# US 2019/0378664 A1 · Contact material, method of manufacturing same, and vacuum valve

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0378664 A1
- Document ID: US20190378664A1
- Status: Published application
- Kind: A1
- Application number: 16/477,410
- Filed: 2017-10-24
- Published: 2019-12-12
- Earliest claimed: 2017-02-22
- Assignees: Mitsubishi Electric Corporation
- Applicants: Mitsubishi Electric Corporation
- Inventors: Hiroyuki CHIBAHARA
- Web page: https://patentgrep.com/patent/US20190378664A1

## CPC

- C23C 18/32: Coating with nickel, cobalt or mixtures thereof with phosphorus or boron (C23C18/50 takes precedence)
- B22F 1/18: Non-metallic particles coated with metal
- B22F 3/16: in successive or repeated steps
- C22C 1/05: Mixtures of metal powder with non-metallic powder (C22C1/08 takes precedence)
- C22C 9/00: Alloys based on copper
- C22C 19/03: based on nickel
- C22C 29/08: based on tungsten carbide
- C23C 18/1639: {Substrates other than metallic, e.g. inorganic or organic or non-conductive}
- C23C 18/1692: {Heat-treatment}
- H01H 1/0203: {specially adapted for vacuum switches}
- H01H 1/0233: and containing carbides
- H01H 1/025: having copper as the basic material
- H01H 11/04: of switch contacts
- B22F 2301/10: Copper
- B22F 2301/15: Nickel or cobalt
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C23C 18/36: using hypophosphites
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01H: ELECTRIC SWITCHES; RELAYS; SELECTORS; EMERGENCY PROTECTIVE DEVICES (contact cables H01B7/10; electrolytic self-interrupters H01G9/18; emergency protective circuit arrangements H02H; switching by electronic means without contact-making H03K17/00)

## Abstract

Provided is a method of manufacturing a contact material, including the steps of: forming a Ni alloy film having a film thickness of 40 nm or more and 110 nm or less on a surface of WC powder having an average particle diameter of 2 μm or more and 10 μm or less by an electroless Ni plating method; performing heat treatment for degassing at a temperature of 500° C. or more and 860° C. or less; crushing Ni alloy-coated WC powder after the heat treatment; mixing the crushed Ni alloy-coated WC powder and Cu powder having an average particle diameter of 1 μm or more and 100 μm or less; and compressing the resultant mixture, followed by sintering the mixture at a temperature of more than 1,083° C. and less than 1,455° C.

## Claims

### Claim at position 1

1-5. (canceled)

### Claim at position 2

6: A contact material having a structure in which WC particles each coated with a Ni alloy are dispersed in a matrix formed of Cu,
wherein a content of the Ni alloy with respect to the contact material falls within a range of 1.2 mass % or more and 3.7 mass % or less, and
wherein a relative density of the contact material is 90% or more of a theoretical density of the contact material.

### Claim at position 3 (depends on 6)

7: The contact material according to claim 6, wherein the Ni alloy is a Ni—P alloy.

### Claim at position 4 (depends on 6)

8: The contact material according to claim 6, wherein the content of the Ni alloy with respect to the contact material falls within a range of 1.2 mass % or more and 3.7 mass % or less, and a balance being Cu, WC and unavoidable impurities.

### Claim at position 5 (depends on 7)

9: The contact material according to claim 7, wherein the content of the Ni alloy with respect to the contact material falls within a range of 1.2 mass % or more and 3.7 mass % or less, and a balance being Cu, WC and unavoidable impurities.

### Claim at position 6

10: A method of manufacturing a contact material, the method comprising:
forming a Ni alloy film having a film thickness of 40 nm or more and 110 nm or less on a surface of WC powder having an average particle diameter of 2 μm or more and 10 μm or less by an electroless Ni plating method;
performing heat treatment for degassing at a temperature of 500° C. or more and 860° C. or less;
crushing Ni alloy-coated WC powder after the heat treatment;
mixing the crushed Ni alloy-coated WC powder and Cu powder having an average particle diameter of 1 μm or more and 100 μm or less; and
compressing the resultant mixture, followed by sintering the mixture at a temperature of more than 1,083° C. and less than 1,455° C.

### Claim at position 7 (depends on 10)

11: The method of manufacturing a contact material according to claim 10, further comprising:
recompressing the resultant sintered compact, followed by resintering the sintered compact at a temperature of more than 1,083° C. and less than 1,455° C.

### Claim at position 8 (depends on 6)