# US 2020/0005996 A1 · Gradient nd-fe-b magnet and a method of production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0005996 A1
- Document ID: US20200005996A1
- Status: Published application
- Kind: A1
- Application number: 16/459,448
- Filed: 2019-07-01
- Published: 2020-01-02
- Earliest claimed: 2018-06-29
- Assignees: Yantai Shougang Magnetic Materials Inc.
- Applicants: Yantai Shougang Magnetic Materials, Inc.
- Inventors: Kunkun Yang; Zhongjie Peng; Chuanshen Wang
- Web page: https://patentgrep.com/patent/US20200005996A1

## CPC

- H01F 41/0293: {diffusion of rare earth elements, e.g. Tb, Dy or Ho, into permanent magnets}
- H01F 1/0555: {pressed, sintered or bonded together}
- H01F 1/0577: {sintered}
- H01F 7/0215: {Flexible forms, sheets}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A gradient Nd—Fe—B magnet includes an Nd—Fe—B magnet block extending along a magnetization direction and having a plurality of surfaces perpendicular to the magnetization direction. A first film, is disposed on one of the surfaces. A second film is disposed on another one of the surfaces, opposite of the one of the surfaces. The first film and the second film are diffused into the Nd—Fe—B magnet block dividing the Nd—Fe—B magnet block into an edge region, a transition region, and a central region along a plane perpendicular to the magnetization direction wherein the edge region has a coercivity that remains constant in a direction perpendicular to the magnetization direction, and the coercivity, along said magnetization direction, gradually decreases from the one of the surfaces and the another one of the surfaces towards a point located therebetween. A method of making the gradient Nd—Fe—B magnet is disclosed herein.

## Claims

### Claim 1

A gradient Nd—Fe—B magnet comprising:
an Nd—Fe—B magnet block extending along a magnetization direction and having a plurality of surfaces perpendicular to said magnetization direction;
a first film containing at least one heavy rare earth element, disposed on one of said surfaces, attached to said Nd—Fe—B magnet block and extending along a periphery of said one of said surfaces; and
a second film containing at least one heavy rare earth element, disposed on another one of said surfaces, opposite of said one of said surfaces, attached to said Nd—Fe—B magnet block and extending along a periphery of said another one of said surfaces; and
said first film and said second film being diffused into said Nd—Fe—B magnet block dividing said Nd—Fe—B magnet block into an edge region, a transition region, and a central region along a plane extending perpendicular to said magnetization direction;
wherein said edge region has a coercivity that remains constant in a direction perpendicular to said magnetization direction, and said coercivity of said edge region, along said magnetization direction, gradually decreases from said one of said surfaces and said another one of said surfaces towards a point located between said one of said surfaces and said another one of said surfaces.

### Claim 2 (depends on 1)

The gradient Nd—Fe—B magnet as set forth in claim 1 wherein said transition region has a coercivity that decreases toward said central portion in said direction perpendicular to said magnetization direction and said coercivity of said transition region, along said magnetization direction, gradually decreases from said one of said surfaces and said another one of said surfaces to said point between said one of said surfaces and said another one of said surfaces.

### Claim 3 (depends on 1)

The gradient Nd—Fe—B magnet as set forth in claim 1 wherein said center region has a coercivity that remains constant in said direction perpendicular to said magnetization direction and along said magnetization direction.

### Claim 4 (depends on 1)

The gradient Nd—Fe—B magnet as set forth in claim 1 wherein an average of said coercivity of said edge region is greater than an average of said coercivity of said transition region and said average of said coercivity of said transition region is greater than an average of said coercivity of said central region.

### Claim 5 (depends on 1)

The gradient Nd—Fe—B magnet as set forth in claim 1 wherein said Nd—Fe—B magnet block has a thickness of between 2-10 mm along said magnetization direction.

### Claim 6 (depends on 1)

The gradient Nd—Fe—B magnet as set forth in claim 1 wherein said Nd—Fe—B magnet block has a length and a width of at least 10 mm.

