# US 2019/0378806 A1 · Film scheme for bumping

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0378806 A1
- Document ID: US20190378806A1
- Status: Published application
- Kind: A1
- Application number: 16/549,013
- Filed: 2019-08-23
- Published: 2019-12-12
- Earliest claimed: 2016-11-29
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Yao-Wen Chang; Chern-Yow Hsu; Cheng-Yuan Tsai; Kong-Beng Thei
- Web page: https://patentgrep.com/patent/US20190378806A1

## CPC

- H10P 50/283: {by chemical means}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10P 14/46: using a liquid
- H10W 72/01233: {in liquid form, e.g. spin coating, spray coating or immersion coating}
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01238: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/019: {of bond pads}
- H10W 72/01938: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/222: {Multilayered bumps, e.g. a coating on top and side surfaces of a bump core}
- H10W 72/224: {Bumps having multiple side-by-side cores}
- H10W 72/231: {Shapes}
- H10W 72/232: {Plan-view shape, i.e. in top view}
- H10W 72/234: {Cross-sectional shape, i.e. in side view}
- H10W 72/242: {relative to the surface, e.g. recessed, protruding}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/253: {not comprising solid metals or solid metalloids, e.g. polymers or ceramics}
- H10W 72/287: {Flow barriers}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/90: Bond pads, in general
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/934: {Cross-sectional shape, i.e. in side view}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/987: {Flow barriers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A bump structure with a barrier layer, and a method for manufacturing the bump structure, are provided. In some embodiments, the bump structure comprises a conductive pad, a conductive bump, and a barrier layer. The conductive pad comprises a pad material. The conductive bump overlies the conductive pad, and comprises a lower bump layer and an upper bump layer covering the lower bump layer. The barrier layer is configured to block movement of the pad material from the conductive pad to the upper bump layer along sidewalls of the lower bump layer. In some embodiments, the barrier layer is a spacer lining the sidewalls of the lower bump layer. In other embodiments, the barrier layer is between the barrier layer and the conductive pad, and spaces the sidewalls of the lower bump layer from the conductive pad.

## Claims

### Claim 1

A method comprising:
forming a passivation layer covering a conductive pad;
patterning the passivation layer to form a first opening directly over the conductive pad and having a first passivation sidewall in the first opening, wherein the passivation layer underlies and spaces the first opening from the conductive pad;
depositing a sacrificial layer covering the passivation layer and filling the first opening;
patterning the sacrificial layer to form a second opening directly over the conductive pad, wherein the sacrificial layer defines a sacrificial sidewall that is in the second opening and that is laterally offset from the first passivation sidewall;
depositing a conductive layer covering the sacrificial layer and lining second opening on the sacrificial sidewall;
etching back the conductive layer to remove laterally elongated segments of the conductive layer;
forming a conductive bump in the second opening and laterally separated from the sacrificial sidewall by the conductive layer; and
removing the sacrificial layer after the forming of the conductive bump.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising:
performing an etch into the passivation layer through the second opening and while the sacrificial layer and the conductive layer are in place, wherein the etch uses the conductive layer and the sacrificial layer as a mask and extends the second opening to the conductive pad.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the passivation layer is patterned with the sacrificial layer while forming the second opening, such that the second opening exposes the conductive pad and the passivation layer defines a second passivation sidewall in the second opening, wherein the second passivation sidewall is even with the sacrificial sidewall, and wherein the conductive layer is deposited lining the second passivation sidewall.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising:
performing a planarization into the sacrificial layer, the conductive bump, and the conductive layer before the removing.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the forming of the conductive bump comprises:
depositing a nickel layer on the conductive pad and in the second opening by a first plating process; and
depositing a gold layer on the nickel layer and in the second opening by a second plating process.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the nickel layer directly contacts the conductive pad, wherein the gold layer directly contacts the nickel layer, wherein the conductive layer comprises tantalum nitride and/or titanium nitride, and wherein the conductive layer directly contacts the nickel and gold layers, the second passivation sidewall, and the sacrificial sidewall.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the forming of the passivation layer comprises:
depositing a first dielectric layer covering the conductive pad; and
depositing a second dielectric layer covering the first dielectric layer, wherein the second dielectric layer is a different material than the first dielectric layer, and wherein the patterning of the passivation layer comprises performing an etch into the second dielectric layer that stops on the first dielectric layer.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising:
depositing an etch stop layer covering the passivation layer and lining the first opening, wherein the sacrificial layer is deposited over the etch stop layer, wherein the etch stop layer is patterned with the sacrificial layer while forming the second opening, such that the etch stop layer defines an etch stop sidewall that is in the second opening and that is even with the sacrificial sidewall, and wherein the removing comprises performing an etch into the sacrificial layer and stopping on the etch stop layer.

