# US 2019/0379344 A1 · Film bulk acoustic wave resonators and fabrication methods thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0379344 A1
- Document ID: US20190379344A1
- Status: Published application
- Kind: A1
- Application number: 16/395,002
- Filed: 2019-04-25
- Published: 2019-12-12
- Earliest claimed: 2018-06-08
- Assignees: Shanghai Jadic Optoelectronics Technology Co., Ltd.
- Applicants: Shanghai Jadic Optoelectronics Technology Co., Ltd.
- Inventors: Xiaochuan WANG
- Web page: https://patentgrep.com/patent/US20190379344A1

## CPC

- H03H 9/02118: {of lateral leakage between adjacent resonators}
- H03H 9/02157: {Dimensional parameters, e.g. ratio between two dimension parameters, length, width or thickness}
- H03H 3/02: for the manufacture of piezoelectric or electrostrictive resonators or networks (H03H3/08 takes precedence)
- H03H 9/02015: {Characteristics of piezoelectric layers, e.g. cutting angles}
- H03H 9/02102: {of temperature influence (cutting angles H03H9/02015)}
- H03H 9/1021: {the BAW device being of the cantilever type}
- H03H 9/1042: {the enclosure being defined by a housing formed by a cavity in a resin}
- H03H 9/105: {the enclosure being defined by a cover cap mounted on an element forming part of the BAW device}
- H03H 9/13: for networks consisting of piezoelectric or electrostrictive materials (for networks using surface acoustic waves H03H9/145)
- H03H 9/173: {Air-gaps}
- H03H 9/562: {comprising a ceramic piezoelectric layer}
- H03H 9/564: {implemented with thin-film techniques}
- H10N 30/06: Forming electrodes or interconnections, e.g. leads or terminals
- H10N 30/082: by etching, e.g. lithography
- H10N 30/704: {based on piezoelectric or electrostrictive films or coatings}
- H10N 30/877: {Conductive materials}
- H03H 2003/021: {the resonators or networks being of the air-gap type}
- H03H 2003/023: {the resonators or networks being of the membrane type}
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A film bulk acoustic wave resonator (BAWR) includes a first substrate; a first insulating material layer; and a first cavity, formed in the first insulating material layer. The film BAWR also includes a first electrode containing a first electrode cavity; a second electrode containing a second electrode cavity; and a first piezoelectric oscillation plate, sandwiched between the first electrode and the second electrode. Without having any parallel edges, the boundary of the first piezoelectric oscillation plate is entirely enclosed in the first cavity boundary, and at least includes an overlapping region of the boundary of the first electrode cavity and the boundary of the second electrode cavity. The film BAWR further includes a plurality of second and third piezoelectric oscillation plates, disposed between the first electrode and the second electrode to receive and absorb vibration energy transmitted out through vibration waves induced in the first electrode and the second electrode.

## Claims

### Claim 1

A film bulk acoustic wave resonator (BAWR), comprising:
a first substrate;
a first insulating material layer, formed on the first substrate;
a first cavity, formed in the first insulating material layer with an opening facing away from the first substrate, wherein the first cavity forms a first cavity boundary at a surface of the first insulating material layer;
a first electrode and a second electrode stacked on the first insulating material layer, wherein the first electrode includes a first electrode cavity formed above the first cavity, and the second electrode includes a second electrode cavity formed above the first cavity;
a first piezoelectric oscillation plate sandwiched between the first electrode and the second electrode, and having a first piezoelectric-oscillation-plate boundary, wherein at least a portion of the first piezoelectric-oscillation-plate boundary is an overlapping region of a portion of a boundary of the first electrode cavity and a portion of a boundary of the second electrode cavity, and the first piezoelectric-oscillation-plate boundary has an irregular polygonal shape without having any two edges parallel to each other, and is entirely enclosed in the first cavity boundary;
a plurality of second piezoelectric oscillation plates and a plurality of third piezoelectric oscillation plates disposed at least partially above the first cavity and sandwiched between the first electrode and the second electrode, wherein the plurality of second piezoelectric oscillation plates and the plurality of third piezoelectric oscillation plates receive and absorb a portion of vibration energy transmitted out through vibration waves induced in the first electrode and the second electrode.