### Claim 7 (depends on 1)

The gradient Nd—Fe—B magnet as set forth in claim 1 wherein said at least one heavy rare earth element is selected from a group consisting of Tb, Dy, or an alloy containing Dy or Tb.

### Claim 8 (depends on 1)

The gradient Nd—Fe—B magnet as set forth in claim 1 wherein said first film and said second film are attached to said Nd—Fe—B magnet block by melting a powder containing said at least one heavy rare earth metal on said one and said another one of the surfaces and along said periphery using a laser.

### Claim 9 (depends on 8)

The gradient Nd—Fe—B magnet has set forth in claim 8 wherein said at least one heavy rare earth element is selected from a group consisting of Tb, Dy, or an alloy containing Dy or Tb and is present in said powder in an amount of 0.1 wt. % and 2 wt. %.

### Claim 10 (depends on 8)

The gradient Nd—Fe—B magnet a set forth in claim 8 wherein said powder has an average particle size of between 1 μm and 300 μm.

### Claim 11 (depends on 1)

A method of making the gradient Nd—Fe—B magnet of claim 1, said method including the steps of:
providing the Nd—Fe—B magnet block having a thickness of between 2-10 mm along the magnetization direction and having the surfaces perpendicular to the magnetization direction;
placing the Nd—Fe—B magnet block in a chamber containing an inert gas of argon with the magnetization direction of the Nd—Fe—B magnet block being arranged in a vertical direction;
depositing a powder, containing at least one heavy rare earth element, on the one of the surfaces;
forming the first film containing the at least one heavy rare earth element on the one of the surfaces and along the periphery of the one of the surfaces;
said step of forming the first film further including a step of melting the powder on the one of the surfaces and along the periphery using a laser to form the first film and adhering the first film to the periphery;
removing excess powder from the one of the surfaces;
rotating the Nd—Fe—B magnet block 180°;
depositing the powder, containing at least one heavy rare earth element, on the another one of the surfaces opposite of the one of the surfaces;
forming the second film containing the at least one heavy rare earth element on the another one of the surfaces and along the periphery of the another one of the surfaces;
said step of forming the second film further including a step of melting the powder on the another one of the surfaces and along the periphery using a laser to form the second film and adhering the second film to the periphery;
removing excess powder from the another one of the surfaces;
diffusing the first film and the second film into the Nd—Fe—B magnet block under a vacuum environment or an inert environment containing argon and at a predetermined temperature.

### Claim 12 (depends on 11)

The method as set forth in claim 11 wherein the Nd—Fe—B magnet block has a length and a width of at least 10 mm.

### Claim 13 (depends on 11)

The method as set forth in claim 11 wherein the powder has an average particle size of between 1 μm and 300 μm.

### Claim 14 (depends on 11)

The method as set forth in claim 11 wherein the at least one heavy rare earth element is selected from a group consisting of Tb, Dy, or an alloy containing Dy or Tb and the powder is present in an amount of 0.1 wt. % and 2 wt. % of the total mass of the Nd—Fe—B magnet block.

### Claim 15 (depends on 11)

The method as set forth in claim 11 wherein an area covered by the first film is 10% to 65% of an area covered by the powder on one of the surfaces of the Nd—Fe—B magnet block.

### Claim 16 (depends on 11)

The method as set forth in claim 11 wherein an area covered by the second film is 10% to 65% of an area covered by the powder on the another one of the surfaces of the Nd—Fe—B magnet block.

### Claim 17 (depends on 11)

The method set forth in claim 11 wherein said step of diffusing is further defined as heating the Nd—Fe—B magnet block including the first film and the second film at the predetermined temperature of between 850° C. and 950° C. at a diffusing time of between 6 hours and 72 hours.

### Claim 18 (depends on 17)

The method as set forth in claim 17 wherein said step of diffusing further including a step of aging the Nd—Fe—B magnet block including the first film and the second film at an aging temperature of between 450° C. and 650° C. at an aging time of between 3 hours and 15 hours.