# US 2020/0002210 A1 · High-strength geopolymer hollow microsphere, preparation method thereof and phase change energy storage microsphere

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0002210 A1
- Document ID: US20200002210A1
- Status: Published application
- Kind: A1
- Application number: 16/485,450
- Filed: 2018-05-25
- Published: 2020-01-02
- Earliest claimed: 2017-06-21
- Assignees: China University of Petroleum (East China)
- Applicants: China University of Petroleum (East China)
- Inventors: Huajie LIU; Yuhuan BU; Rui MA; Shenglai GUO; Longlong AN
- Web page: https://patentgrep.com/patent/US20200002210A1

## CPC

- C03B 19/1075: {by blowing, pressing, centrifuging, rolling or dripping}
- C03C 11/005: {obtained by leaching after a phase separation step}
- C04B 12/005: {Geopolymer cements, e.g. reaction products of aluminosilicates with alkali metal hydroxides or silicates}
- C04B 20/0036: {Microsized or nanosized}
- C04B 28/006: {containing mineral polymers, e.g. geopolymers of the Davidovits type}
- C04B 33/13: Compounding ingredients (C04B33/36, C04B35/71 take precedence {; pigments for ceramics C09C1/0009})
- C03B 19/107: {Forming hollow beads (chemical aspects C03C11/002)}
- C04B 14/044: {Polysilicates, e.g. geopolymers}
- C04B 20/1037: {obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds}
- C04B 2103/0071: {Phase-change materials, e.g. latent heat storage materials used in concrete compositions}
- C04B 2111/28: Fire resistance, i.e. materials resistant to accidental fires or high temperatures
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A high-strength geopolymer hollow microsphere, a preparation method thereof and a phase change energy storage microsphere are provided, including: dissolving sodium hydroxide, sodium silicate and spheroidizing aid in water to form a solution A, and adding active powder to the solution A, stirring and uniformly mixing to form a slurry B, adding the slurry B to an oil phase, stirring and dispersing into balls, filtering to obtain geopolymer microspheres I, washing the geopolymer microspheres I, and then carrying out a high-temperature calcination to obtain the high-strength geopolymer hollow microspheres II; using the high-strength geopolymer hollow microsphere as a carrier, absorbing a phase change material into the carrier, and mixing a microsphere carrying the phase change material with an epoxy resin, adding a powder dispersant and stirring to disperse the microsphere, after the epoxy resin is solidified, screening the superfluous powder dispersant to obtain the phase energy storage microsphere.

## Claims

### Claim 1

A method of preparing high-strength geopolymer hollow microspheres, comprising: dissolving sodium hydroxide (NaOH), sodium silicate (Na2SiO3.9H2O) and a spheroidizing aid in water to form a solution, adding active powder to the solution to obtain a first mixture, stirring and uniformly mixing the first mixture to form a slurry, adding the slurry to an oil phase dispersion medium to obtain a second mixture, stirring the second mixture to disperse the slurry into the oil phase dispersion medium to form balls, after the stirring, filtering the second mixture to obtain geopolymer microspheres, washing the geopolymer microspheres, and then carrying out a high-temperature calcination on the geopolymer microspheres to obtain the high-strength geopolymer hollow microspheres; wherein a mass percentage of the sodium hydroxide (NaOH), the sodium silicate (Na2SiO3.9H2O) and the spheroidizing aid is (10-40%):(20-60%):(20-60%), a mass ratio of the water to the active powder is 1:2-1, the slurry accounts for 5%-50% of a volume of the oil phase dispersion medium, a temperature of the high-temperature calcination is 800-1500° C., and a time of the high-temperature calcination is 1-8 hours.

### Claim 2 (depends on 1)

The method of preparing the high-strength geopolymer hollow microspheres of claim 1, wherein the mass percentage of the sodium hydroxide (NaOH), the sodium silicate (Na2SiO3.9H2O) and the spheroidizing aid is (12-20%):(40-60%):(30-50%), the mass ratio of the water to the active powder is 1:1.5-1, and the slurry B accounts for 10%-40% of the volume of the oil phase dispersion medium.

### Claim 3 (depends on 1)

The method of preparing the high-strength geopolymer hollow microspheres of claim 1, wherein the temperature of the high-temperature calcination is 850-1200° C., and the time of the high-temperature calcination is 1-2 hours.

