# US 2019/0379037 A1 · High performance cathode active material for lithium ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0379037 A1
- Document ID: US20190379037A1
- Status: Published application
- Kind: A1
- Application number: 16/006,009
- Filed: 2018-06-12
- Published: 2019-12-12
- Earliest claimed: 2018-06-12
- Inventors: Mehran Javanbakht
- Web page: https://patentgrep.com/patent/US20190379037A1

## CPC

- H01M 4/364: {as mixtures}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/587: for inserting or intercalating light metals
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/028: {Positive electrodes}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A cathode active material for use in high-performance lithium-ion battery, is disclosed. The cathode active material comprises a lithium iron phosphate/sulfonated graphene oxide (LFP/SG) nanocomposite material. The molar ratio of sulfonated graphene oxide (SG) to lithium iron phosphate (LFP) in the cathode active material is 0.1:1. The cathode active material is synthesized by microwave-assisted hydrothermal method. The high-performance lithium-ion battery comprises an anode plate, a cathode plate, a separator between the anode plate and the cathode plate, and a non-aqueous electrolyte solution. The cathode plate is composed of a layer of cathode active material, and the cathode active material is lithium iron phosphate/sulfonated graphene oxide (LFP/SG) nanocomposite material. The lithium iron phosphate/sulfonated graphene oxide (LFP/SG) nanocomposite material used for lithium-ion battery possess high rate capability, capacity and cycle stability.

## Claims

### Claim 1

A high-performance lithium-ion battery, comprising:
an anode plate, a cathode plate, a separator between the anode plate and the cathode plate, and a non-aqueous electrolyte solution, wherein the cathode plate is composed of a layer of cathode active material, wherein the cathode active material is lithium iron phosphate/sulfonated graphene oxide (LFP/SG) nanocomposite material.

### Claim 2 (depends on 1)

The battery of claim 1, wherein the molar ratio of sulfonated graphene oxide (SG) to lithium iron phosphate (LFP) in said cathode active material is 0.1:1.

### Claim 3 (depends on 1)

The battery of claim 1, wherein said cathode active material is synthesized by microwave-assisted hydrothermal method.

### Claim 4 (depends on 1)

The battery of claim 1, wherein the discharge capacity of said cathode active material is 168 mAh g−1 at 0.2 C rate.

### Claim 5 (depends on 1)

The battery of claim 1, wherein the discharge capacity of said cathode active material is 149 mAh g−1 at 2 C rate.

### Claim 6 (depends on 1)

The battery of claim 1, wherein the discharge capacity of said cathode active material is 113 mAh g−1 at 20 C rate.

### Claim 7 (depends on 1)

The battery of claim 1, wherein the discharge capacity of said cathode active material is 93 mAh g−1 at 30 C rate.

### Claim 8

A cathode active material for a lithium-ion battery, comprising:
a lithium iron phosphate/sulfonated graphene oxide (LFP/SG) nanocomposite material.

### Claim 9 (depends on 8)

The cathode active material of claim 8, wherein the molar ratio of sulfonated graphene oxide (SG) to lithium iron phosphate (LFP) in said cathode active material is 0.1:1.

### Claim 10 (depends on 8)

The cathode active material of claim 8, is synthesized by microwave-assisted hydrothermal method.

### Claim 11 (depends on 8)

The cathode active material of claim 8, wherein the discharge capacity of said cathode active material is 168 mAh g−1 at 0.2 C rate.

### Claim 12 (depends on 8)

The cathode active material of claim 8, wherein the discharge capacity of said cathode active material is 149 mAh g−1 at 2 C rate.

### Claim 13 (depends on 8)

The cathode active material of claim 8, wherein the discharge capacity of said cathode active material is 113 mAh g−1 at 20 C rate.

### Claim 14 (depends on 8)

The cathode active material of claim 8, wherein the discharge capacity of said cathode active material is 93 mAh g−1 at 30 C rate.