# US 2019/0379038 A1 · Transition metal-containing composite hydroxide and production method thereof, and production method of positive electrode active material for nonaqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0379038 A1
- Document ID: US20190379038A1
- Status: Published application
- Kind: A1
- Application number: 16/461,072
- Filed: 2017-11-21
- Published: 2019-12-12
- Earliest claimed: 2016-11-22
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Takahiro TOMA; Hiroko SENBA; Taira AIDA; Tetsufumi KOMUKAI
- Web page: https://patentgrep.com/patent/US20190379038A1

## CPC

- H01M 4/364: {as mixtures}
- C01G 53/502: containing lithium and cobalt
- C01G 53/84: Hydroxides
- C30B 7/14: the crystallising materials being formed by chemical reactions in the solution
- C30B 29/22: Complex oxides
- H01M 4/366: {as layered products}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2004/03: obtained by SEM
- C01P 2004/20: extending in two dimensions, e.g. plate-like
- C01P 2004/50: Agglomerated particles
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2004/82: two phases having the same anion, e.g. both oxidic phases
- H01M 2004/028: {Positive electrodes}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A transition metal-containing composite hydroxide comprises secondary particles having: a center portion of fine primary particles; and an outer-shell portion having a high-density layer of plate-shaped primary particles formed outside the center portion, a low-density layer of the fine primary particles formed outside the high-density layer, and an outer-shell layer of the plate-shaped primary particles formed outside the low-density layer. The composite hydroxide is obtained by a method comprising a nucleation step in an oxidizing atmosphere and a particle growth step, the particle growth step comprising: a first stage of maintaining the oxidizing atmosphere; a second stage of switching to and maintaining a non-oxidizing atmosphere; a third stage of switching again to and maintaining the oxidizing atmosphere; and a fourth stage of switching again to and maintaining the non-oxidizing atmosphere.

## Claims

### Claim 1

A transition metal-containing composite hydroxide comprising secondary particles respectively formed by aggregates of plate-shaped primary particles and fine primary particles having a smaller particle size than the plate-shaped primary particles;
the secondary particles comprising: a center portion constructed by the fine primary particles; and an outer-shell portion having a high-density layer formed on the outside of the center portion and constructed by the plate-shaped primary particles, a low-density layer formed on the outside of the high-density layer and constructed by the fine primary particles, and an outer-shell layer formed on the outside of the low-density layer and constructed by the plate-shaped primary particles.

### Claim 2 (depends on 1)

The transition metal-containing composite hydroxide according to claim 1, wherein the average ratio of the outer diameter of the center portion with respect to the particle size of the secondary particles is within a range of 35% to 85%; the average ratio of the sum of the thicknesses of the high-density layer and the outer shell layer with respect to the particle size of the secondary particles is within a range of 5% to 30%; the average ratio of the thickness of the low-density layer with respect to the particle size of the secondary particles is within a range of 2% to 20%; and the ratio of respective thicknesses of the high-density layer and the outer-shell layer with respect to the particle size of the secondary particles is within a range of 2.5% to 15%.

### Claim 3 (depends on 1)

The transition metal-containing composite hydroxide according to claim 1, wherein the outer-shell portion further comprises between the low-density layer and the outer-shell layer: a second high-density layer formed on the outside of the low-density layer and constructed by the plate-shaped primary particles; and a second low-density layer formed on the outside of the second high-density layer and constructed by the fine primary particles.

### Claim 4 (depends on 3)

The transition metal-containing composite hydroxide according to claim 3, wherein the average ratio of the outer diameter of the center portion with respect to the particle size of the secondary particles is within a range of 35% to 80%; the average ratio of the sum of the thicknesses of the high-density layer, the second high-density layer, and the outer-shell layer with respect to the particle size of the secondary particles is within a range of 8% to 30%; the average ratio of the sum of the thicknesses of the low-density layer and the second low-density layer with respect to the particle size of the secondary particles is within a range of 2% to 20%; the ratio of the respective thicknesses of the high-density layer, the second high-density layer, and the outer-shell layer is 2.5% to 15%; and the ratio of the respective thicknesses of the low-density layer and the second low-density layer is 1% to 10%.

### Claim 5 (depends on 1)

The transition metal-containing composite hydroxide according to claim 1, wherein the average particle size of the plate-shaped primary particles is within a range of 0.3 μm to 3 μm, and the average primary particle size of the fine primary particles is smaller than the average particle size of the plate-shaped primary particles and is within a range of 0.01 μm to 0.3 μm.

### Claim 6 (depends on 1)

The transition metal-containing composite hydroxide according to claim 1, wherein the average particle size of the secondary particles is within a range of 1 μm to 15 μm, and the value of [(d90-d10)/average particle size] as an index indicating the spread of the particle size distribution of the secondary particles is 0 .65 or less.

### Claim 7 (depends on 1)

The transition metal-containing composite hydroxide according to claim 1 having a composition represented by a general formula (A): NixMnyCozMt(OH)2+a (where x+y+z+t=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0≤t≤0.1, 0≤a≤0.5, and M is one or more additional element selected from Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, Ta, and W).

