# US 2019/0378755 A1 · Controlling grain boundaries in high aspect-ratio conductive regions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0378755 A1
- Document ID: US20190378755A1
- Status: Published application
- Kind: A1
- Application number: 16/003,766
- Filed: 2018-06-08
- Published: 2019-12-12
- Earliest claimed: 2018-06-08
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Conal Murray; Chih-Chao Yang
- Web page: https://patentgrep.com/patent/US20190378755A1

## CPC

- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/0526: {by thermal treatment thereof}
- H10W 20/072: {of dielectric parts comprising air gaps}
- H10W 20/075: {of multilayered thin functional dielectric layers}
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/098: {by filling between adjacent conductive parts}
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 20/46: comprising air gaps
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Methods for forming high aspect-ratio conductive regions of a metallization network with reduced grain boundaries are described. Aspects of the invention include forming a trench in a dielectric material on the substrate. A conductive material is formed in the trench, wherein the conductive material includes a first grain boundary level. Portions of the dielectric material are removed to expose sidewalls of the conductive material. The conductive material is annealed to reduce the first grain boundary level.

## Claims

### Claim 1

A method of forming a conductive region of a metallization network associated with a substrate, the method comprising:
forming a trench in a dielectric material on the substrate;
forming a conductive material in the trench, wherein the conductive material includes a first grain boundary level;
removing portions of the dielectric material to expose sidewalls of the conductive material; and
annealing the conductive material to reduce the first grain boundary level.

### Claim 2 (depends on 1)

The method of claim 1, wherein the trench comprises an aspect ratio less than about 2.5.

### Claim 3 (depends on 1)

The method of claim 1, wherein the annealing results in heat being driven through the sidewalls of the conductive material.

### Claim 4 (depends on 1)

The method of claim 1 further comprising conformally forming a protective layer on the exposed sidewalls of the conductive material prior to the annealing.

### Claim 5 (depends on 1)

The method of claim 1 further comprising forming a liner layer on the conductive material, wherein the liner layer is a metallic liner.

### Claim 6 (depends on 1)

The method of claim 1, wherein:
the trench comprises a first trench;
the conductive material comprises a first conductive material; and
the method further comprises:
forming a second trench in the dielectric material on the substrate;
forming a second conductive material in the second trench, wherein the second conductive material includes a second grain boundary;
removing portions of the dielectric material to expose sidewalls of the second conductive material; and
annealing the second conductive material to reduce the second grain boundary layer.

### Claim 7 (depends on 6)

The method of claim 6 further comprising:
forming a liner layer on the first conductive material and the second conductive material;
depositing a second dielectric material over the liner layer; and
forming one or more airgaps in the second dielectric material between the first conductive material and the second conductive material.

### Claim 8 (depends on 4)

The method of claim 4, wherein the protective layer comprises hydrogen silsesquixane.

### Claim 9 (depends on 1)

The method of claim 1, wherein annealing the conductive material comprises a thermal anneal at a temperature of about 100 C to about 500 C for about 20 minutes to about five hours.

### Claim 10 (depends on 1)

The method of claim 1, wherein annealing the conductive material comprises a laser anneal at a temperature of about 400 C to about 1200 C for about 20 nanoseconds to about fifteen minutes.

### Claim 11

A method of forming conductive regions in a metallization network associated with a substrate, the method comprising:
forming a first trench in a dielectric material on the substrate;
forming a second trench in the dielectric material on the substrate;
forming a first conductive material in the first trench, wherein the first conductive material includes a first grain boundary level;
forming a second conductive material in the second trench, wherein the second conductive material includes a second grain boundary level;
removing portions of the dielectric material to expose sidewalls of the first conductive material; and
annealing the first conductive material to reduce the first grain boundary level.

### Claim 12 (depends on 11)

The method of claim 11, wherein the first trench comprises an aspect ratio greater than or equal to about 2.5.

### Claim 13 (depends on 11)

The method of claim 11, wherein the second trench comprises an aspect ratio less than or equal to about 2.5.

### Claim 14 (depends on 11)

The method of claim 11, further comprising:
exposing a top surface of the first conductive material; and
wherein the annealing the first conductive material results in heat being driven through the exposed sidewalls and the exposed top surface of the first conductive material.

### Claim 15 (depends on 11)

The method of claim 11 further comprising forming a protective layer on the exposed sidewalls of the first conductive material.

### Claim 16 (depends on 11)

The method of claim 11 further comprising annealing the first conductive material and the second conductive material prior to removing the portions of the dielectric material to expose sidewalls of the first conductive material.

### Claim 17 (depends on 15)

The method of claim 15, wherein the protective layer comprises hydrogen silsesquixane.

### Claim 18 (depends on 11)

The method of claim 11, wherein the first trench and the second trench each comprise an aspect ratio less than about 2.5

### Claim 19 (depends on 18)

The method of claim 18 further comprising:
forming a liner layer on the first conductive material and the second conductive material;
depositing a second dielectric material over the liner layer; and
forming one or more airgaps in the second dielectric material between the first conductive material and the second conductive material.

### Claim 20

A semiconductor structure comprising:
a first conductive material formed in a first trench, wherein the first conductive material includes a first grain boundary level;
a second conductive material formed in a second trench, wherein the second conductive material includes a second grain boundary level;
a third conductive material formed in a third trench, wherein the third conductive material includes a third grain boundary level;
a first liner layer formed over the first conductive material and the second conductive material; and
a second liner layer formed over the first liner layer and the third conductive material.