### Claim 9

A method comprising:
forming a first passivation layer covering a conductive pad, wherein the conductive pad comprises a pad material;
forming a second passivation layer covering the first passivation layer;
performing a first etch into the second passivation layer to form a first opening overlying the conductive pad and exposing the first passivation layer, wherein the first etch stops on the first passivation layer, and wherein the second passivation layer has a pair of sidewall segments in the first opening and respectively on opposite sides of the first opening;
forming a sacrificial layer filling the first opening, and further covering the first and second passivation layers;
performing a second etch into the sacrificial layer to form a second opening overlying the conductive pad and laterally spaced between the sidewall segments;
forming a sidewall spacer structure on a sidewall of the sacrificial layer in the second opening, wherein the sidewall spacer structure comprises a pair of spacer segments respectively on opposite sides of the second opening, and wherein the sidewall spacer structure is configured to block diffusion of the pad material through the sidewall spacer structure;
forming a conductive bump within the second opening and directly between the spacer segments, wherein the conductive bump comprises a first bump layer and a second bump layer covering the first bump layer; and
performing a third etch into the sacrificial layer to remove the sacrificial layer.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the forming of the sidewall spacer structure comprises:
depositing a barrier layer covering the sacrificial layer and lining the second opening; and
performing a fourth etch into the barrier layer to remove horizontal segments of the barrier layer without removing vertical segments of the barrier layer.

### Claim 11 (depends on 9)

The method according to claim 9, further comprising:
performing a fourth etch into the first passivation layer with the sidewall spacer structure and the sacrificial layer in place to expand the second opening to the conductive pad, wherein the conductive bump is formed after expanding the second opening.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the second etch is further performed into the first passivation layer, such that the second opening exposes the conductive pad.

### Claim 13 (depends on 9)

The method according to claim 9, further comprising:
performing a planarization into a top surface of the sacrificial layer, a top surface of the sidewall spacer structure, and a top surface of the conductive bump until the top surfaces respectively of the sacrificial layer, the sidewall spacer structure, and the conductive bump are about even.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the forming of the conductive bump comprises:
depositing the first bump layer by a plating process directly on the conductive pad; and
depositing the second bump layer directly on the first bump layer by a plating process, wherein the second bump layer defines the top surface of the conductive bump.

### Claim 15 (depends on 9)

The method according to claim 9, wherein a majority element in the conductive bump is absent in the conductive pad.

### Claim 16

A method comprising:
forming a first passivation layer covering a conductive pad that comprises a pad material;
patterning the first passivation layer to form a first opening directly over and exposing the conductive pad, wherein the first passivation layer has a pair of first passivation sidewalls in the first opening when viewed in cross section, and wherein the first passivation sidewalls are respectively on opposite sides of the first opening and are separated by a first distance;
depositing a barrier layer covering the first passivation layer and lining the first opening, wherein the barrier layer directly contacts the conductive pad and the first passivation sidewalls, and wherein the barrier layer is conductive and configured to block diffusion of the pad material;
depositing a sacrificial layer covering the first passivation layer;
patterning the sacrificial layer to form a second opening directly over the conductive pad, wherein the sacrificial layer has a pair of sacrificial sidewalls in the second opening when viewed in cross section, and wherein the sacrificial sidewalls are respectively on opposite sides of second opening and are separated by a second distance less than or equal to the first distance;
depositing a nickel layer in the second opening, wherein the barrier layer separates the nickel layer from the first passivation sidewalls, and wherein a bottom surface of the nickel layer is recessed below a top surface of the barrier layer;
depositing a gold layer directly on the nickel layer and in the second opening; and
removing the sacrificial layer after the forming of the gold layer.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the barrier layer is deposited after the patterning of the sacrificial layer and directly contacts the sacrificial sidewalls, and wherein the patterning of the first passivation layer and the patterning of the sacrificial layer are performed together by performing an etch into the first passivation layer and the sacrificial layer with a common photoresist mask in place.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the barrier layer is deposited with a barrier thickness, and wherein the method further comprises:
performing a vertical etch into the barrier layer to recess a top surface of the barrier layer by the barrier thickness.

### Claim 19 (depends on 16)

The method according to claim 16, further comprising:
depositing a second passivation layer overlying the first passivation layer; and
etching the second passivation layer to form a third opening overlying the conductive pad, wherein etching stops on the first passivation layer, and wherein the sacrificial layer is formed overlying the second passivation layer and filling the third opening.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the second passivation layer has a pair of second passivation sidewalls in the third opening when viewed in cross section, wherein the second passivation sidewalls are respectively on opposite sides of the third opening, and wherein the first passivation sidewalls are formed laterally between and laterally spaced from the second passivation sidewalls.