# US 2019/0378890 A1 · Rolled-up electromagnetic component for on-chip applications and method of making a rolled-up electromagnetic component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0378890 A1
- Document ID: US20190378890A1
- Status: Published application
- Kind: A1
- Application number: 16/434,524
- Filed: 2019-06-07
- Published: 2019-12-12
- Earliest claimed: 2018-06-08
- Assignees: The Board of Trustees of the University of Illinois
- Applicants: The Board of Trustees of the University of Illinois
- Inventors: Xiuling Li; Wen Huang; Zhendong Yang; Mark D. Kraman; Jimmy Ni; Zihao Ou; Qian Chen; J. Gary Eden
- Web page: https://patentgrep.com/patent/US20190378890A1

## CPC

- H10D 1/20: Inductors
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A rolled-up electromagnetic component for on-chip applications comprises: a multilayer sheet in a rolled configuration comprising at least one turn about a longitudinal axis; a core defined by a first turn of the rolled configuration; and a soft magnetic material disposed within the core, where the multilayer sheet comprises a conductive pattern layer on a strain-relieved layer. A method of making a rolled-up electromagnetic component for on-chip applications includes forming a rolled-up device comprising: a multilayer sheet in a rolled configuration having at least one turn about a longitudinal axis, where the multilayer sheet comprises a conductive pattern layer on a strain-relieved layer; and a core defined by a first turn of the rolled configuration. The method further includes introducing a soft magnetic material into the core.

## Claims

### Claim 1

A rolled-up electromagnetic component for on-chip applications, the rolled-up electromagnetic component comprising:
a multilayer sheet in a rolled configuration comprising at least one turn about a longitudinal axis, the multilayer sheet comprising a conductive pattern layer on a strain-relieved layer;
a core defined by a first turn of the rolled configuration; and
a soft magnetic material disposed within the core.

### Claim 2 (depends on 1)

The rolled-up electromagnetic component of claim 1, wherein the soft magnetic material comprises iron, nickel, chromium, iron oxide, a ferrite, iron nitride, manganese selenide, a nickel-iron alloy, and/or an iron-silicon-aluminum alloy.

### Claim 3 (depends on 2)

The rolled-up electromagnetic component of claim 2, wherein the ferrite is selected from the group consisting of: ZnFe2O4, MnFe2O4, NiFe2O4, CoFe2O4, CoxNi1-xFe2O4, CoxZn1-xFe2O4, NixZn1-xFe2O4, MnxZn1-xFe2O4, where 0<x<1.

### Claim 4 (depends on 1)

The rolled-up electromagnetic component of claim 1, wherein magnetic particles comprising the soft magnetic material are disposed within the core.

### Claim 5 (depends on 1)

The rolled-up electromagnetic component of claim 1, wherein a solid body comprising the soft magnetic material is disposed within the core.

### Claim 6 (depends on 1)

The rolled-up electromagnetic component of claim 1, wherein a magnetic layer comprising the soft magnetic material is disposed on the conductive pattern layer.

### Claim 7 (depends on 1)

The rolled-up electromagnetic component of claim 1, wherein the strain-relieved layer comprises silicon nitride, and
wherein the conductive pattern layer comprises carbon, gold, silver, aluminum, palladium, platinum, and/or copper.

### Claim 8 (depends on 1)

The rolled-up electromagnetic component of claim 1, wherein the conductive pattern layer comprises at least one conductive strip having a length extending in a rolling direction so as to wrap around the longitudinal axis in the rolled configuration, the length being at least about 1 mm.

### Claim 9 (depends on 1)

The rolled-up electromagnetic component of claim 1 being selected from the group consisting of: a rolled-up inductor, a rolled-up transformer, and a tubular resonant filter.

### Claim 10 (depends on 9)

The rolled-up electromagnetic component of claim 9, wherein the rolled-up inductor comprises an inductance of at least about 1 μH at a frequency up to 10 MHz.

### Claim 11 (depends on 1)

An array of the rolled-up electromagnetic components of claim 1.

### Claim 12

A method of making a rolled-up electromagnetic component, the method comprising:
forming a rolled-up device structure comprising: a multilayer sheet in a rolled configuration comprising at least one or multiple turns about a longitudinal axis, the multilayer sheet comprising a conductive pattern layer on a strain-relieved layer; and a core defined by a first turn of the rolled configuration; and
introducing a soft magnetic material into the core.

### Claim 13 (depends on 12)

The method of claim 12, wherein introducing the soft magnetic material into the core comprises:
delivering a ferrofluid including magnetic particles comprising the soft magnetic material into the core; and/or
inserting a solid body comprising the soft magnetic material into the core; and/or
depositing a magnetic layer comprising the soft magnetic material on the conductive pattern layer after forming the rolled-up device structure.

### Claim 14 (depends on 12)

The method of claim 12, wherein the soft magnetic material is introduced into the core as the rolled-up device structure is being formed, the multilayer sheet further comprising, prior to roll-up, a magnetic layer comprising the soft magnetic material on the conductive pattern layer.

### Claim 15 (depends on 12)

The method of claim 12, wherein the conductive pattern layer comprises at least one conductive strip having a length extending in a rolling direction, the length of the conductive strip being at least about 1 mm.

### Claim 16 (depends on 12)

The method of claim 12, wherein forming the rolled-up device structure comprises:
forming a sacrificial layer on a substrate;
forming a strained layer on the sacrificial layer, the strained layer comprising an upper portion under tensile stress and a lower portion under compressive stress, the strained layer being held on the substrate by the sacrificial layer;
forming a conductive pattern layer on the strained layer;
initiating removal of the sacrificial layer from the substrate, thereby releasing an end of the strained layer, and
continuing the removal of the sacrificial layer, thereby allowing the strained layer to move away from the substrate and roll up to relieve strain in the strained layer, the conductive pattern layer adhering to the strained layer during the roll-up, and
thereby forming the rolled-up device structure.

### Claim 17 (depends on 16)

The method of claim 16, wherein removing the sacrificial layer comprises vapor-phase etching of the sacrificial layer.

### Claim 18 (depends on 16)

The method of claim 16, further comprising forming discrete bumps on the strained layer to serve as spacers during roll-up, wherein, during the roll-up, the discrete bumps keep adjacent turns spaced apart such that the rolled-up device structure includes gaps between adjacent turns.

### Claim 19 (depends on 18)

The method of claim 18, further comprising, after the roll-up, directing a soft magnetic material into the core and into the gaps between adjacent turns, the soft magnetic material being deposited on the conductive pattern layer as a magnetic layer.

### Claim 20 (depends on 18)

The method of claim 18, further comprising, after the roll-up, directing a conductive material into the core and into the gaps between adjacent turns, the conductive material being deposited on and increasing a thickness of the conductive pattern layer.