Claim 4 (depends on 1)

The method of claim 1, wherein the silicon carbide structure comprises a predefined electronic carrier concentration.

### Claim 5 (depends on 1)

The method of claim 1, wherein the silicon carbide structure comprises a predefined crystalline designation.

### Claim 6 (depends on 1)

The method of claim 1, wherein the oxidizing agent comprises water, an alcohol, hydrogen peroxide, or a mixture thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein the reducing agent comprises hydrofluoric acid.

### Claim 8 (depends on 7)

The method of claim 7, wherein the concentration of the hydrofluoric acid is from about 1% to about 50%, from about 1% to about 20%, from about 1% to about 15%, from about 1% to about 10%, from about 1% to about 5%, or from about 2% to about 5%, by volume.

### Claim 9 (depends on 7)

The method of claim 7, wherein the etch propagation rate is dependent upon the concentration of the hydrofluoric acid.

### Claim 10 (depends on 7)

The method of claim 7, wherein the concentration of hydrofluoric acid is inversely proportional to a porosity of the porous silicon carbide structure.

### Claim 11 (depends on 1)

The method of claim 1, wherein the etching solution further comprises a surfactant.

### Claim 12 (depends on 1)

The method of claim 1, wherein the voltage is from about 20 V to about 40 V, from about 20 V to about 30 V, or from about 20 V to about 26 V.

### Claim 13 (depends on 1)

The method of claim 1, wherein the current density is proportional to a removal rate of the material.

### Claim 14 (depends on 1)

The method of claim 1, wherein the current density decreases at a substantially constant rate during the electrochemical etching step.

### Claim 15 (depends on 1)

The method of claim 1, wherein the selected morphology comprises at least one of a selected average pore diameter, a selected pore wall thickness, or a selected porosity.

### Claim 16 (depends on 1)

The method of claim 1, wherein the selected morphology comprises an average pore wall thickness of between about 2 nm and about 200 nm.

### Claim 17 (depends on 1)

The method of claim 1, wherein the selected morphology comprises an average pore diameter of between about 0.1 μm and about 3 μm.

### Claim 18 (depends on 1)

The method of claim 1, wherein the selected morphology comprises an average pore diameter of between about 0.1 μm and about 3 μm, and an average pore wall thickness of between about 2 nm and about 200 nm.

### Claim 19 (depends on 1)

The method of claim 1, wherein the selected morphology comprises a porosity of from about 60% to about 96%.

### Claim 20 (depends on 1)

The method of claim 1, wherein the selected morphology comprises a substantially uniform material density.

### Claim 21 (depends on 1)

The method of claim 1, wherein controlling the etch propagation rate comprises:
selecting a concentration of reducing agent; and
selecting a voltage;
wherein the etch propagation rate is inversely proportional to a porosity of the morphology at the selected concentration and selected voltage.

### Claim 22 (depends on 21)

The method of claim 21, wherein the selected concentration is from about 1% to about 50%, from about 1% to about 20%, from about 1% to about 15%, from about 1% to about 10%, from about 1% to about 5%, or from about 2% to about 5%, by volume, and the selected voltage is from about 20 V to about 40 V, from about 20 V to about 30 V, or from about 20 V to about 26 V.

### Claim 23 (depends on 1)

The method of claim 1, wherein the silicon carbide structure is electrochemically etched beginning at an “Si” face.

### Claim 24 (depends on 1)

The method of claim 1, wherein the silicon carbide structure is electrochemically etched beginning at a “C” face.

### Claim 25

A method of fabricating a porous structure, comprising:
providing a starting structure to be rendered porous;
providing an etching solution comprising a selected reducing agent and an oxidizing agent;
electrochemically etching the starting structure with the etching solution to produce pores through a region of the starting structure to form a porous structure, wherein electrochemically etching the structure comprises applying a voltage to a surface of the structure to produce a current density through the region of the structure; and
controlling an etch propagation rate of the etching solution through the region of the structure to achieve a selected porosity, wherein the selected porosity is greater than 90%.

### Claim 26 (depends on 25)

The method of claim 25, wherein the structure comprises silicon carbide.

### Claim 27 (depends on 25)

The method of claim 25, wherein the reducing agent comprises hydrofluoric acid.

### Claim 28 (depends on 25)

The method of claim 25, wherein controlling the etch propagation rate comprises:
selecting a concentration of reducing agent; and
selecting a voltage;
wherein the etch propagation rate is inversely proportional to the porosity at the selected concentration and selected voltage.

### Claim 29 (depends on 28)

The method of claim 28, wherein the selected concentration is from about 1% to about 50%, from about 1% to about 20%, from about 1% to about 15%, from about 1% to about 10%, from about 1% to about 5%, or from about 2% to about 5%, and the selected voltage is from about 20 V to about 40 V, from about 20 V to about 30 V, or from about 20 V to about 26 V.

### Claim 30 (depends on 25)

The method of claim 25, wherein the structure is electrochemically etched beginning at an “Si” face.

### Claim 31 (depends on 25)

The method of claim 25, wherein the structure is electrochemically etched beginning at a “C” face.

### Claim 32

A method of fabricating a porous semiconductor structure via an electrochemical etch process, comprising:
providing a semiconductor structure;
providing an etching solution comprising a reducing agent and an oxidizing agent;
selecting a concentration of the reducing agent; and
electrochemically etching the semiconductor structure with the etching solution to produce pores through a region of the semiconductor structure to form a porous semiconductor structure, wherein electrochemically etching the semiconductor structure comprises selecting a voltage and applying the selected voltage to a surface of the semiconductor structure to produce a current density through the region of the semiconductor structure;
wherein the porous semiconductor structure comprises a selected porosity.

### Claim 33 (depends on 32)

The method of claim 32, wherein the semiconductor structure comprises silicon carbide.

### Claim 34 (depends on 32)

The method of claim 32, further comprising:
controlling an etch propagation rate of the etching solution through the region of the semiconductor structure to achieve the selected porosity, wherein the etch propagation rate is inversely proportional to the porosity at the selected concentration and selected voltage.

### Claim 35 (depends on 34)

The method of claim 34, wherein the selected concentration is from about 1% to about 50%, from about 1% to about 20%, from about 1% to about 15%, from about 1% to about 10%, from about 1% to about 5%, or from about 2% to about 5%, by volume, and the selected voltage is from about 20 V to about 40 V, from about 20 V to about 30 V, or from about 20 V to about 26 V.

### Claim 36 (depends on 32)

The method of claim 32, wherein an etch propagation rate is dependent upon the selected concentration.

### Claim 37 (depends on 32)

The method of claim 32, wherein the porous semiconductor structure comprises a selected average pore diameter.

### Claim 38 (depends on 32)

The method of claim 32, further comprising:
monitoring the current density during the electrochemical etching step.