# US 2020/0002786 A1 · Green metal composite material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0002786 A1
- Document ID: US20200002786A1
- Status: Published application
- Kind: A1
- Application number: 16/560,962
- Filed: 2019-09-04
- Published: 2020-01-02
- Earliest claimed: 2018-06-29
- Inventors: Fan Fan
- Web page: https://patentgrep.com/patent/US20200002786A1

## CPC

- C22C 1/059: Making alloys comprising less than 5% by weight of dispersed reinforcing phases
- B22F 3/14: simultaneously
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 1/1084: {by mechanical alloying (blending, milling)}
- C22C 23/00: Alloys based on magnesium
- C22C 23/04: with zinc or cadmium as the next major constituent
- C22C 26/00: Alloys containing diamond {or cubic or wurtzitic boron nitride, fullerenes or carbon nanotubes}
- C22C 32/0084: {carbon or graphite as the main non-metallic constituent}
- B22F 2009/043: {by ball milling}
- B22F 2301/058: Magnesium
- B22F 2302/40: Carbon, graphite
- B22F 2302/403: Carbon nanotube
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C 2026/002: {Carbon nanotubes}
- C22C 2202/04: Hydrogen absorbing
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

The invention provides a green metal composite material, which is prepared by the following method: Provide Mg, Mo, Al, Ni, and Ti powders; weigh the Mg, Mo, Al, Ni, and Ti powders; and perform the first ball milling on the Mg, Mo, Al, Ni, and Ti powders; perform vacuum melting to obtain a Mg-based alloy ingots; crush the Mg-based alloy ingots; provide carbon nano tubes and graphene powders; and perform surface modification; mix well the crushed Mg-based alloy ingots and the surface modified carbon nano tubes and the graphene powders, and perform a second ball milling to obtain a second mixed powder; then perform a first heat treatment to obtain a third mixed powder, then perform a second hot pressed sintering. The process technology of this invention solves the problems of poor compatibility, easy to be segregated and unstable property of the non-metallic particles and metallic matrix.

## Claims

### Claim 1

A green metal composite material, characterized in that: the green metal composite material mentioned in this patent is prepared by the following method:
Provide Mg, Mo, Al, Ni, and Ti powders;
Weigh the Mg, Mo, Al, Ni, and Ti powders according to a predetermined chemical formula;
Perform a first ball milling on the Mg, Mo, Al, Ni, and Ti powders after weighing to obtain a first mixed powder,
Perform vacuum melting on the first mixed powder to obtain a Mg-based alloy ingots;
Crush the Mg-based alloy ingots;
Provide carbon nano tubes and graphene powders;
Perform surface modification on the mentioned carbon nano tubes and graphene powders;
Mix well the crushed Mg-based alloy ingots and the surface modified carbon nano tubes and the graphene powders, and perform a second ball milling on the mixture to obtain a second mixed powder;
Perform a first heat treatment on the second mixed powder to obtain a third mixed powder,
Perform a second hot pressed sintering on the third mixed powder.

### Claim 2 (depends on 1)

The green metal composite material mentioned in claim 1, characterized in that: the predetermined chemical formula mentioned in claim 1 is Mg100-x-y-z-aMoxAlyNizTia, wherein x-=0.5-1.5, y=2-3, z=10-12, a=1-3.

### Claim 3 (depends on 1)

The green metal composite material mentioned in claim 1, characterized in that: perform a first ball milling on the Mg, Mo, Al, Ni, and Ti powders after weighing, and the specific methods are as follows: the ball milling atmosphere is argon atmosphere, the ball milling speed is 1500-1800 r/min, the ball milling time is 10-20 h, the ratio of ball to material is 8:1-9:1, in the ball milling process, each ball milling lasts 60-70 min, and suspend the ball milling for 4-5 min, the temperature in the ball milling tank is controlled to be lower than 600° C. during the ball milling process.

### Claim 4 (depends on 1)

The green metal composite material mentioned in claim 1, characterized in that: specifically, the vacuum melting performed on the first mixed powder is as follows: the vacuum degree is less than 0.01 Pa, the smelting time is 80-100 min, and the alloy ingots are flipped once every 200-250 s during the smelting process.

### Claim 5 (depends on 1)

The green metal composite material mentioned in claim 1, characterized in that: specifically, the surface modification performed on the mentioned carbon nano tubes and graphene powders is as follows: prepare the silane coupling agent organic solvent, wherein the weight percentage of silane coupling agent is 2-3 wt %; place the carbon nano tubes and graphene powders into the organic solution of the silane coupling agent, and stir, the stirring time is 50-70 min, and the stirring temperature is 70-80° C.

### Claim 6 (depends on 1)

The green metal composite material mentioned in claim 1, characterized in that: specifically, the second ball milling is as follows: the ball milling atmosphere is argon atmosphere, the ball milling speed is 500-600 r/min, the ball milling time is 5-8 h, the ratio of ball to material is 4:1-5:1, in the ball milling process, each ball milling lasts 30-40 min, and suspend the ball milling for 4-5 min, the temperature in the ball milling tank is controlled to be lower than 300° C. during the ball milling process.

### Claim 7 (depends on 1)

The green metal composite material mentioned in claim 1, characterized in that: in the second mixture powder, Mg-based alloy ingots account for 100-120 parts by weight after being crushed, surface modified carbon nano tubes account for 10-20 parts, and surface modified graphene powders account for 3-5 parts.

### Claim 8 (depends on 1)

The green metal composite material mentioned in claim 1, characterized in that: the first heat treatment performed on the second mixed powder is as follows: the heat treatment atmosphere is hydrogen atmosphere, the heat treatment temperature is 600-650° C., the heat treatment time is 10-20 min, and the heating rate is 10-20° C./min.

### Claim 9 (depends on 1)

The green metal composite material mentioned in claim 1, characterized in that: a second hot pressed sintering performed on the third mixed powder is as follows: the hot pressing pressure is lower than 0.03 Pa, the hot pressing to temperature is 700-780° C., the hot pressing pressure is 5-10 MPa, and the hot pressing time is 5-10 min.