# US 2019/0379056 A1 · Materials and methods for components of lithium batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0379056 A1
- Document ID: US20190379056A1
- Status: Published application
- Kind: A1
- Application number: 16/433,944
- Filed: 2019-06-06
- Published: 2019-12-12
- Earliest claimed: 2018-06-07
- Assignees: Shenzhen Xworld Technology Limited
- Inventors: Lin Chen
- Web page: https://patentgrep.com/patent/US20190379056A1

## CPC

- H01M 4/381: {Alkaline or alkaline earth metals elements (H01M4/40 takes precedence)}
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/38: of elements or alloys
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to materials and methods for components of lithium batteries, such as metal anodes having a protective coating.

## Claims

### Claim 1

A metal anode having a protective coating comprising:
a metal layer comprising lithium, sodium, or potassium; and
a protective coating on the metal layer, wherein the protective coating comprises a composite material, and the composite material comprises an oxide or fluoride of lithium, sodium, or potassium.

### Claim 2 (depends on 1)

The metal anode of claim 1, wherein the composite material comprises lithium fluoride-lithium oxide (LiF—Li2O), lithium fluoride-lithium carbonate (LiF—Li2CO3), lithium fluoride-lithium hexafluorophosphate (LiF—LiPF6), lithium fluoride-lithium phosphate (LiF—LiPO4), lithium fluoride-lithium tetrafluoroborate (LiF—LiBF4), lithium fluoride-carbon fluoride (LiF—CF4), Li2O—Li2CO3, Li2O—LiF, Li2O—LiPO4, Li2O—LiBF4, Li2O—CF4, HfO2, LixHfO2, SiO2, LiF—NbO2, Li3N—AlN, LixSi3N4, LixNb3N4, where X≥0 or any combination of these materials.

### Claim 3 (depends on 1)

The metal anode of claim 1, wherein the composite material comprises (a) a lithium oxide-containing material when the metal layer comprises lithium; (b) a sodium oxide-containing material when the metal layer comprises sodium; or (c) a potassium oxide-containing material when the metal layer comprises potassium.

### Claim 4 (depends on 3)

The metal anode of claim 3, wherein the composite material comprises (a) Li2O—Li2CO3, Li2O—LiF, Li2O—LiPO4, Li2O—LiBF4, Li2O—CF4, or any combination of these materials when the metal layer comprises lithium; (b) Na2O—Na2CO3, Na2O—NaF, Na2O—NaPO4, Na2O—NaBF4, Na2O—CF4, or any combination of these materials when the metal layer comprises sodium, and (c) K2O—K2CO3, K2O—KF, K2O—KPO4, K2O—KBF4, K2O—CF4, or any combination of these materials when the metal layer comprises potassium.

### Claim 5 (depends on 1)

The metal anode of claim 1, wherein the protective layer comprises HfO2, MxHfO2, SiO2, MF-M2O, MF-M2CO3, MF-MPF6, MF-M3PO4, MF-MBF4, MF-CF4, MF-NbO2, M2O-M2CO3, M2O-MF, M2O-M3PO4, M2O-MBF4, M2O—CF4, M3N—AlN, M3N—AlN, MxSi3N4, MxNb3N4, or any combination thereof, where X≥1 and M is Li, Na, K, or a mixture thereof.

### Claim 6 (depends on 1)

The metal anode of claim 1, wherein the metal layer of the metal anode has a thickness of 10 μm to 150 μm.

### Claim 7 (depends on 1)

The metal anode of claim 1, wherein the protective coating has a thickness from 1 nm to 10 microns.

### Claim 8 (depends on 1)

The metal anode of claim 1, wherein the protective coating is formed on the metal layer by atomic layer deposition, plasma enhanced atomic layer deposition, chemical vapor deposition, plasma enhanced chemical vapor deposition, sputtering, physical vapor deposition, spinning coating, dip coating, or pulsed laser deposition.

