# US 2019/0377105 A1 · Flexible window stack structure and display device including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0377105 A1
- Document ID: US20190377105A1
- Status: Published application
- Kind: A1
- Application number: 16/547,929
- Filed: 2019-08-22
- Published: 2019-12-12
- Earliest claimed: 2017-02-22
- Assignees: Dongwoo Fine-Chem Co., Ltd.
- Applicants: Dongwoo Fine-Chem Co., Ltd.
- Inventors: Geo San LIM; Seung Hee KIM
- Web page: https://patentgrep.com/patent/US20190377105A1

## CPC

- C09D 4/00: Coating compositions, e.g. paints, varnishes or lacquers, based on organic non-macromolecular compounds having at least one polymerisable carbon-to-carbon unsaturated bond {; Coating compositions, based on monomers of macromolecular compounds of groups C09D183/00 - C09D183/16}
- B32B 7/02: Physical, chemical or physicochemical properties
- B32B 27/08: of synthetic resin
- B32B 27/30: comprising vinyl {(co)polymers; comprising acrylic (co)polymers}
- C08F 292/00: Macromolecular compounds obtained by polymerising monomers on to inorganic materials
- C08J 7/042: {with two or more layers, where at least one layer of a composition contains a polymer binder}
- C08J 7/0427: {with only one layer of a composition containing a polymer binder (with more layers C08J7/042)}
- C08J 7/046: Forming abrasion-resistant coatings; Forming surface-hardening coatings
- C09D 135/02: Homopolymers or copolymers of esters (C09D135/06, C09D135/08 take precedence)
- C09D 151/10: grafted on to inorganic materials
- G02B 1/14: Protective coatings, e.g. hard coatings
- G02B 6/32: having lens focusing means {positioned between opposed fibre ends (with lens being an integral part of the single fibre end G02B6/262)}
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- C08J 2379/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08J 2435/02: Characterised by the use of homopolymers or copolymers of esters (C08J2435/06, C08J2435/08 take precedence)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A flexible window stack structure includes a substrate, a first hard coating layer formed on a surface of the substrate and a second hard coating layer formed on an opposite surface of the substrate. The first hard coating layer has a curing contraction greater than that of the second hard coating layer, and the second hard coating layer is disposed at an elongated side when the window stack structure is folded. Cracks may be prevented by a curl property of the first hard coating layer when being bent.

## Claims

### Claim 1

A flexible window stack structure, comprising:
a substrate;
a first hard coating layer formed on a surface of the substrate; and
a second hard coating layer formed on an opposite surface of the substrate,
wherein the first hard coating layer has a curing contraction greater than that of the second hard coating layer, and the second hard coating layer is disposed at an elongated side when the window stack structure is folded.

### Claim 2 (depends on 1)

The flexible window stack structure according to claim 1, wherein the window stack structure has a normal curl in a folding direction such that a surface of the first hard coating layer faces each other.

### Claim 3 (depends on 2)

The flexible window stack structure according to claim 2, wherein a degree of the normal curl is in a range from 5 to 50 mm.

### Claim 4 (depends on 1)

The flexible window stack structure according to claim 1, wherein the first hard coating layer and the second hard coating layer are formed of a hard coating composition that includes a photo-curable compound containing an acrylate functional group, a photo-initiator and a solvent.

### Claim 5 (depends on 4)

The flexible window stack structure according to claim 4, wherein the first hard coating layer and the second hard coating layer have the same thickness, and
a functionality relative to a molecular weight of the photo-curable compound used in the first hard coating layer is greater than that in the second hard coating layer.

### Claim 6 (depends on 4)

The flexible window stack structure according to claim 4, wherein a thickness of the first hard coating layer is greater than that of the second hard coating layer.

### Claim 7 (depends on 1)

The flexible window stack structure according to claim 1, wherein the first hard coating layer or the second hard coating layer has a multi-layered structure.

### Claim 8 (depends on 1)

The flexible window stack structure according to claim 1, wherein the substrate includes at least one selected from a group consisting of polyimide (PI), polyethersulphone (PES), polyacrylate (PAR), polyetherimide (PEI), polyethyelenen napthalate (PEN), polyethyelene terephthalate (PET), polyphenylene sulfide (PPS), polyallylate, polycarbonate (PC), cellulose triacetate (TAC) and cellulose acetate propionate (CAP).

### Claim 9 (depends on 1)

A display device including the flexible window stack structure according to claim 1.

### Claim 10 (depends on 9)

The display device according to claim 9, wherein the image display device is a flexible display where the flexible window stack structure is bent along a direction in which the first hard coating layer is compressed.