### Claim 8 (depends on 7)

The transition metal-containing composite hydroxide according to claim 7, wherein the additional element M is uniformly distributed inside the secondary particles of the transition metal composite hydroxide, and/or a surface of the secondary particles of the transition metal composite hydroxide is coated by a compound that includes the additional element M.

### Claim 9

A method for producing a transition metal-containing composite hydroxide as a precursor of a positive electrode active material for a secondary battery, by mixing a raw material aqueous solution including at least a transition metal element and an aqueous solution including a complexing agent to form a reaction aqueous solution, and performing a crystallization reaction, the method comprising:
a nucleation step in which nucleation is performed in an oxidizing atmosphere in which the pH value at a standard liquid temperature of 25° C. of the reaction aqueous solution is adjusted to be within a range of 12.0 to 14.0, and the oxygen concentration exceeds 5% by volume; and
a particle growth step in which the pH value at a standard liquid temperature 25° C. of the reaction aqueous solution including the nuclei obtained in the nucleation step is adjusted to lower than the pH value of the nucleation step and to be within a range of 10.5 to 12.0 to cause to growth of the nuclei; and
the particle growth step comprising:
a first stage of maintaining the oxidizing atmosphere from the start of the particle growth step;
a second stage after the first stage of switching from the oxidizing atmosphere to a non-oxidizing atmosphere in which the oxygen concentration is 5% by volume or less, and maintaining the non-oxidizing atmosphere;
a third stage after the second stage of switching from the non-oxidizing atmosphere to the oxidizing atmosphere, and maintaining the oxidizing atmosphere; and
a fourth stage after the third stage of switching from the oxidizing atmosphere to the non-oxidizing atmosphere, and maintaining the non-oxidizing atmosphere.

### Claim 10 (depends on 9)

The method for producing a transition metal-containing composite hydroxide according to claim 9, wherein the time of the first stage is within a range of 0.5% to 20% with respect to the total time of the particle growth step; the time of the second stage is within a range of 10% to 80% with respect to the total time of the particle growth step; the time of the third stage is within a range of 2% to 30% with respect to the total time of the particle growth step; and the time of the fourth stage is within a range of 10% to 80% with respect to the total time of the particle growth step.

### Claim 11 (depends on 9)

The method for producing a transition metal-containing composite hydroxide according to claim 9 further comprising:
a fifth stage after the fourth stage of switching from the non-oxidizing atmosphere to the oxidizing atmosphere, and maintaining the oxidizing atmosphere; and
a sixth stage after the fifth stage of switching from the oxidizing atmosphere to the non-oxidizing atmosphere, and maintaining the non-oxidizing atmosphere.

### Claim 12 (depends on 11)

The method for producing a transition metal-containing composite hydroxide according to claim 11, wherein the time of the first stage is within a range of 0.5% to 20% with respect to the total time of the particle growth step; the time of the second stage is within a range of 10% to 75% with respect to the total time of the particle growth step; the time of the third stage is within a range of 2% to 30% with respect to the total time of the particle growth step; the time of the fourth stage is within a range of 10% to 75% with respect to the total time of the particle growth step; the time of the fifth stage is within a range of 2% to 30% with respect to the total time of the particle growth step; and the time of the sixth stage is within a range of 10% to 75% with respect to the total time of the particle growth step.

### Claim 13 (depends on 9)

The method for producing a transition metal-containing composite hydroxide according to claim 9 wherein the transition metal-containing composite hydroxide has a composition represented by a general formula (A): NixMnyCozMt(OH)2+a (where x+y+z+t=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0≤t≤0.1, 0≤a≤0.5, and M is one or more additional element selected from Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, Ta, and W).

### Claim 14 (depends on 13)

The method for producing a transition metal-containing composite hydroxide according to claim 13, wherein after the particle growth step, a coating step is provided for coating the surface of the transition metal-containing composite hydroxide with a compound that includes the additional element M.

### Claim 15 (depends on 1)

A method for producing a positive electrode active material for a nonaqueous electrolyte secondary battery, comprising:
a mixing step of mixing a transition metal-containing composite hydroxide according to claim 1 and a lithium compound to form a lithium mixture; and
a firing step of firing the lithium mixture in an oxidizing atmosphere at a temperature within a range of 650° C. to 1000° C. to obtain a positive electrode active material for a nonaqueous electrolyte secondary battery constructed by a lithium transition metal-containing composite oxide.

### Claim 16 (depends on 15)

The method for producing a positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 15, wherein the mixing amount of the lithium compound is adjusted so that the ratio of the number of atoms of lithium included in the lithium mixture with respect to the total number of atoms of the metal elements other than lithium is within a range of 0.95 to 1.5.

### Claim 17 (depends on 15)

The method for producing a positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 15 further comprising a heat treatment step before the mixing step of heat treating the transition metal composite hydroxide at a temperature within a range of 105° C. to 750° C.

### Claim 18 (depends on 15)

The method for producing a positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 15, wherein the lithium transition metal-containing composite oxide is represented by a general formula (B): Li1+uNixMnyCozMtO2 (where −0.05≤u≤0.50, x+y+z+t=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0≤t≤0.1, and M is at least one or more additional element selected from among Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, Ta, and W).