### Claim 9

A lithium-free metal or carbon electrode for a lithium ion battery, the electrode comprising:
a metal or carbon layer;
a protective coating on the metal layer,
wherein the protective coating comprises aluminum oxide, titanium oxide, hafnium oxide, zirconium dioxide, lithium oxide, lanthanum oxide, zinc oxide, antimony tetroxide, antimony pentoxide, arsenic trioxide, arsenic pentoxide, barium oxide, bismuth oxide, bismuth oxide, calcium oxide, cerium oxide, cerium oxide, chromium oxide, chromium oxide, chromium oxide, chromium oxide, cobalt oxide, cobalt oxide, cobalt oxide, copper oxide, copper oxide, iron oxide, iron oxide, lead oxide, magnesium oxide, manganese oxide, mercury oxide, nickel oxide, rubidium oxide, silicon dioxide, silver oxide, thallium oxide, thallium oxide, thorium oxide, tin oxide, uranium oxide, tungsten oxide, selenium dioxide, tellurium dioxide, lithium sulfide, lithium nitride, lithium nitrate, lithium carbonate, lithium fluoride, lithium chloride, lithium bromide, lithium carbide, lithium borate, lithium sulfate, lithium hexafluorophosphate, lithium hydroxide, lithium tantalite, lithium iodide, lithium tetrakispentafluorophenyl borate, yttrium lithium fluoride, polyethylene glycol, gelatin, lithium hafnium oxide, a lithium fluoride-lithium carbonate composite or polytetrafluoroethylene, or any combination thereof.

### Claim 10 (depends on 9)

The electrode of claim 9, wherein the metal layer is selected from copper, nickel, titanium, carbon, graphite, tantalum (Ta) foil, tungsten (W) foil, vanadium (V) foil, or stainless steel or any combination thereof.

### Claim 11 (depends on 9)

The electrode of claim 9, wherein the protective coating is formed by atomic layer deposition, chemical vapor deposition, plasma enhanced chemical vapor deposition, physical vapor deposition, pulsed laser deposition or plasma enhanced atomic layer deposition.

### Claim 12 (depends on 9)

The electrode of claim 9, wherein the thickness of the protective coating can range from 0.1 nanometers to 50 microns, with particular interest of the thickness from 0.5 nm to 10 microns. The metal foil thickness can range from 0.1 μm to 50 μm.

### Claim 13

A method of preparing a thin layer comprising lithium, the method comprising
a) applying one or more interlayer material onto a substrate to form an interlayer material coated substrate;
b) heating the interlayer material coated substrate to an elevated temperature; and
c) applying one or more metal layers onto the interlayer material coated substrate, wherein the metal layer comprises lithium.

### Claim 14 (depends on 13)

The method of claim 13, wherein the interlayer material comprises aluminum metal, tin metal, indium metal, zinc metal, nickel metal, molybdenum metal and titanium metal, or any metal oxide or metal nitride, such as Al2O3, CuO, ZnO, TiO2, HfO2, aluminum nitride (AlN), Li2O, SiO2, NbO2, Fe2O3, Fe3O4, FeO, MnO2, Li3N, Li2CO3, Si3N4 and Nb3N4, or any organic materials such as carbonates and ester, or silicon, or any combination thereof.

### Claim 15 (depends on 13)

The method of claim 13, wherein the substrate comprises copper (Cu) foil, nickel (Ni) foil, stainless steel foil, titanium (Ti) foil, carbon or graphite clothing, tantalum (Ta) foil, tungsten (W) foil, vanadium (V) foil, or a polymer film.

### Claim 16 (depends on 13)

The method of claim 13, wherein the interlayer material has a thickness of 0.1 nm to 50 μm, and the substrate has a thickness of 1.0 μm to 45 μm.

### Claim 17 (depends on 13)

The method of claim 13, wherein the metal layer has a thickness of from 10 nm to 100 microns (μm).

### Claim 18 (depends on 13)

The method of claim 13, wherein the elevated temperature is between 100 and 250° C.

### Claim 19 (depends on 13)

The method of claim 13, wherein the metal layer is applied onto the interlayer material coated substrate by pressing, rolling, printing or extruding.

### Claim 20 (depends on 13)

The method of claim 13, wherein the interlayer material is applied to the substrate by chemical vapor deposition, plasma enhanced chemical vapor deposition, spraying, 3D printing, sputtering, physical vapor deposition, atomic layer deposition, plasma enhanced atomic layer deposition, spinning coating, dip coating, pulsed laser deposition, or any combination thereof.