# US 2019/0378753 A1 · Method for transfer of a thin layer of silicon

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0378753 A1
- Document ID: US20190378753A1
- Status: Published application
- Kind: A1
- Application number: 16/420,637
- Filed: 2019-05-23
- Published: 2019-12-12
- Earliest claimed: 2018-06-08
- Assignees: GlobalWafers Co., Ltd.
- Applicants: GlobalWafers Co. Ltd.
- Inventors: Gaurab Samanta; Salvador Zepeda
- Web page: https://patentgrep.com/patent/US20190378753A1

## CPC

- H10P 90/1916: {with separation or delamination along an ion implanted layer, e.g. Smart-cut}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for preparing semiconductor on insulator structures comprises transferring a thin layer of silicon from a donor substrate onto a handle substrate.

## Claims

### Claim 1

A method of transferring a silicon layer from a single crystal silicon donor substrate to a handle substrate, the method comprising:
(a) implanting H2+ ions, H+ ions, or a combination of H2+ ions and H+ ions through a silicon dioxide layer in contact with a front surface of the single crystal silicon donor substrate and through the front surface of the single crystal silicon donor substrate, the single crystal silicon donor substrate comprising two major, parallel surfaces one of which is the front surface and one of which is the back surface, a circumferential edge joining the front surface and the back surface, a central plane between the front surface and the back surface, a central axis perpendicular to the front surface, and a bulk region between the front surface and the back surface;
(b) implanting He+ ions through the silicon dioxide layer in contact with the front surface of a single crystal silicon donor substrate and through the front surface of the single crystal silicon donor substrate;
(c) annealing the ion implanted single crystal silicon donor substrate at a temperature and for a duration sufficient to form a damage layer in the single crystal silicon donor substrate;
(d) bonding the silicon dioxide layer in contact with the front surface of the single crystal silicon donor substrate to a dielectric layer in contact with the handle substrate to thereby prepare the multilayer substrate;
(e) annealing the multilayer substrate; and
(f) cleaving the annealed multilayer substrate at the damage layer in the single crystal silicon donor substrate to thereby transfer the silicon layer having a thickness between about 500 Angstroms and about 2500 Angstroms from the single crystal silicon donor substrate to the handle substrate.

### Claim 2 (depends on 1)

The method of claim 1 wherein step (a) occurs before step (b).

### Claim 3 (depends on 1)

The method of claim 1 wherein step (b) occurs before step (a).

### Claim 4 (depends on 1)

The method of claim 1 wherein steps (a) and (b) occur simultaneously.

### Claim 5 (depends on 1)

The method of claim 1 wherein the single crystal donor substrate has a diameter between 150 mm and 450 mm, or about 300 mm.

### Claim 6 (depends on 1)

The method of claim 1 wherein the silicon dioxide layer has a thickness between about 100 angstroms and about 1000 angstroms, or between about 100 angstroms and about 700 angstroms, or between about 100 angstroms and about 500 angstroms, or between about 100 angstroms and about 250 angstroms.

### Claim 7 (depends on 1)

The method of claim 1 wherein the silicon dioxide layer has a thickness between about 5 angstroms and about 25 angstroms, or between about 10 angstroms and about 15 angstroms.

### Claim 8 (depends on 1)

The method of claim 1 wherein step (a) comprises (i) implanting H2| ions at a dosage between about 4.3×1015 ions/cm2 and about 1.1×1016 ions/cm2 at an implant energy between about 10 Kev and about 40 Kev, or between about 20 Kev and about 40 Kev, (ii) implanting H+ ions at a dosage between about 5×1015 ions/cm2 and about 2×1016 ions/cm2 at an implant energy between about 5 Kev and about 20 Kev, or (iii) implanting H2+ ions at a dosage between about 4.3×1015 ions/cm2 and about 1.1×1016 ions/cm2 at an implant energy between about 10 Kev and about 40 Kev, or between about 20 Kev and about 40 Kev and implanting H+ ions at a dosage between about 5×1015 ions/cm2 and about 2×1016 ions/cm2 at an implant energy between about 5 Kev and about 20 Kev.

