# US 2020/0002812 A1 · Thin-film deposition method and manufacturing method of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0002812 A1
- Document ID: US20200002812A1
- Status: Published application
- Kind: A1
- Application number: 16/454,063
- Filed: 2019-06-27
- Published: 2020-01-02
- Earliest claimed: 2018-06-29
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: ManSu Lee; SungKyu Kang; EunSook Lee; MinSoo Kim; SeungWoo Choi
- Web page: https://patentgrep.com/patent/US20200002812A1

## CPC

- C23C 16/45542: {Plasma being used non-continuously during the ALD reactions}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/402: {Silicon dioxide}
- C23C 16/455: characterised by the method used for introducing gases into reaction chamber or for modifying gas flows in reaction chamber
- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6687: {the compound comprising silicon and nitrogen}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10P 50/283: {by chemical means}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of depositing a thin film having a desired etching characteristic while improving a loss amount and loss uniformity of a lower film includes, on the semiconductor substrate and the pattern structure: a first operation of depositing a portion of the thin film by repeating a first cycle comprising (a1) a source gas supply operation, (b1) a reactant gas supply operation, and (c1) a plasma supply operation for a certain number of times; a second operation of depositing a remaining portion of the thin film by repeating a second cycle comprising (a2) a source gas supply operation, (b2) a reactant gas supply operation, and (c2) a plasma supply operation for a certain number of times after the first operation, wherein a supply time of the source gas supply operation (a1) is longer than a supply time of the source gas supply operation (a2).

## Claims

### Claim 1

A method of depositing a thin film on a pattern structure of a semiconductor substrate, the method comprising, on the semiconductor substrate and the pattern structure:
a first operation of depositing a portion of the thin film by repeating a first cycle comprising a source gas supply operation (a1), a reactant gas supply operation (b1), and a plasma supply operation (c1) for a certain number of times; and
a second operation of depositing a remaining portion of the thin film by repeating a second cycle comprising a source gas supply operation (a2), a reactant gas supply operation (b2), and a plasma supply operation (c2) for a certain number of times after the first operation,
wherein a supply time of the source gas supply operation (a1) is longer than a supply time of the source gas supply operation (a2).

### Claim 2 (depends on 1)

The method of claim 1, wherein the supply time of the source gas supply operation (a1) is two to five times the supply time of the source gas supply operation (a2).

### Claim 3 (depends on 1)

The method of claim 1, wherein the supply time of the source gas supply operation (a1) is 0.2 seconds to 1 second.

### Claim 4 (depends on 1)

The method of claim 1, wherein the number of repetitions of the first cycle is less than the number of repetitions of the second cycle.

### Claim 5 (depends on 1)

The method of claim 1, wherein a ratio of the number of repetitions of the first cycle to the number of repetitions of the second cycle is 1/12 to 1/10.

### Claim 6 (depends on 1)

The method of claim 1, wherein a loss amount and loss uniformity of the pattern structure is adjusted by controlling at least one of the supply time of the source gas supply operation (a1), plasma power of the plasma supply operation (c1), and a plasma duty ratio of the plasma supply operation (c1) in the first operation.

### Claim 7 (depends on 6)

The method of claim 6, wherein the loss amount of the pattern structure during the first operation is reduced when the supply time of the source gas supply operation (a1) is increased.

### Claim 8 (depends on 6)

The method of claim 6, wherein the loss amount of the pattern structure during the first operation is reduced and the loss uniformity of the pattern structure is improved by increasing the plasma power of the plasma supply operation (c1) and decreasing the plasma duty ratio of the plasma supply operation (c1) while maintaining multiplication of the plasma power by the plasma duty ratio of the plasma supply operation (c1) constant.

### Claim 9 (depends on 8)

The method of claim 8, wherein the plasma power of the plasma supply operation (c1) in the first operation is in the range of about 650 W to about 1200 W, and
the plasma duty ratio of the plasma supply operation (c1) in the first operation is in the range of about 25% to about 50%.

### Claim 10 (depends on 1)

The method of claim 1, wherein plasma power of the plasma supply operation (c1) is greater than plasma power of the plasma supply operation (c2), and
a plasma duty ratio of the plasma supply operation (c1) is less than a plasma duty ratio of the plasma supply operation (c2).

### Claim 11 (depends on 1)

The method of claim 1, wherein a desired wet etch rate (WER) of the thin film is obtained by controlling at least one of plasma power of the plasma supply operation (c2) and a plasma duty ratio of the plasma supply operation (c2).

### Claim 12 (depends on 11)

The method of claim 11, wherein the WER of the thin film is reduced when the plasma power of the plasma supply operation (c2) is increased.

### Claim 13 (depends on 11)

The method of claim 11, wherein the WER of the thin film is reduced when the plasma duty ratio of the plasma supply operation (c2) is increased.

### Claim 14

A method of depositing a thin film on a pattern structure of a semiconductor substrate, the method comprising:
repeating a first cycle of applying first plasma power in a pulse form m times while using a plasma atomic layer deposition process, and improving a loss amount and loss uniformity of the pattern structure; and
repeating a second cycle of applying second plasma power in a pulse form n times while using the plasma atomic layer deposition process, and depositing the thin film.

### Claim 15 (depends on 14)

The method of claim 14, wherein the improving of the loss amount and loss uniformity of the pattern structure comprises:
improving the loss amount and loss uniformity of the pattern structure by increasing a supply time of a source gas supply operation in the plasma atomic layer deposition process.

### Claim 16 (depends on 14)

The method of claim 14, wherein the improving of the loss amount and loss uniformity of the pattern structure comprises:
improving the loss amount and loss uniformity of the pattern structure by adjusting at least one of the first plasma power and a duty ratio.

### Claim 17 (depends on 14)

The method of claim 14, further comprising forming the thin film by setting a ratio of the number of repetitions (m times) of the first cycle to the number of repetitions (n times) of the second cycle to 1/12 to 1/10.

### Claim 18 (depends on 14)

The method of claim 14, wherein the depositing of the thin film by repeating the second cycle n times comprises:
controlling a wet etch rate (WER) of the thin film by adjusting at least one of the second plasma power and a duty ratio.

### Claim 19 (depends on 14)

The method of claim 14, further comprising:
removing at least a portion of the thin film to form a spacer pattern of the thin film,
wherein the spacer pattern of the thin film has a constant linewidth size over the semiconductor substrate.

### Claim 20

A method of depositing a thin film on a pattern structure of a semiconductor substrate, the method comprising:
improving a loss amount and loss uniformity of the pattern structure by controlling at least one of a supply time of a source gas supply operation, plasma power and a plasma duty ratio of a plasma supply operation while using a plasma atomic layer deposition process; and
controlling a wet etch rate (WER) of the thin film by controlling at least one of the plasma power and the plasma duty ratio of the plasma supply operation while using the plasma atomic layer deposition process.