### Claim 2 (depends on 1)

The film BAWR according to claim 1, wherein:
the plurality of second piezoelectric oscillation plates have a second piezoelectric-oscillation-plate boundary including at least one pair of parallel edges; and
the plurality of third piezoelectric oscillation plates have a third piezoelectric-oscillation-plate boundary including at least one pair of parallel edges.

### Claim 3 (depends on 2)

The film BAWR according to claim 2, wherein:
any portion of the second piezoelectric-oscillation-plate boundary is not parallel to any portion of the first piezoelectric-oscillation-plate boundary;
the plurality of second piezoelectric oscillation plates and the second piezoelectric-oscillation-plate boundary are entirely enclosed in the first cavity boundary;
any portion of the second piezoelectric-oscillation-plate boundary is not parallel to any portion of the first cavity boundary;
any portion of the third piezoelectric-oscillation-plate boundary is not parallel to any portion of the first piezoelectric-oscillation-plate boundary;
the plurality of third piezoelectric oscillation plates and the third piezoelectric-oscillation-plate boundary are entirely enclosed in the first cavity boundary; and
any portion of the third piezoelectric-oscillation-plate boundary is not parallel to any portion of the first cavity boundary.

### Claim 4 (depends on 3)

The film BAWR according to claim 3, wherein:
the plurality of second piezoelectric oscillation plates and/or the plurality of third piezoelectric oscillation plates provide boundary mechanical support.

### Claim 5 (depends on 2)

The film BAWR according to claim 2, further including a second insulating material layer disposed above the second electrode, wherein:
a second cavity, with an opening facing the first piezoelectric oscillation plate, is formed in the second insulating material layer; and
the second cavity forms a second cavity boundary at a surface of the second insulating material layer.

### Claim 6 (depends on 5)

The film BAWR according to claim 5, wherein:
the first piezoelectric oscillation plate and the first piezoelectric-oscillation-plate boundary are entirely enclosed in the second cavity boundary;
any position of the second piezoelectric-oscillation-plate boundary is not parallel to any portion of the second cavity boundary, and/or any position of the third piezoelectric-oscillation-plate boundary is not parallel to any portion of the second cavity boundary; and
the plurality of second piezoelectric oscillation plates and the second piezoelectric-oscillation-plate boundary are entirely enclosed in the second cavity boundary, and/or the plurality of third piezoelectric oscillation plates and the third piezoelectric-oscillation-plate boundary are entirely enclosed in the second cavity boundary.

### Claim 7 (depends on 1)

The film BAWR according to claim 1, wherein:
the first electrode and the second electrode are made of a material including at least one of Al, Cu, Ni, W, Ti, Mo, Ag, Au, and Pt; and
the first piezoelectric oscillation plate, the plurality of second piezoelectric oscillation plates, and the plurality of third piezoelectric oscillation plates are made of a material including at least one of piezoelectric crystal or piezoelectric ceramic.

### Claim 8 (depends on 7)

The film BAWR according to claim 7, wherein:
the first piezoelectric oscillation plate, the plurality of second piezoelectric oscillation plates, and the plurality of third piezoelectric oscillation plates are made of a material including at least one of quartz, lithium gallate, lithium germanate, titanium germanate, lithium niobate, lithium tantalate, aluminum nitride, zinc oxide, and lead-zinc titanite.

### Claim 9 (depends on 1)

The film BAWR according to claim 1, further including:
a first temperature compensation film formed above the first cavity and on a surface of the first electrode far away from the first piezoelectric oscillation plate, wherein:
the first temperature compensation film is made of a material including at least one of oxide, nitride, and carbide,
a thermal expansion coefficient of the first temperature compensation film is lower than thermal expansion coefficients of the first electrode and the second electrode.

### Claim 10 (depends on 1)

The film BAWR according to claim 1, further including:
a second temperature compensation film formed above the first cavity and on a surface of the second electrode far away from the first piezoelectric oscillation plate, wherein:
the second temperature compensation film is made of a material including at least one of oxide, nitride, and carbide,
a thermal expansion coefficient of the second temperature compensation film is lower than thermal expansion coefficients of the first electrode and the second electrode.