### Claim 9 (depends on 8)

The method of claim 8 wherein a peak density, (D1), of H2+ ions, H+ ions, or a combination of H2+ ions and H+ ions is between about 100 Angstroms and about 3000 Angstroms, or between about 500 Angstroms and about 2500 Angstroms, as measured from the front surface of the single crystal silicon donor substrate and along the central axis.

### Claim 10 (depends on 1)

The method of claim 1 wherein step (b) comprises implanting He+ ions at a dosage between about 6×1015 ions/cm2 and about 8×1015 ions/cm2 at an implant energy between about 5 Kev and about 30 Kev, or between about 10 Kev and about 25 Kev.

### Claim 11 (depends on 10)

The method of claim 10 wherein a peak density, (D2), of He+ ions is between about 100 Angstroms and about 4000 Angstroms, or between about 500 Angstroms and about 3000 Angstroms, as measured from the front surface of the single crystal silicon donor substrate and along the central axis.

### Claim 12 (depends on 8)

The method of claim 8 wherein the peak density, (D1), of H2+ ions, H+ ions, or a combination of H2+ ions and H+ ions and the peak density, (D2), of He+ ions are within about 600 angstroms of each other, or within about 500 angstroms of each other, within about 450 angstroms of each other, within about 400 angstroms of each other, within about 300 angstroms of each other, or within about 200 angstroms of each other.

### Claim 13 (depends on 8)

The method of claim 8 wherein step (c) comprises annealing the ion implanted single crystal silicon donor substrate at a temperature between about 250° C. and about 300° C. for a duration between 10 minutes and 60 minutes.

### Claim 14 (depends on 8)

The method of claim 8 wherein step (e) comprises annealing the ion implanted single crystal silicon donor substrate at a temperature between about 300° C. and about 400° C. for a duration between 10 minutes and 60 minutes.

### Claim 15 (depends on 8)

The method of claim 8 wherein the silicon layer having the thickness between about 500 Angstroms and about 2500 Angstroms transferred from the single crystal silicon donor substrate to the handle substrate has a thickness variation less than about 10 angstroms.

### Claim 16 (depends on 1)

The method of claim 1 wherein step (a) comprises (i) implanting H2| ions at a dosage between about 4.3×1015 ions/cm2 and about 1.1×1016 ions/cm2, or between about 6×1015 ions/cm2 and about 1.1×1016 ions/cm2, at an implant energy between about 20 Kev and about 40 Kev, (ii) implanting H+ ions at a dosage between about 1.1×1016 ions/cm2 and about 2×1016 ions/cm2 at an implant energy between about 5 Kev and about 20 Kev, or (iii) implanting H2+ ions at a dosage between about 4.3×1015 ions/cm2 and about 1.1×1016 ions/cm2, or between about 6×1015 ions/cm2 and about 1.1×1016 ions/cm2, at an implant energy between about 20 Kev and about 40 Kev and implanting H+ ions at a dosage between about 1.1×1016 ions/cm2 and about 2×1016 ions/cm2 at an implant energy between about 5 Kev and about 20 Kev.

### Claim 17 (depends on 16)

The method of claim 16 wherein a peak density, (D1), of H2+ ions, H+ ions, or a combination of H2+ ions and H+ ions is between about 100 Angstroms and about 3000 Angstroms, or between about 500 Angstroms and about 2500 Angstroms, as measured from the front surface of the single crystal silicon donor substrate and along the central axis.

### Claim 18 (depends on 16)

The method of claim 16 wherein step (b) comprises implanting He+ ions at a dosage between about 6×1015 ions/cm2 and about 8×1015 ions/cm2 at an implant energy between about 10 Kev and about 30 Kev.

### Claim 19 (depends on 18)

The method of claim 18 wherein a peak density, (D2), of He| ions is between about 100 Angstroms and about 4000 Angstroms, or between about 500 Angstroms and about 3000 Angstroms, as measured from the front surface of the single crystal silicon donor substrate and along the central axis.

