# US 2019/0378975 A1 · Fabrication of electrodes for memory cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0378975 A1
- Document ID: US20190378975A1
- Status: Published application
- Kind: A1
- Application number: 16/001,795
- Filed: 2018-06-06
- Published: 2019-12-12
- Earliest claimed: 2018-06-06
- Assignees: Micron Technology, Inc.
- Applicants: Micron Technology, Inc.
- Inventors: Pengyuan Zheng; Yongjun J. Hu; Yao Jin; Hongqi Li; Andrea Gotti
- Web page: https://patentgrep.com/patent/US20190378975A1

## CPC

- H10N 70/8413: {adapted for resistive heating}
- H10B 63/24: {of the Ovonic threshold switching type}
- H10B 63/80: {Arrangements comprising multiple bistable or multi-stable switching components of the same type on a plane parallel to the substrate, e.g. cross-point arrays}
- H10N 70/011: {Manufacture or treatment of multistable switching devices}
- H10N 70/20: Multistable switching devices, e.g. memristors
- H10N 70/231: {based on solid-state phase change, e.g. between amorphous and crystalline phases, Ovshinsky effect}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/841: {Electrodes}
- H10N 70/882: {Compounds of sulfur, selenium or tellurium, e.g. chalcogenides}
- H10N 70/8825: {Selenides, e.g. GeSe}
- H10N 70/8828: {Tellurides, e.g. GeSbTe}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

Methods, systems, and devices for fabrication of memory cells are described. An electrode layer may have an initial thickness variation after being formed. The electrode layer may be smoothened prior to forming additional layers of a memory cell, thus decreasing the thickness variation. The subsequent layer fabricated may have a thickness variation that may be dependent on the thickness variation of the electrode layer. By decreasing the thickness variation of the electrode layer prior to forming the subsequent layer, the subsequent layer may also have a decreased thickness variation. The decreased thickness variation of the subsequent layer may impact the electrical behavior of memory cells formed from the subsequent layer. In some cases, the decreased thickness variation of the subsequent layer may allow for more predictable voltage thresholds for such memory cells, thus increasing the read windows for the memory cells.

## Claims

### Claim 1

An apparatus, comprising:
a first access line for a memory cell;
a first electrode for the memory cell, the first electrode disposed above the first access line and comprising oxidized carbon; and
an active component for the memory cell, the active component in contact with the first electrode and comprising chalcogenide.

### Claim 2 (depends on 1)

The apparatus of claim 1, wherein the oxidized carbon is oxidized based at least in part on a chemical-mechanical planarization (CMP) process associated with the first electrode.

### Claim 3 (depends on 2)

The apparatus of claim 2, wherein the oxidized carbon is oxidized based at least in part on breaking a vacuum seal in association with the CMP process.

### Claim 4 (depends on 1)

The apparatus of claim 1, wherein the active component for the memory cell comprises a selection component, a storage component, or a combination thereof for the memory cell.

### Claim 5 (depends on 1)

The apparatus of claim 1, further comprising:
a second electrode for the memory cell; and
a second active component for the memory cell, the second active component in contact with the second electrode and comprising chalcogenide.

### Claim 6 (depends on 5)

The apparatus of claim 5, wherein:
the first electrode comprises a first surface in contact with the active component, the first surface having a first roughness; and
the second electrode comprises a second surface in contact with the second active component, the second surface having a second roughness that is greater than the first roughness.

### Claim 7 (depends on 5)

The apparatus of claim 5, wherein:
the active component comprises a first chalcogenide material; and
the second active component comprises a second chalcogenide material, the second chalcogenide material different from the first chalcogenide material.

### Claim 8 (depends on 5)

The apparatus of claim 5, wherein the active component and the second active component comprise a same chalcogenide material.

### Claim 9 (depends on 5)

The apparatus of claim 5, wherein the second electrode comprises oxidized carbon.

