# US 2019/0378807 A1 · Semiconductor package and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0378807 A1
- Document ID: US20190378807A1
- Status: Published application
- Kind: A1
- Application number: 16/427,033
- Filed: 2019-05-30
- Published: 2019-12-12
- Earliest claimed: 2018-06-12
- Assignees: Nepes Co., Ltd.
- Applicants: Nepes CO., LTD.
- Inventors: Yong Tae KWON; Hee Cheol KIM; Seung Jun MOON; Jini SHIM
- Web page: https://patentgrep.com/patent/US20190378807A1

## CPC

- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/019: {of bond pads}
- H10W 72/90: Bond pads, in general
- H10W 70/60: Insulating or insulated package substrates; Interposers; Redistribution layers (leadframes H10W70/40)
- H10W 72/07236: {Soldering or alloying}
- H10W 72/07252: {changes in structures or sizes}
- H10W 72/221: {Structures or relative sizes}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/281: {Auxiliary members}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/981: {Auxiliary members, e.g. spacers}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention relates to a semiconductor package and a method of manufacturing the same. In a semiconductor package which electrically connects a semiconductor chip and a printed circuit board using a solder ball, the semiconductor package further includes a thermal buffer layer which is positioned on a semiconductor chip, absorbs and disperse heat generated by the semiconductor chip, increases a distance between the semiconductor chip and a printed circuit board to decrease a deviation of a heat conduction process, and has a thickness ranging from 7.5 to 50% of a diameter of a solder ball.

## Claims

### Claim 1

A semiconductor package which electrically connects a semiconductor chip and a printed circuit board using a solder ball, the semiconductor package further comprising a thermal buffer layer which is positioned on a semiconductor chip, absorbs and disperse heat generated by the semiconductor chip, increases a distance between the semiconductor chip and a printed circuit board to decrease a deviation of a heat conduction process, and has a thickness ranging from 7.5 to 50% of a diameter of a solder ball.

### Claim 2 (depends on 1)

The semiconductor package of claim 1, wherein the thermal buffer layer includes a resin coated film in contact with one surface of the semiconductor chip or a passivation layer formed on the resin coated film.

### Claim 3 (depends on 2)

The semiconductor package of claim 2, wherein the thermal buffer layer has the thickness ranging from 15 to 100 μm.

### Claim 4 (depends on 3)

The semiconductor package of claim 3, wherein the passivation layer has a multilayer structure,
wherein:
a lowest layer of the multilayer structure is positioned on an entirety of the resin coated layer; and
a highest layer of the multilayer structure is disposed on a part of the resin coated layer such that a step is formed on an under bump metallization on which the solder ball is seated.

### Claim 5 (depends on 4)

The semiconductor package of claim 4, wherein:
the under bump metallization includes a lower region of the step, which is a region in contact with a re-distribution layer, an upper region of the step, which is positioned on the passivation layer, and a step surface, which connects the upper region and the lower region of the step; and
a central portion of the solder ball is positioned on the lower region of the step and a peripheral portion of the solder ball is positioned on the upper region of the step.

### Claim 6 (depends on 3)

The semiconductor package of claim 3, wherein the thickness of the thermal buffer layer and a thickness of the semiconductor chip are adjusted such that an overall thickness of the semiconductor package is constant.

### Claim 7 (depends on 2)

The semiconductor package of claim 2, further comprising an epoxy molding compound which supports a side portion of the solder ball on the thermal buffer layer.

### Claim 8

A method of manufacturing a semiconductor package, the method comprising:
a) forming a resin coated film on a semiconductor chip and forming a re-distribution layer in contact with an electrode of the semiconductor chip on a part of an upper portion of the resin coated film;
b) forming a passivation layer which is positioned on the resin coated film and is a thermal buffer layer, which exposes an upper central portion of the re-distribution layer, to have a thickness ranging from 7.5 to 50% of a diameter of a solder ball;
c) forming an under bump metallization in contact with the re-distribution layer; and
d) forming the solder ball which electrically connects the under bump metallization and a printed circuit board.

### Claim 9 (depends on 8)

The method of claim 8, wherein the passivation layer is formed as a plurality of layers,
wherein:
a lowest layer of the plurality of layers is formed on an entirety of the resin coated film; and
a highest layer thereof is formed to be positioned under a peripheral portion of the under bump metallization.

### Claim 10 (depends on 8)

The method of claim 8, wherein:
the under bump metallization includes a lower region of a step, which is a region in contact with the re-distribution layer, an upper region of the step, which is positioned on the passivation layer, and a step surface which connects the upper region and the lower region of the step; and
a central portion of the solder ball is positioned on the lower region of the step and a peripheral portion of the solder ball is positioned on the upper region of the step.

### Claim 11 (depends on 8)

The method of claim 8, further comprising forming an epoxy molding compound, which supports a side portion of the solder ball, on the thermal buffer layer.

### Claim 12 (depends on 8)

The method of claim 8, wherein a thickness of the thermal buffer layer and a thickness of the semiconductor chip are adjusted such that an overall thickness of the semiconductor package is constant.

### Claim 13 (depends on 12)

The method of claim 12, wherein a rear surface of the semiconductor chip is ground by an amount by which the thickness of the thermal buffer layer is increased.

### Claim 14

A method of manufacturing a semiconductor package comprising:
a-1) forming a resin coated film, which is a thermal buffer layer, on a semiconductor chip to have a thickness ranging from 7.5 to 50% of a diameter of a solder ball and forming a re-distribution layer in contact with an electrode of the semiconductor chip on a part of an upper portion of the resin coated film;
b-1) forming a passivation layer which is positioned on the resin coated film and is a thermal buffer layer which exposes an upper central portion of the re-distribution layer;
c-1) forming an under bump metallization in contact with the re-distribution layer; and
d-1) forming the solder ball which electrically connects the under bump metallization and a printed circuit board.

### Claim 15 (depends on 14)

The method of claim 14, wherein:
the under bump metallization includes a lower region of a step, which is a region in contact with the re-distribution layer, an upper region of the step, which is positioned on the passivation layer, and a step surface which connects the upper region and the lower region of the step; and
a central portion of the solder ball is positioned on the lower region of the step and a peripheral portion of the solder ball is positioned on the upper region of the step.

### Claim 16 (depends on 14)

The method of claim 14, further comprising forming an epoxy molding compound, which supports a side portion of the solder ball, on the thermal buffer layer.

### Claim 17 (depends on 14)

The method of claim 14, wherein a thickness of the thermal buffer layer and a thickness of the semiconductor chip are adjusted such that an overall thickness of the semiconductor package is constant.

### Claim 18 (depends on 17)

The method of claim 17, wherein a rear surface of the semiconductor chip is ground by an amount by which the thickness of the thermal buffer layer is increased.