### Claim 11

A method for fabricating a film BAWR, comprising:
forming a first insulating material layer on a first substrate;
forming a first cavity in the first insulating material layer with an opening facing away from the first substrate;
sequentially forming a second conductive film, a piezoelectric film, and a first conductive film on a sacrificial substrate;
etching a portion of the first conductive film and the piezoelectric film close to an end of the sacrificial substrate to expose a portion of the second conductive film, a remaining portion of the first conductive film becoming a first electrode, a plurality of trenches formed through the first conductive film and the piezoelectric film becoming a plurality of first electrode cavities, and a portion of the piezoelectric film located between adjacent first electrode cavities becoming a plurality of second piezoelectric oscillation plates;
bonding the first substrate and the sacrificial substrate together by bonding the first insulating material layer to the first conductive film, wherein after bonding, the plurality of first electrode cavities are located above the first cavity;
removing the sacrificial substrate; and
etching a portion of the second conductive film and a portion of the piezoelectric film close to an end of the sacrificial substrate opposite to the end where the plurality of first electrode cavities are formed to expose a portion of the first electrode, a remaining portion of the second conductive film becoming a second electrode, a remaining portion of the piezoelectric film sandwiched between the first electrode and the second electrode becoming a first piezoelectric oscillation plate, a plurality of trenches formed through the second conductive film and the piezoelectric film becoming a plurality of second electrode cavities, and a portion of the piezoelectric film located between adjacent second electrode cavities becoming a plurality of third piezoelectric oscillation plates, wherein:
the first piezoelectric oscillation plate has a first piezoelectric-oscillation-plate boundary,
at least a portion of the first piezoelectric-oscillation-plate boundary is an overlapping region of a portion of a boundary of the first electrode cavity and a portion of a boundary of the second electrode cavity,
the first piezoelectric-oscillation-plate boundary has an irregular polygonal shape without having any two edges parallel to each other, and is entirely enclosed in the first cavity boundary, and
the plurality of second piezoelectric oscillation plates and the plurality of third piezoelectric oscillation plates receive and absorb a portion of vibration energy transmitted out through vibration waves induced in the first electrode and the second electrode.

### Claim 12 (depends on 11)

The method for fabricating the film BAWR according to claim 11, wherein:
the plurality of second piezoelectric oscillation plates have a second piezoelectric-oscillation-plate boundary including at least one pair of parallel edges; and
the plurality of third piezoelectric oscillation plates have a third piezoelectric-oscillation-plate boundary including at least one pair of parallel edges.

### Claim 13 (depends on 11)

The method for fabricating the film BAWR according to claim 11, wherein:
any portion of the second piezoelectric-oscillation-plate boundary is not parallel to any portion of the first piezoelectric-oscillation-plate boundary;
the plurality of second piezoelectric oscillation plates and the second piezoelectric-oscillation-plate boundary are entirely enclosed in the first cavity boundary;
any portion of the second piezoelectric-oscillation-plate boundary is not parallel to any portion of the first cavity boundary;
any portion of the third piezoelectric-oscillation-plate boundary is not parallel to any portion of the first piezoelectric-oscillation-plate boundary;
the plurality of third piezoelectric oscillation plates and the third piezoelectric-oscillation-plate boundary are entirely enclosed in the first cavity boundary; and
any portion of the third piezoelectric-oscillation-plate boundary is not parallel to any portion of the first cavity boundary.

### Claim 14 (depends on 13)

The method for fabricating the film BAWR according to claim 13, wherein:
the plurality of second piezoelectric oscillation plates and/or the plurality of third piezoelectric oscillation plates provide boundary mechanical support.

### Claim 15 (depends on 11)

The method for fabricating the film BAWR according to claim 11, further including:
when forming the second conductive film, the piezoelectric film, and the first conductive film on the sacrificial substrate, forming a second temperature compensation film between the sacrificial substrate and the second conductive film, and a first temperature compensation film on the first conductive film;
prior to etching the portion of the first conductive film and the portion of the piezoelectric film to expose the second conductive film, etching a portion of the first temperature compensation film; and
prior to etching the portion of the second conductive film and the portion of the piezoelectric film to expose the first electrode, etching a portion of the second temperature compensation film.

### Claim 16 (depends on 11)

The method for fabricating the film BAWR according to claim 11, further including:
providing a second insulating material layer;
forming a second cavity in the second insulating material layer, wherein the second cavity forms a second cavity boundary at a surface of the second insulating material layer; and
bonding the second insulating material layer to the second electrode on the first substrate, wherein an opening of the second cavity faces the second electrode, and the first piezoelectric oscillation plate and the first piezoelectric-oscillation-plate boundary are entirely enclosed in the second cavity boundary.

