# US 2020/0002779 A1 · Hot-rolled ferritic stainless steel sheet and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0002779 A1
- Document ID: US20200002779A1
- Status: Published application
- Kind: A1
- Application number: 16/480,785
- Filed: 2018-01-12
- Published: 2020-01-02
- Earliest claimed: 2017-01-26
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Masataka YOSHINO; Mitsuyuki FUJISAWA
- Web page: https://patentgrep.com/patent/US20200002779A1

## CPC

- C21D 6/004: {containing Cr and Ni}
- C21D 8/0226: {Hot rolling}
- C21D 6/02: Hardening by precipitation
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0263: {following hot rolling}
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/52: with cobalt
- C22C 38/54: with boron
- C21D 2211/005: Ferrite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a hot-rolled ferritic stainless steel sheet which has sufficient corrosion resistance and which can prevent the occurrence of cracking when subjected to blanking to be formed into a thick flange, and also provided is a method for manufacturing the hot-rolled ferritic stainless steel sheet. A hot-rolled ferritic stainless steel sheet having a chemical composition containing, in mass %, C: 0.001 to 0.020%, Si: 0.05 to 1.00%, Mn: 0.05 to 1.00%, P: 0.04% or less, S: 0.01% or less, Al: 0.001 to 0.50%, N: 0.001 to 0.020%, Cr: 11.0 to 24.0%, Ni: 0.01 to 2.00%, and Nb: 0.12 to 0.80%, with the balance being Fe and incidental impurities, wherein the hot-rolled ferritic stainless steel sheet has a threshold stress intensity factor KIC of 25 MPa·m1/2 or more.

## Claims

### Claim 1

A hot-rolled ferritic stainless steel sheet having a chemical composition comprising, in mass %,
C: 0.001 to 0.020%,
Si: 0.05 to 1.00%,
Mn: 0.05 to 1.00%,
P: 0.04% or less,
S: 0.01% or less,
Al: 0.001 to 0.50%,
N: 0.001 to 0.020%,
Cr: 11.0 to 24.0%,
Ni: 0.01 to 2.00%, and
Nb: 0.12 to 0.80%, with a balance of Fe and incidental impurities,
wherein the hot-rolled ferritic stainless steel sheet has a threshold stress intensity factor KIC of 25 MPa·m1/2 or more.

### Claim 2

A hot-rolled ferritic stainless steel sheet having a chemical composition comprising, in mass %,
C: 0.001 to 0.020%,
Si: 0.05 to 1.00%,
Mn: 0.05 to 1.00%,
P: 0.04% or less,
S: 0.01% or less,
Al: 0.001 to 0.50%,
N: 0.001 to 0.020%,
Cr: 13.0 to 24.0%,
Ni: 0.01 to 0.60%, and
Nb: 0.12 to 0.80%, with a balance of Fe and incidental impurities,
wherein the hot-rolled ferritic stainless steel sheet has a threshold stress intensity factor KIC of 25 MPa·m1/2 or more.

### Claim 3 (depends on 1)

The hot-rolled ferritic stainless steel sheet according to claim 1, wherein the chemical composition further comprises, in mass %, one or more selected from
Cu: 0.01 to 1.50%,
Mo: 0.01 to 2.00%,
W: 0.01 to 0.20%, and
Co: 0.01 to 0.20%.

### Claim 4 (depends on 2)

The hot-rolled ferritic stainless steel sheet according to claim 2, wherein the chemical composition further comprises, in mass %, one or more selected from
Cu: 0.01 to 1.50%,
Mo: 0.01 to 2.00%,
W: 0.01 to 0.20%, and
Co: 0.01 to 0.20%.

### Claim 5 (depends on 1)

The hot-rolled ferritic stainless steel sheet according to claim 1, wherein the chemical composition further comprises, in mass %, one or more selected from
Ti: 0.01 to 0.30%,
V: 0.01 to 0.20%,
Zr: 0.01 to 0.20%,
REM: 0.001 to 0.100%,
B: 0.0002 to 0.0025%,
Mg: 0.0005 to 0.0030%, and
Ca: 0.0005 to 0.0030%.

