# US 2019/0378723 A1 · Film forming method and film forming apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0378723 A1
- Document ID: US20190378723A1
- Status: Published application
- Kind: A1
- Application number: 16/433,325
- Filed: 2019-06-06
- Published: 2019-12-12
- Earliest claimed: 2018-06-08
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Hideo Nakamura; Yosuke Serizawa; Yoshikazu Ideno; Hiroaki Ashizawa; Takaya Shimizu; Seishi Murakami
- Web page: https://patentgrep.com/patent/US20190378723A1

## CPC

- H10D 64/01344: {in a nitrogen-containing ambient, e.g. N2O oxidation}
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A film forming method includes: repeatedly performing a source gas adsorption process including supplying a source gas containing a metal element to form a nitride film on a substrate in a chamber and purging a residual gas, and a nitriding process including supplying a nitriding gas onto the substrate and purging a residual gas; and supplying a hydrazine-based compound gas as a part or all of the nitriding gas.

## Claims

### Claim 1

A film forming method comprising:
repeatedly performing a source gas adsorption process including supplying a source gas containing a metal element to form a nitride film on a substrate in a chamber and purging a residual gas, and a nitriding process including supplying a nitriding gas onto the substrate and purging a residual gas; and
supplying a hydrazine-based compound gas as a part or all of the nitriding gas.

### Claim 2 (depends on 1)

The film forming method of claim 1, wherein the nitride film is a binary nitride film or a ternary or higher nitride film.

### Claim 3 (depends on 2)

The film forming method of claim 2, wherein the binary nitride film is formed of any one of BN, AlN, SiN, ScN, TiN, VN, CrN, MnN, FeN, CoN, NiN, CuN, ZnN, GaN, GeN, YN, ZrN, NbN, MoN, RuN, RhN, PdN, AgN, CdN, InN, SnN, HfN, TaN, WN, ReN, IrN, HgN, TlN, and PbN.

### Claim 4 (depends on 3)

The film forming method of claim 3, wherein the nitriding process includes supplying NH3 gas as the nitriding gas; purging a residual gas; supplying a hydrazine compound gas as the nitriding gas; and purging a residual gas.

### Claim 5 (depends on 4)

The film forming method of claim 4, wherein the nitride film is a TiN film, and a substrate temperature during film formation ranges from 200° C. to 450° C.

### Claim 6 (depends on 5)

The film forming method of claim 5, wherein the substrate temperature during the film formation ranges from 200° C. to 450° C.

### Claim 7 (depends on 5)

The film forming method of claim 5, wherein, when a volume in the chamber is 0.5 L to 2.0 L, a supply amount in the supplying the hydrazine compound gas is 5 sccm to 300 sccm, and a supply time is 0.01 sec to 0.5 sec when the substrate temperature is 300° C. or higher and 0.03 sec to 1.0 sec when the substrate temperature is less than 300° C.

### Claim 8 (depends on 7)

The film forming method of claim 7, wherein a time of the purging the residual gas after the supplying the hydrazine compound gas is 0.1 sec or longer.

### Claim 9 (depends on 1)

The film forming method of claim 1, wherein the nitriding process includes supplying a hydrazine compound gas as the nitriding gas and purging a residual gas.

### Claim 10 (depends on 9)

The film forming method of claim 9, wherein the nitride film is a TiN film, and a substrate temperature during the film formation is 200° C. to 450° C.

### Claim 11 (depends on 10)

The film forming method of claim 10, wherein, when a volume in the chamber is 0.5 L to 2.0 L, a supply amount of the supplying the hydrazine compound gas is 5 sccm to 300 sccm, and the supply time is 0.01 sec to 1.0 sec.

### Claim 12

A film forming method comprising:
a source gas adsorption process including supplying a source gas containing a metal element to form a nitride film on a substrate in a chamber, and purging a residual gas;
a nitriding process including supplying NH3 gas as a nitriding gas on the substrate and purging a residual gas; and
a process of supplying a hydrazine compound gas on the substrate,
wherein the process of supplying the hydrazine compound gas is performed after repeatedly performing the source gas adsorption process and the nitriding process a plurality of times.

### Claim 13 (depends on 12)

The film forming method of claim 12, wherein the nitride film is a binary nitride film or a ternary or higher nitride film, and the binary nitride film is formed of any one of BN, AlN, SiN, ScN, TiN, VN, CrN, MnN, FeN, CoN, NiN, CuN, ZnN, GaN, GeN, YN, ZrN, NbN, MoN, RuN, RhN, PdN, AgN, CdN, InN, SnN, HfN, TaN, WN, ReN, IrN, HgN, TlN, and PbN.

### Claim 14 (depends on 12)

The film forming method of claim 12, wherein the nitride film is a TiN film, and a substrate temperature during film formation is 300° C. to 450° C.

### Claim 15 (depends on 14)

The film forming method of claim 14, wherein, when a volume in the chamber is 0.5 L to 2.0 L, a supply amount of the supplying the hydrazine compound gas is 5 sccm to 300 sccm, and a supply time is 10 sec or longer.

### Claim 16 (depends on 15)

The film forming method of claim 15, wherein the supply time in the process of supplying the hydrazine compound gas is 30 sec or longer.

### Claim 17 (depends on 16)

The film forming method of claim 16, wherein a sequence of repeatedly performing the source gas adsorption process and the nitriding process a plurality of times and then performing the process of supplying the hydrazine compound gas is repeated two or more times with purging between sequences.

### Claim 18 (depends on 16)

The film forming method of claim 16, wherein the source gas containing the metal element is TiCl4.

### Claim 19 (depends on 18)

The film forming method of claim 18, wherein the hydrazine compound gas is selected from hydrazine, monomethyl hydrazine, and dimethyl hydrazine.

### Claim 20 (depends on 1)

A film forming apparatus comprising:
a chamber configured to accommodate a substrate;
a stage configured to place the substrate thereon in the chamber;
a heater configured to heat the substrate on the stage;
a gas supply configured to supply a source gas and a nitriding gas to form a nitride film on the substrate, and supply a purge gas to purge an interior of the chamber;
an exhauster configured to exhaust the interior of the chamber; and
a controller configured to control the heater, the gas supply, and the exhauster,
wherein the controller controls the heater, the gas supply, and the exhauster such that the film forming method of claim 1 is performed.