### Claim 10 (depends on 5)

The apparatus of claim 5, further comprising:
a third electrode for the memory cell, the third electrode in contact with the second active component; and
a second access line for the memory cell.

### Claim 11 (depends on 10)

The apparatus of claim 10, wherein the third electrode comprises oxidized carbon.

### Claim 12 (depends on 1)

The apparatus of claim 1, wherein the first electrode comprises two sub-layers, and a sublayer in contact with the active component comprises carbon.

### Claim 13

A method, comprising:
forming a metal layer for an access line;
forming, above the metal layer, an electrode layer for a memory cell, wherein a surface of the electrode layer has an initial surface roughness;
polishing the surface of the electrode layer to change the surface from having the initial surface roughness to having a subsequent surface roughness that is less than the initial surface roughness; and
forming, after the polishing, an active layer in contact with the surface of the electrode layer, wherein a uniformity of a thickness of the active layer is based at least in part on the subsequent surface roughness.

### Claim 14 (depends on 13)

The method of claim 13, wherein polishing the surface of the electrode layer comprises:
applying a chemical-mechanical planarization (CMP) process to the surface of the electrode layer.

### Claim 15 (depends on 13)

The method of claim 13, wherein:
forming the electrode layer comprises depositing an electrode material via a deposition process; and
polishing the surface of the electrode layer comprises breaking a vacuum seal associated with the deposition process.

### Claim 16 (depends on 13)

The method of claim 13, further comprising:
forming a second electrode layer for the memory cell above the active layer; and
forming a second active layer above the second electrode layer.

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
polishing a surface of the second electrode layer before forming the second active layer to change the surface of the second electrode layer from a second initial surface roughness to a second subsequent surface roughness that is less than the second initial surface roughness.

### Claim 18 (depends on 16)

The method of claim 16, further comprising:
polishing a surface of the active layer before forming the second electrode layer; or
polishing a surface of the second active layer.

### Claim 19 (depends on 16)

The method of claim 16, wherein a storage component for the memory cell comprises at least a portion of the second active layer.

### Claim 20 (depends on 16)

The method of claim 16, wherein:
the active layer comprises a first chalcogenide material;
the second active layer comprises a second chalcogenide material, the second chalcogenide material different from the first chalcogenide material; and
the electrode layer and the second electrode layer each comprise carbon.

### Claim 21 (depends on 16)

The method of claim 16, further comprising:
forming a third electrode layer for the memory cell above the second active layer;
forming a second metal layer for a second access line for the memory cell, the second metal layer above the third electrode layer; and
polishing a surface of the third electrode layer prior to forming the second metal layer.

### Claim 22

A method, comprising:
forming a metal layer for an access line;
forming, above the metal layer, a first electrode layer comprising carbon for a memory cell;
reducing a surface roughness of an upper surface of the first electrode layer by applying a chemical-mechanical planarization (CMP) process to the upper surface of the first electrode layer;
forming a chalcogenide layer in contact with the upper surface of the first electrode layer after applying the CMP process; and
forming, above the chalcogenide layer, a second electrode layer comprising carbon for the memory cell.

### Claim 23 (depends on 22)

The method of claim 22, wherein:
forming the first electrode layer comprises depositing an electrode material via a deposition process; and
applying the CMP process to the upper surface of the first electrode layer comprises breaking a vacuum seal associated with the deposition process.

### Claim 24 (depends on 22)

The method of claim 22, further comprising:
reducing a surface roughness of an upper surface of the second electrode layer by applying a second CMP process to the upper surface of the second electrode layer; and
forming a second chalcogenide layer in contact with the upper surface of the second electrode layer, wherein a thickness of the second chalcogenide layer is based at least in part on reducing the surface roughness of the upper surface of the second electrode layer.

### Claim 25 (depends on 22)

The method of claim 22, further comprising:
forming a second chalcogenide layer in contact with the upper surface of the second electrode layer, wherein a thickness of the second chalcogenide layer is based at least in part on an initial surface roughness of the upper surface of the second electrode layer.