# US 2020/0002799 A1 · Spray coating, sraying powder, spraying powder manufacturing method and spray coating manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0002799 A1
- Document ID: US20200002799A1
- Status: Published application
- Kind: A1
- Application number: 16/489,070
- Filed: 2018-02-28
- Published: 2020-01-02
- Earliest claimed: 2017-03-01
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Noriaki HAMAYA; Ichiro UEHARA
- Web page: https://patentgrep.com/patent/US20200002799A1

## CPC

- C23C 4/11: Oxides
- B32B 9/005: {comprising one layer of ceramic material, e.g. porcelain, ceramic tile (layered products with at least two ceramic layers composed mainly of ceramic B32B18/00)}
- C01F 17/259: Oxyhalides
- C01F 17/265: Fluorides
- C04B 35/50: based on rare-earth compounds {(non-oxide rare earth compounds C04B35/5156)}
- C04B 35/5156: {based on rare earth compounds}
- C09D 1/00: Coating compositions, e.g. paints, varnishes or lacquers, based on inorganic substances
- C09D 5/03: Powdery paints
- C09D 5/033: {characterised by the additives}
- C09D 7/61: inorganic
- C23C 4/04: characterised by the coating material
- C23C 4/134: Plasma spraying
- H10P 50/00: Etching of wafers, substrates or parts of devices
- C01P 2002/52: containing elements as dopants
- C01P 2006/62: L* (lightness axis)
- C01P 2006/63: a* (red-green axis)
- C01P 2006/64: b* (yellow-blue axis)
- C04B 2237/34: Oxidic
- C04B 2237/36: Non-oxidic
- C08K 3/16: Halogen-containing compounds
- C08K 2003/221: {of rare earth metal}
- C08K 2201/014: Additives containing two or more different additives of the same subgroup in C08K
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A spray coating containing a rare earth fluoride and/or a rare earth acid fluoride contains, carbon at 0.01-2% by mass or titanium or molybdenum at 1-1000 ppm. When an acid fluoride is not contained, the spray coating is gray to black in which, in terms of the L*a*b* chromaticity, L* is 25-64, a* is −3.0 to +5.0, and b* is −4.0 to +8.0. When an acid fluoride is contained, the spray coating is white or gray to black in which, in terms of the L*a*b* chromaticity, L* is equal to or greater than 25 and less than 91, a* is −3.0 to +5.0, and b* is −6.0 to +8.0. By forming this coating on a plasma resistant member, a partial color change is reduced, thus, a member that is capable of reliably realizing the original longevity is obtained.

## Claims

### Claim 1

A sprayed coating composed of the following (1) and/or (2), or the mixture of the following (1) and/or (2) and one or two or more selected from the following (3) to (5):
(1) a fluoride of at least one rare earth element selected from rare earth elements comprising yttrium that belong in Group 3A;
(2) an oxyfluoride of the rare earth element;
(3) an oxide of the rare earth element;
(4) a composite oxide of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In; and
(5) a composite fluoride of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In,
wherein, the sprayed coating contains 0.004 to 2% by weight of carbon or 1 to 1,000 ppm of titanium or molybdenum, and
in case where the sprayed coating does not contain the oxyfluoride (2), the sprayed coating displays a gray to black color having an L* value of 25 to 64, an a* value of −3.0 to +5.0, and a b* value of −6.0 to +8.0 expressed by L*a*b* colorimetric system, or
in case where the sprayed coating contains the oxyfluoride (2), the sprayed coating displays a white color or gray to black color having an L* value of at least 25 and less than 91, an a* value of −3.0 to +5.0, and a b* value of −6.0 to +8.0, expressed by L*a*b* colorimetric system.

### Claim 2 (depends on 1)

The sprayed coating of claim 1 wherein the rare earth element is at least one selected from Y, Gd, Yb, and La.

### Claim 3 (depends on 1)

The sprayed coating of claim 1, having an oxygen content of 0.01 to 13.5% by weight.