### Claim 4 (depends on 1)

The method of preparing the high-strength geopolymer hollow microspheres of claim 1, wherein the spheroidizing aid is a sodium salt and a potassium salt.

### Claim 5 (depends on 4)

The method of preparing the high-strength geopolymer hollow microspheres of claim 4, wherein the sodium salt comprises one or more selected from the group consisting of sodium carbonate, sodium chloride, sodium nitrate, and sodium sulfate; and the potassium salt comprises one or more selected from the group consisting of potassium chloride, potassium carbonate, and potassium sulfate.

### Claim 6 (depends on 1)

The method of preparing the high-strength geopolymer hollow microspheres of claim 1, wherein the active powder comprises one or more selected from the group consisting of fly ash, metakaolin and slag, and the active powder has a mesh number of 500-1000 mesh.

### Claim 7 (depends on 1)

The method of preparing the high-strength geopolymer hollow microspheres of claim 1, wherein the oil phase dispersion medium is a corn oil, a soybean oil, a peanut oil, a kerosene, a castor oil, or a rapeseed oil.

### Claim 8 (depends on 1)

The method of preparing the high-strength geopolymer hollow microspheres of claim 1, wherein a temperature of the oil phase dispersion medium is 50-90° C.

### Claim 9 (depends on 1)

The method of preparing the high-strength geopolymer hollow microspheres of claim 1, wherein a stirring speed of dispersing the slurry into the oil phase dispersion medium is 400-1000 r/min, and a stirring time is 0.5-3 hours.

### Claim 10 (depends on 1)

A high-strength geopolymer hollow microsphere prepared by the method of preparing the high-strength geopolymer hollow microspheres of claim 1.

### Claim 11

(canceled)

### Claim 12 (depends on 10)

A method of preparing a phase change energy storage microsphere, comprising: using the high-strength geopolymer hollow microsphere of claim 10 as a carrier, absorbing a phase change material into a hollow of the carrier by a vacuum suction, and mixing a microsphere carrying the phase change material with an epoxy resin to make the epoxy resin coat on a surface of the microsphere carrying the phase change material, adding a powder dispersant and stirring to disperse the microsphere carrying the phase change material, after the epoxy resin is solidified, screening a superfluous powder dispersant to obtain the phase energy storage microsphere.

### Claim 13 (depends on 12)

The method of preparing the phase change energy storage microsphere of claim 12, wherein the phase change material is paraffin wax having a carbon number of 18-30.

### Claim 14 (depends on 12)

The method of preparing the phase change energy storage microsphere of claim 12, wherein an addition amount of the phase change material is 10%-20% of a mass of the high-strength geopolymer hollow microsphere, and an addition amount of the epoxy resin is 5%-15% of the mass of the high-strength geopolymer hollow microsphere.

### Claim 15 (depends on 12)

The method of preparing the phase change energy storage microsphere of claim 12, wherein the epoxy resin is an ambient cured waterborne epoxy resin or an ambient cured oily epoxy resin.

### Claim 16 (depends on 12)

The method of preparing the phase change energy storage microsphere of claim 12, wherein a component of the powder dispersant is one or more selected from the group consisting of ultrafine calcium carbonate, silicon powder, metakaolin, graphite powder and ultrafine slag.

### Claim 17 (depends on 12)

The method of preparing the phase change energy storage microsphere of claim 12, wherein the powder dispersant has a particle size of 1000-2000 mesh.

### Claim 18 (depends on 12)

The method of preparing the phase change energy storage microsphere of claim 12, wherein a stirring speed of dispersing the microsphere carrying the phase change material in the powder dispersant is 100-500 r/min, and a stirring time is 0.5-2 hours.

### Claim 19 (depends on 10)

The high-strength geopolymer hollow microsphere of claim 10, wherein the mass percentage of the sodium hydroxide (NaOH), the sodium silicate (Na2SiO3.9H2O) and the spheroidizing aid is (12-20%):(40-60%):(30-50%), the mass ratio of the water to the active powder is 1:1.5-1, and the slurry B accounts for 10%-40% of the volume of the oil phase dispersion medium.

### Claim 20 (depends on 10)

The high-strength geopolymer hollow microsphere of claim 10, wherein the temperature of the high-temperature calcination is 850-1200° C., and the time of the high-temperature calcination is 1-2 hours.

### Claim 21 (depends on 10)

The high-strength geopolymer hollow microsphere of claim 10, wherein the spheroidizing aid is a sodium salt and a potassium salt.