### Claim 17 (depends on 16)

The method for fabricating the film BAWR according to claim 16, wherein:
any position of the second piezoelectric-oscillation-plate boundary is not parallel to any portion of the second cavity boundary, and/or any position of the third piezoelectric-oscillation-plate boundary is not parallel to any portion of the second cavity boundary; and
the plurality of second piezoelectric oscillation plates and the second piezoelectric-oscillation-plate boundary are entirely enclosed in the second cavity boundary, and/or the plurality of third piezoelectric oscillation plates and the third piezoelectric-oscillation-plate boundary are entirely enclosed in the second cavity boundary.

### Claim 18

A method for fabricating a film BAWR, comprising:
forming a first insulating material layer on a first substrate;
forming a first cavity in the first insulating material layer with an opening facing away from the first substrate;
forming a first sacrificial material layer in the first cavity, wherein a top surface of the first sacrificial material layer is leveled with a top surface of the first insulating material layer;
sequentially forming a first conductive film and a piezoelectric film on the first insulating material layer and the first sacrificial material layer;
etching a portion of the piezoelectric film and a portion of the first conductive film above the first sacrificial material layer to expose a portion of the first sacrificial material layer, a plurality of trenches formed through the piezoelectric film and the first conductive film becoming a plurality of first electrode cavities, a remaining portion of the first conductive film becoming a first electrode, and a portion of the piezoelectric film located between adjacent first electrode cavities becoming a plurality of second piezoelectric oscillation plates;
forming a second sacrificial material layer to fill the plurality of first electrode cavities;
forming a second conductive film on the piezoelectric film and the second sacrificial material layer;
etching a portion of the second conductive film and a portion of the piezoelectric film formed above the first sacrificial material layer to expose a portion of the first electrode, a remaining portion of the second conductive film becoming a second electrode, a remaining portion of the piezoelectric film sandwiched between the first electrode and the second electrode becoming a first piezoelectric oscillation plate, a plurality of trenches formed through the second conductive film and the piezoelectric film becoming a plurality of second electrode cavities, and a portion of the piezoelectric film located between adjacent second electrode cavities becoming a plurality of third piezoelectric oscillation plates; and
removing the first sacrificial material layer and the second sacrificial material layer, wherein:
the first piezoelectric oscillation plate has a first piezoelectric-oscillation-plate boundary,
at least a portion of the first piezoelectric-oscillation-plate boundary is an overlapping region of a portion of a boundary of the first electrode cavity and a portion of a boundary of the second electrode cavity,
the first piezoelectric-oscillation-plate boundary has an irregular polygonal shape without having any two edges parallel to each other, and the first piezoelectric-oscillation-plate boundary is entirely enclosed in the first cavity boundary, and
the plurality of second piezoelectric oscillation plates and the plurality of third piezoelectric oscillation plates receive and absorb a portion of vibration energy transmitted out through vibration waves induced in the first electrode and the second electrode.

### Claim 19 (depends on 18)

The method for fabricating the film BAWR according to claim 18, further including:
forming a second insulating material layer on a second substrate;
forming a second cavity in the second insulating material layer with an opening facing away from the second substrate; and
bonding the second substrate and the first substrate together by bonding the second insulating material layer to the first insulating material layer, wherein:
the first piezoelectric oscillation plate has a first piezoelectric-oscillation-plate boundary,
at least a portion of the first piezoelectric-oscillation-plate boundary is an overlapping region of a portion of a boundary of the first electrode cavity and a portion of a boundary of the second electrode cavity,
the first piezoelectric-oscillation-plate boundary has an irregular polygonal shape without having any two edges parallel to each other, and the first piezoelectric-oscillation-plate boundary is entirely enclosed in the first cavity boundary, and
the plurality of second piezoelectric oscillation plates and the plurality of third piezoelectric oscillation plates receive and absorb a portion of vibration energy transmitted out through vibration waves induced in the first electrode and the second electrode.

### Claim 20 (depends on 18)

The method for fabricating the film BAWR according to claim 18, further including:
providing a second insulating material layer;
forming a second cavity in the second insulating material layer, wherein the second cavity forms a second cavity boundary at a surface of the second insulating material layer; and
bonding the second insulating material layer to the second electrode on the first substrate, wherein an opening of the second cavity faces the second electrode, and the first piezoelectric oscillation plate and the first piezoelectric-oscillation-plate boundary are entirely enclosed in the second cavity boundary.