# US 2020/0002838 A1 · Methods for producing a silicon ingot that involve monitoring a moving average of the ingot neck pull rate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0002838 A1
- Document ID: US20200002838A1
- Status: Published application
- Kind: A1
- Application number: 16/021,948
- Filed: 2018-06-28
- Published: 2020-01-02
- Earliest claimed: 2018-06-28
- Applicants: Global Wafers Co., Ltd.
- Inventors: Zheng Lu; Chun-Sheng Wu; Feng-Chien Tsai; Chi-Yung Chen; Yeong-Ming Sheu; Hsien-Ta Tseng
- Web page: https://patentgrep.com/patent/US20200002838A1

## CPC

- C30B 15/22: Stabilisation or shape controlling of the molten zone near the pulled crystal; Controlling the section of the crystal
- C30B 15/203: {the relationship of pull rate (v) to axial thermal gradient (G)}
- C30B 29/06: Silicon
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

Methods for producing monocrystalline silicon ingots in which the pull rate during neck growth is monitored are disclosed. A moving average of the pull rate may be calculated and compared to a target moving average to determine if dislocations were not eliminated and the neck is not suitable for producing an ingot main body suspended from the neck.

## Claims

### Claim 1

A method for producing a monocrystalline silicon ingot having a neck and a main body suspended from the neck, the method comprising:
contacting a seed crystal with a silicon melt held within a crucible;
pulling a neck from the silicon melt;
measuring a pull rate at which the neck is pulled from the silicon melt;
calculating a moving average from the measured pull rate;
comparing the moving average of the measured pull rate to a target range; and
pulling an ingot main body from the melt if the moving average is within the target range, the main body being suspended from the neck.

### Claim 2 (depends on 1)

The method as set forth in claim 1 wherein a main body is not grown from the melt if the moving average is outside the target range.

### Claim 3 (depends on 2)

The method as set forth in claim 2 wherein the neck is lowered into the melt if the moving average is outside the target range.

### Claim 4 (depends on 2)

The method as set forth in claim 2 wherein the neck is a first neck, the method further comprising:
pulling a second neck from the silicon melt if the main body is not grown from the first neck;
measuring a pull rate at which the second neck is pulled from the silicon melt;
calculating a moving average from the measured pull rate of the second neck;
comparing the moving average of the measured pull rate of the second neck to the target range; and
pulling an ingot main body from the melt if the moving average of the measured pull rate of the second neck is within the target range, the main body being suspended from the second neck.

### Claim 5 (depends on 1)

The method as set forth in claim 1 wherein the target range comprises a maximum moving average.

### Claim 6 (depends on 1)

The method as set forth in claim 1 wherein the target range comprises a minimum moving average.

### Claim 7 (depends on 1)

The method as set forth in claim 1 wherein the target range is bound by a minimum moving average and a maximum moving average.

### Claim 8 (depends on 1)

The method as set forth in claim 1 wherein the moving average is time-averaged.

### Claim 9 (depends on 8)

The method as set forth in claim 8 wherein the calculated moving average is a moving average over at least the previous 5 seconds of neck growth.

### Claim 10 (depends on 1)

The method as set forth in claim 1 wherein the moving average is length-averaged.

### Claim 11 (depends on 10)

The method as set forth in claim 10 wherein the moving average is a moving average over at least about the previous 0.2 mm of neck grown.

### Claim 12 (depends on 1)

The method as set forth in claim 1 wherein comparing the moving average of the measured pull rate to a target range is performed for only a portion of the neck.

### Claim 13 (depends on 1)

The method as set forth in claim 1 wherein comparing the moving average of the measured pull rate to a target range is performed for the entire length of the neck.

### Claim 14 (depends on 1)

The method as set forth in claim 1 wherein the ingot main body has a diameter of at least about 200 mm or at least about 300 mm.

### Claim 15 (depends on 1)

The method as set forth in claim 1 wherein the ingot main body has a resistivity of less than about 20 mohm-cm.

### Claim 16 (depends on 1)

The method as set forth in claim 1 wherein the ingot main body is nitrogen-doped, the ingot main body comprising nitrogen at a concentration of at least about 1×1013 atoms/cm3.

### Claim 17 (depends on 1)

The method as set forth in claim 1 further comprising operating a heating system while measuring the pull rate, the heating system being operated at an average power while pulling the neck, the output power of the heating system being within about +/−0.5 kW of the average power while measuring the pull rate.

### Claim 18 (depends on 1)

The method as set forth in claim 1 further comprising operating a heating system while measuring the pull rate, the heating system being operated at an average power while pulling the neck, the output power of the heating system being within about +/−0.25 kW of the average power while measuring the pull rate.

### Claim at position 19

19-42. (canceled)