### Claim 4 (depends on 1)

The sprayed coating of claim 1, having a carbon content of 0.004 to 0.15% by weight.

### Claim 5

A spraying powder composed of the following (1) and/or 2), or the mixture of the following (1) and/or (2) and one or two or more selected from the following (3) to (6):
(1) a fluoride of at least one rare earth element selected from rare earth elements comprising yttrium that belong in Group 3A;
(2) an oxyfluoride of the rare earth element;
(3) an oxide of the rare earth element;
(4) a composite oxide of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In;
(5) a composite fluoride of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In; and
(6) an oxide of at least one or two or more metals selected from Al, Si, Zr and In,
wherein, the spraying powder contains 0.004 to 2% by weight of carbon or 1 to 1,000 ppm of titanium or molybdenum, and
the spraying powder displays a white color or gray to black color having L* value of at least 25 and less than 91, an a* value of −3.0 to +5.0, and a b* value of −6.0 to +8.0, expressed by L*a*b* colorimetric system.

### Claim 6 (depends on 5)

The spraying powder of claim 5 wherein the rare earth element is at least one selected from Y, Gd, Yb, and La.

### Claim 7 (depends on 5)

The spraying powder of claim 5, having an oxygen content of 0.01 to 13.5% by weight.

### Claim 8 (depends on 5)

The spraying powder of claim 5, being a fired spraying powder and having a carbon content of 0.004 to 0.15% by weight.

### Claim 9 (depends on 5)

The spraying powder of claim 5, being an unfired spraying powder and having a carbon content, of 0.004 to 1.5% by weight.

### Claim 10 (depends on 5)

A method for preparing a spraying powder of claim 5, the method comprising the steps of:
drying a slurry comprising a powder displaying a white color and composed of the following (1) and/or (2), or the mixture of the following (1) and/or (2) and one or two or more selected from the following (3) to (6);
(1) a fluoride of at least one rare earth element selected from rare earth elements comprising yttrium that belong in Group 3A;
(2) an oxyfluoride of the rare earth element;
(3) an oxide of the rare earth element;
(4) a composite oxide of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In;
(5) a composite fluoride of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In; and
(6) an oxide of at least one or two or more metals selected from Al, Si, Zr and In, and an appropriate amount of a carbon source to produce a spraying powder having a carbon concentration of 0.004 to 2% by weight,
roasting and firing the resulting dried material, and
thereby obtaining a spraying powder displaying a white color or gray to black color having an L* value of at least 25 and less than 91, an a* value of −3.0 to +5.0, and a b* value of −6.0 to +8.0, expressed by L*a*b* colorimetric system.

### Claim 11 (depends on 10)

The method for preparing a spraying powder of claim 10 wherein the roasting is subjected at 500 to 800° C. in nitrogen gas, and then the firing is subjected to the roasted powder at 800 to 1,000° C. in vacuum or an inert gas atmosphere.

### Claim 12 (depends on 10)

The method for preparing a spraying powder of claim 10 wherein the powder displaying a white color and composed of said (1) and/or (2), or the mixture of said (1) and/or (2) and one or two or more selected from said (3) to (6) has an oxygen content of 0.01 to 13.5% by weight.

### Claim 13 (depends on 10)

The method for preparing a spraying powder of claim 10 wherein the carbon source is used in an appropriate amount to produce a spraying powder having a carbon concentration of 0.004 to 0.15% by weight.