### Claim 6 (depends on 2)

The hot-rolled ferritic stainless steel sheet according to claim 2, wherein the chemical composition further comprises, in mass %, one or more selected from
Ti: 0.01 to 0.30%,
V: 0.01 to 0.20%,
Zr: 0.01 to 0.20%,
REM: 0.001 to 0.100%,
B: 0.0002 to 0.0025%,
Mg: 0.0005 to 0.0030%, and
Ca: 0.0005 to 0.0030%.

### Claim 7 (depends on 3)

The hot-rolled ferritic stainless steel sheet according to claim 3, wherein the chemical composition further comprises, in mass %, one or more selected from
Ti: 0.01 to 0.30%,
V: 0.01 to 0.20%,
Zr: 0.01 to 0.20%,
REM: 0.001 to 0.100%,
B: 0.0002 to 0.0025%,
Mg: 0.0005 to 0.0030%, and
Ca: 0.0005 to 0.0030%.

### Claim 8 (depends on 4)

The hot-rolled ferritic stainless steel sheet according to claim 4, wherein the chemical composition further comprises, in mass %, one or more selected from
Ti: 0.01 to 0.30%,
V: 0.01 to 0.20%,
Zr: 0.01 to 0.20%,
REM: 0.001 to 0.100%,
B: 0.0002 to 0.0025%,
Mg: 0.0005 to 0.0030%, and
Ca: 0.0005 to 0.0030%.

### Claim 9 (depends on 1)

A method for manufacturing the hot-rolled ferritic stainless steel sheet according to claim 1, the method comprising hot rolling, the hot rolling including performing finish rolling including three or more passes,
wherein a temperature range for final three passes of the finish rolling is 800 to 1100° C., and an accumulated rolling reduction ratio for the final three passes is 25% or more.

### Claim 10 (depends on 2)

A method for manufacturing the hot-rolled ferritic stainless steel sheet according to claim 2, the method comprising hot rolling, the hot rolling including performing finish rolling including three or more passes,
wherein a temperature range for final three passes of the finish rolling is 800 to 1100° C., and an accumulated rolling reduction ratio for the final three passes is 25% or more.

### Claim 11 (depends on 3)

A method for manufacturing the hot-rolled ferritic stainless steel sheet according to claim 3, the method comprising hot rolling, the hot rolling including performing finish rolling including three or more passes,
wherein a temperature range for final three passes of the finish rolling is 800 to 1100° C., and an accumulated rolling reduction ratio for the final three passes is 25% or more.

### Claim 12 (depends on 4)

A method for manufacturing the hot-rolled ferritic stainless steel sheet according to claim 4, the method comprising hot rolling, the hot rolling including performing finish rolling including three or more passes,
wherein a temperature range for final three passes of the finish rolling is 800 to 1100° C., and an accumulated rolling reduction ratio for the final three passes is 25% or more.

### Claim 13 (depends on 5)

A method for manufacturing the hot-rolled ferritic stainless steel sheet according to claim 5, the method comprising hot rolling, the hot rolling including performing finish rolling including three or more passes,
wherein a temperature range for final three passes of the finish rolling is 800 to 1100° C., and an accumulated rolling reduction ratio for the final three passes is 25% or more.

### Claim 14 (depends on 6)

A method for manufacturing the hot-rolled ferritic stainless steel sheet according to claim 6, the method comprising hot rolling, the hot rolling including performing finish rolling including three or more passes,
wherein a temperature range for final three passes of the finish rolling is 800 to 1100° C., and an accumulated rolling reduction ratio for the final three passes is 25% or more.

### Claim 15 (depends on 7)

A method for manufacturing the hot-rolled ferritic stainless steel sheet according to claim 7, the method comprising hot rolling, the hot rolling including performing finish rolling including three or more passes,
wherein a temperature range for final three passes of the finish rolling is 800 to 1100° C., and an accumulated rolling reduction ratio for the final three passes is 25% or more.

### Claim 16 (depends on 8)

A method for manufacturing the hot-rolled ferritic stainless steel sheet according to claim 8, the method comprising hot rolling, the hot rolling including performing finish rolling including three or more passes,
wherein a temperature range for final three passes of the finish rolling is 800 to 1100° C., and an accumulated rolling reduction ratio for the final three passes is 25% or more.