# US 2020/0002843 A1 · Growth of plural sample rods to determine impurity build-up during production of single crystal silicon ingots

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0002843 A1
- Document ID: US20200002843A1
- Status: Published application
- Kind: A1
- Application number: 16/020,701
- Filed: 2018-06-27
- Published: 2020-01-02
- Earliest claimed: 2018-06-27
- Assignees: GlobalWafers Co., Ltd.
- Applicants: Global Wafers Co., Ltd.
- Inventors: Carissima Marie Hudson; JaeWoo Ryu
- Web page: https://patentgrep.com/patent/US20200002843A1

## CPC

- C30B 29/06: Silicon
- C30B 11/002: {Crucibles or containers for supporting the melt}
- C30B 11/003: {Heating or cooling of the melt or the crystallised material}
- C30B 15/04: adding doping materials, e.g. for n-p-junction
- C30B 15/20: Controlling or regulating (controlling or regulating in general G05)
- C30B 15/32: Seed holders, e.g. chucks
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

Methods for forming single crystal silicon ingots in which plural sample rods are grown from the melt are disclosed. A parameter related to the impurity concentration of the melt or ingot is measured. In some embodiments, the sample rods each have a diameter less than the diameter of the product ingot.

## Claims

### Claim 1

A method for producing a single crystal silicon ingot from a silicon melt held within a crucible comprising:
adding polycrystalline silicon to the crucible;
heating the polycrystalline silicon to cause a silicon melt to form in the crucible;
pulling a first sample rod from the melt, the first sample rod having a first sample rod diameter;
measuring a first sample rod parameter related to the quality of the first sample rod and/or the silicon melt;
pulling a second sample rod from the melt, the second sample rod having a second sample rod diameter;
measuring a second sample rod parameter related to the quality of the second sample rod and/or the silicon melt; and
pulling a product ingot from the melt, the product ingot having a diameter, the first sample rod diameter and the second sample rod diameter being less than the diameter of the product ingot.

### Claim 2 (depends on 1)

The method as set forth in claim 1 wherein the first sample rod parameter and the second sample rod parameter are the same parameter.

### Claim 3 (depends on 2)

The method as set forth in claim 2 further comprising comparing the measured first sample rod parameter to the measured second sample rod parameter.

### Claim 4 (depends on 3)

The method as set forth in claim 3 wherein the change of the parameter over time is measured.

### Claim 5 (depends on 1)

The method as set forth in claim 1 wherein the first sample rod parameter and the second sample rod parameter are different parameters.

### Claim 6 (depends on 1)

The method as set forth in claim 1 wherein the first sample rod parameter and the second sample rod parameter is related to the impurity concentration of the melt and/or product ingot.

### Claim 7 (depends on 6)

The method as set forth in claim 6 wherein the parameter is selected from the group consisting of the phosphorous concentration, boron concentration, aluminum concentration, gallium concentration, arsenic concentration, indium concentration, antimony concentration, total impurity concentration, dopant concentration, and resistivity of the sample rod.

### Claim 8 (depends on 1)

The method as set forth in claim 1 wherein polycrystalline silicon is not added to the crucible after the first sample rod is grown.

### Claim 9 (depends on 1)

The method as set forth in claim 1 wherein the impurity concentration of the first rod and second rod are measured, the concentration of impurities in the first and second rods being less than 1×1012 atoms/cm3, the impurity concentration being measured by Fourier-transform infrared spectroscopy or by photoluminescence.

### Claim 10

(canceled)

### Claim 11 (depends on 1)

The method as set forth in claim 1 further comprising altering a growth condition of the product ingot based at least in part on the measured first sample rod parameter and/or the measured second sample rod parameter.

### Claim 12 (depends on 1)

The method as set forth in claim 1 wherein the product ingot is a first product ingot and the melt is a first melt, the method further comprising altering a growth condition of a second product ingot grown from a second melt based at least in part on the measured first sample rod parameter and/or the measured second sample rod parameter.

### Claim 13 (depends on 11)

The method as set forth in claim 11 wherein the growth condition is selected from the group consisting of a hot-zone configuration, side heater power, heater geometry, crucible liner thickness, dopant concentration, impurity and dopant evaporation, gas flow rate, and chamber pressure.

### Claim 14 (depends on 1)

The method as set forth in claim 1 further comprising correlating the measured first sample rod parameter and/or the measured second sample rod parameter to crucible dissolution, hot zone contamination or gas flow impurity.

### Claim 15 (depends on 1)

The method as set forth in claim 1 wherein the first sample rod parameter and the second sample rod parameter are the resistivity of the sample rod, the first sample rod resistivity and the second sample rod resistivity being measured by contacting the rod with a resistivity probe.

### Claim 16 (depends on 15)

The method as set forth in claim 15 further comprising:
forming a planar segment on the first sample rod, the resistivity of the first sample rod being measured on the planar segment; and
forming a planar segment on the second sample rod, the resistivity of the second sample rod being measured on the planar segment.

### Claim 17

(canceled)

### Claim 18 (depends on 1)

The method as set forth in claim 1 further comprising applying a current to the sample rod to measure a resistance of the sample rod.

### Claim 19 (depends on 1)

The method as set forth in claim 1 wherein each sample rod is secured by a measurement apparatus comprising a clamp that holds the sample rod while contacting the sample rod with a resistivity probe.

### Claim 20 (depends on 1)

The method as set forth in claim 1 further comprising annealing each sample rod in a thermal donor kill cycle prior to measuring a resistivity of the sample rod.

### Claim 21 (depends on 1)

The method as set forth in claim 1 wherein the diameters of the first and second sample rods are each less than 0.50 times the diameter of the product ingot.

### Claim at position 22

22-23. (canceled)

### Claim 24 (depends on 1)

The method as set forth in claim 1 wherein the first and second sample rod and the product ingot each has a resistivity of at least about 1,500 Ω-cm.

### Claim at position 24

25-36. (canceled)