### Claim 14 (depends on 5)

A method for preparing a spraying powder of claim 5, the method comprising the steps of:
drying with granulating a slurry comprising a powder displaying a white color and composed of the following (1) and/or (2), or the mixture of the following (1) and/or (2) and one or two or more selected from the following (3) to (6);
(1) a fluoride of at least one rare earth element selected from rare earth elements comprising yttrium that belong in Group 3A;
(2) an oxyfluoride of the rare earth element;
(3) an oxide of the rare earth element;
(4) a composite oxide of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In;
(5) a composite fluoride of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In; and
(6) an oxide of at least one or two or more metals selected from Al, Si, Zr and In, polyvinyl alcohol, and an appropriate amount of a water-soluble salt of titanium or molybdenum to produce a spraying powder having a titanium or molybdenum concentration of 1 to 1,000 ppm,
firing the resulting powder, and
thereby obtaining a spraying powder displaying a white color or gray to black color having an L* value of at least 25 and less than 91, an a* value of −3.0 to +5.0, and a b* value of −6.0 to +8.0, expressed by L*a*b* colorimetric system.

### Claim 15 (depends on 14)

The method for preparing a spraying powder of claim 14 wherein the firing is subjected to the dried/granulated powder at 800 to 1,000° C. in vacuum or an inert gas atmosphere.

### Claim 16 (depends on 14)

The method for preparing a spraying powder of claim 14 wherein the powder displaying a white color and composed of said (1) and/or (2), or the mixture of said (1) and/or (2) and one or two or more selected from said (3) to (6) has an oxygen content of 0.01 to 13.5% by weight.

### Claim 17

A sprayed coating composed of the following (1) and/or (2), or the mixture of the following (1) and/or (2) and one or two or more selected from the following (3) to (5):
(1) a fluoride of at least one rare earth element selected from rare earth elements comprising yttrium that belong in Group 3A;
(2) an oxyfluoride of the rare earth element;
(3) an oxide of the rare earth element;
(4) a composite oxide of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In; and
(5) a composite fluoride of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In,
wherein, the sprayed coating comprises at its surface a gray to black colored layer displaying a gray to black color having an L* value of 25 to 64, an a* value of −3.0 to +5.0, and a b* value of −6.0 to +8.0, expressed by L*a*b* colorimetric system.

### Claim 18 (depends on 17)

The sprayed coating of claim 17 wherein the gray to black colored layer has a depth of up to 2 μm from the surface of the sprayed coating.

### Claim 19 (depends on 17)

The sprayed coating of claim 17, having an oxygen content of 0.01 to 13.5% by weight.

### Claim 20 (depends on 17)

A method for preparing a sprayed coating of claim 17, the method comprising the steps of:
thermally spraying a powder to a surface of a substrate, the powder displaying a white color and composed of the following (1) and/or (2), or the mixture of the following (1) and/or (2) and one or two or more selected from the following (3) to (6):
(1) a fluoride of at least one rare earth element selected from rare earth elements comprising yttrium that belong in Group 3A;
(2) an oxyfluoride of the rare earth element;
(3) an oxide of the rare earth element;
(4) a composite oxide of the rare earth element and at least one or two or more metals selected from Al, Si, Zr and In;
(5) a composite fluoride of the rate earth element and at least one or two or more metals selected from Al, Si, Zr and In; and
(6) an oxide of at least one or two or more metals selected from Al, Si, Zr and In,
forming a sprayed coating displaying a white color having an L* value of at least 81, an a* value of −3.0 to +3.0, and a b* value of −3.0 to +3.0, expressed by L*a*b* colorimetric system, and
effecting plasma exposure treatment on the resulting sprayed coating to form a gray to black colored layer at its surface, the gray to black colored layer displaying a gray to black color having an L* value of 25 to 64, an a* value of −3.0 to +5.0, and a b* value of −6.0 to +8.0, expressed by L*a*b* colorimetric system.

### Claim 21 (depends on 20)

The method for preparing a sprayed coating of claim 20 wherein the gray to black colored layer is formed with a depth of up to 2 μm from the surface of the sprayed coating.

### Claim 22 (depends on 20)

The method for preparing a sprayed coating of claim 20 wherein the powder displaying white color and composed of said (1) and/or (2), or the mixture of said (1) and/or (2) and one or two or more selected from said (3) to (6) has an oxygen content of 0.01 to 13.5% by weight.