# US 2020/0002219 A1 · Glass frit and display device including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0002219 A1
- Document ID: US20200002219A1
- Status: Published application
- Kind: A1
- Application number: 16/454,874
- Filed: 2019-06-27
- Published: 2020-01-02
- Earliest claimed: 2018-06-27
- Assignees: Samsung Display Co., Ltd.; Bass, Inc.
- Applicants: Samsung Display Co., Ltd.; Bass Co., Ltd.
- Inventors: Chanyoung PARK; Danbi CHOI; Soukjune HWANG; Hyunmin HWANG; Hokyum KIM; Taeho PARK; Sanghoon LEE
- Web page: https://patentgrep.com/patent/US20200002219A1

## CPC

- C03C 8/04: containing zinc
- C03C 3/122: {containing oxides of As, Sb, Bi, Mo, W, V, Te as glass formers}
- C03C 3/155: containing zirconium, titanium, tantalum or niobium
- C03C 8/24: Fusion seal compositions being frit compositions having non-frit additions, i.e. for use as seals between dissimilar materials, e.g. glass and metal; Glass solders
- H10K 59/8722: {Peripheral sealing arrangements, e.g. adhesives, sealants}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

A glass frit includes Bi2O3 and has a glass transition temperature (Tg) in a range of 280° C. to 320° C. A display device includes the glass frit including Bi2O3 and the glass transition temperature (Tg) in the range of 280° C. to 320° C. The display device shows excellent internal reliability and drop strength.

## Claims

### Claim 1

A glass frit comprising Bi2O3 and having a glass transition temperature (Tg) in a range of 280° C. to 320° C.

### Claim 2 (depends on 1)

The glass frit of claim 1, wherein a crystallization starting temperature (Tx) of the glass frit is in a range of 360° C. to 450° C.

### Claim 3 (depends on 2)

The glass frit of claim 2, wherein a difference (Tx−Tg) between the crystallization starting temperature (Tx) and the glass transition temperature (Tg) is in a range of 80° C. to 160° C.

### Claim 4 (depends on 1)

The glass frit of claim 1, wherein a thermal expansion coefficient of the glass frit is 45×10−7/° C. to 55×10−7/° C.

### Claim 5 (depends on 1)

The glass frit of claim 1, wherein the glass frit comprises the Bi2O3 in an amount in a range of 1 mol % to 5 mol %.

### Claim 6 (depends on 1)

The glass frit of claim 1, further comprising V2O5, ZnO, ZrO2, and TeO2.

### Claim 7 (depends on 6)

The glass frit of claim 6, wherein the glass frit comprises:
the V2O5 in an amount in a range of 20 mol % to 55 mol %;
the ZnO in an amount in a range of 20 mol % to 55 mol %;
the ZrO2 in an amount in a range of 1 mol % to 25 mol %;
the TeO2 in an amount in a range of 1 mol % to 20 mol %; and
the Bi2O3 in an amount in a range of 1 mol % to 5 mol %.

### Claim 8 (depends on 6)

The glass frit of claim 6, further comprising at least one selected from Fe, Cu, Mn, B, Ti and Ca.

### Claim 9 (depends on 8)

The glass frit of claim 8, wherein the glass frit comprises the at least one selected from Fe, Cu, Mn, B, Ti and Ca in an amount in a range of 0.5 mol % to 25 mol %.

### Claim 10 (depends on 8)

The glass frit of claim 8, further comprising Nb2O5.

### Claim 11 (depends on 10)

The glass frit of claim 10, wherein the glass frit comprises the Nb2O5 in an amount in a range of 1 mol % to 10 mol %.

### Claim 12 (depends on 10)

The glass frit of claim 10, wherein the glass frit comprises:
the V2O5 in an amount in a range of 20 mol % to 55 mol %;
the ZnO in an amount in a range of 20 mol % to 55 mol %;
the ZrO2 in an amount in a range of 1 mol % to 25 mol %;
the Nb2O5 in an amount in a range of 1 mol % to 10 mol %;
the TeO2 in an amount in a range of 1 mol % to 20 mol %;
the Bi2O3 in an amount in a range of 1 mol % to 5 mol %; and
the at least one selected from Fe, Cu, Mn, B, Ti and Ca in an amount in a range of 0.5 mol % to 25 mol %.

### Claim 13 (depends on 1)

The glass frit of claim 1, wherein the glass frit does not include Al.

### Claim 14 (depends on 1)

The glass frit of claim 1, wherein the crystallization temperature (Tc) is in a range of 420° C. to 460° C.

### Claim 15 (depends on 1)

The glass frit of claim 1, wherein a dilatometric softening point temperature (Tdsp) of the glass frit is in a range of 330° C. to 370° C.

### Claim 16

A display device comprising:
a first substrate comprising a base layer and a display unit on the base layer;
a second substrate facing the first substrate; and
an encapsulation unit between the first substrate and the second substrate, and comprising a glass frit comprising Bi2O3 and having a glass transition temperature (Tg) in a range of 280° C. to 320° C.

### Claim 17 (depends on 16)

The display device according to claim 16, wherein the encapsulation unit surrounds the display unit.

### Claim 18 (depends on 16)

The display device according to claim 16, wherein the first substrate and the second substrate are separately arranged and the encapsulation unit is located along each flange of the first substrate and the second substrate.

### Claim 19 (depends on 16)

The display device according to claim 16, wherein the glass frit further comprises V2O5, ZnO, ZrO2, Nb2O5 and TeO2,
wherein the glass frit further comprises at least one selected from Fe, Cu, Mn, B, Ti and Ca, and
wherein the glass frit comprises:
the V2O5 in an amount in a range of 20 mol % to 55 mol %,
the ZnO in an amount in a range of 20 mol % to 55 mol %,
the ZrO2 in an amount in a range of 1 mol % to 25 mol %,
the Nb2O5 in an amount in a range of 1 mol % to 10 mol %,
the TeO2 in an amount in a range of 1 mol % to 20 mol %,
the Bi2O3 in an amount in a range of 1 mol % to 5 mol %, and
the at least one selected from Fe, Cu, Mn, B, Ti and Ca in an amount in a range of 0.5 mol % to 25 mol %.

### Claim 20 (depends on 16)

The display device according to claim 16, wherein the display unit comprises an organic light emitting diode, and
wherein the organic light emitting diode comprises a first electrode, a second electrode and a light emitting layer therebetween.