### Claim 20 (depends on 16)

The method of claim 16 wherein the peak density, (D1), of H2+ ions, H+ ions, or a combination of H2+ ions and H+ ions and the peak density, (D2), of He+ ions are within about 600 angstroms of each other, or within about 500 angstroms of each other, within about 450 angstroms of each other, within about 400 angstroms of each other, within about 300 angstroms of each other, or within about 200 angstroms of each other.

### Claim 21 (depends on 16)

The method of claim 16 wherein step (c) comprises annealing the ion implanted single crystal silicon donor substrate at a temperature between about 250° C. and about 300° C. for a duration between 10 minutes and 60 minutes.

### Claim 22 (depends on 16)

The method of claim 16 wherein step (e) comprises annealing the ion implanted single crystal silicon donor substrate at a temperature between about 300° C. and about 400° C. for a duration between 10 minutes and 60 minutes.

### Claim 23 (depends on 16)

The method of claim 16 wherein the silicon layer having the thickness between about 500 Angstroms and about 2500 Angstroms transferred from the single crystal silicon donor substrate to the handle substrate has a thickness variation less than about 10 angstroms.

### Claim 24 (depends on 1)

The method of claim 1 wherein step (b) comprises implanting He+ ions at a dosage between about 6.6×1015 ions/cm2 and about 7×1015 ions/cm2 at an implant energy between about 5 Kev and about 20 Kev.

### Claim 25 (depends on 24)

The method of claim 24 wherein a peak density, (D2), of He+ ions is between about 100 Angstroms and about 4000 Angstroms, or between about 500 Angstroms and about 3000 Angstroms, as measured from the front surface of the single crystal silicon donor substrate and along the central axis.

### Claim 26 (depends on 24)

The method of claim 24 wherein step (a) comprises (i) implanting H2+ ions at a dosage between about 5.9×1015 ions/cm2 and about 6.7×1015 ions/cm2 at an implant energy between about 10 Kev and about 30 Kev, (ii) implanting H+ ions at a dosage between about 6.1×1015 ions/cm2 and about 6.8×1015 ions/cm2 at an implant energy between about 5 Kev and about 20 Kev, or (iii) implanting H2+ ions at a dosage between about 5.9×1015 ions/cm2 and about 6.7×1015 ions/cm2 at an implant energy between about 10 Kev and about 30 Kev and implanting H+ ions at a dosage between about 6.1×1015 ions/cm2 and about 6.8×1015 ions/cm2 at an implant energy between about 5 Kev and about 20 Kev.

### Claim 27 (depends on 24)

The method of claim 24 wherein a peak density, (D1), of H2+ ions, H+ ions, or a combination of H2+ ions and H+ ions is between about 100 Angstroms and about 3000 Angstroms, or between about 500 Angstroms and about 2500 Angstroms, as measured from the front surface of the single crystal silicon donor substrate and along the central axis.

### Claim 28 (depends on 24)

The method of claim 24 wherein the peak density, (D1), of H2+ ions, H+ ions, or a combination of H2+ ions and H+ ions and the peak density, (D2), of He+ ions are within about 600 angstroms of each other, or within about 500 angstroms of each other, within about 450 angstroms of each other, within about 400 angstroms of each other, within about 300 angstroms of each other, or within about 200 angstroms of each other.

### Claim 29 (depends on 24)

The method of claim 24 wherein step (c) comprises annealing the ion implanted single crystal silicon donor substrate at a temperature between about 250° C. and about 300° C. for a duration between 10 minutes and 60 minutes.

### Claim 30 (depends on 24)

The method of claim 24 wherein step (e) comprises annealing the ion implanted single crystal silicon donor substrate at a temperature between about 300° C. and about 400° C. for a duration between 10 minutes and 60 minutes.

### Claim 31 (depends on 24)

The method of claim 24 wherein the silicon layer having the thickness between about 500 Angstroms and about 2500 Angstroms transferred from the single crystal silicon donor substrate to the handle substrate has a thickness variation less than about 10 angstroms.