# US 2019/0376960 A1 · Electrode for electrochemical sensors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0376960 A1
- Document ID: US20190376960A1
- Status: Published application
- Kind: A1
- Application number: 16/484,884
- Filed: 2018-01-30
- Published: 2019-12-12
- Earliest claimed: 2017-02-10
- Assignees: Eastman Chemical Company
- Applicants: Eastman Chemical Company
- Inventors: DENNIS LEE ASHFORD, II; SPENCER ERICH HOCHSTETLER
- Web page: https://patentgrep.com/patent/US20190376960A1

## CPC

- G01N 33/5438: {Electrodes}
- A61B 5/14532: {for measuring glucose, e.g. by tissue impedance measurement}
- A61B 5/1468: using chemical or electrochemical methods, e.g. by polarographic means
- A61B 5/1477: non-invasive
- C23C 14/08: Oxides (C23C14/10 takes precedence)
- C23C 14/14: Metallic material, boron or silicon
- C23C 14/34: Sputtering
- G01N 27/30: Electrodes, e.g. test electrodes; Half-cells (G01N27/414 takes precedence)
- G01N 27/327: Biochemical electrodes {, e.g. electrical or mechanical details for in vitro measurements}
- G01N 33/54393: {Improving reaction conditions or stability, e.g. by coating or irradiation of surface, by reduction of non-specific binding, by promotion of specific binding}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- G01N 2800/042: Disorders of carbohydrate metabolism, e.g. diabetes, glucose metabolism
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- A61B: DIAGNOSIS; SURGERY; IDENTIFICATION (usefulness limited to only animals A61D)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

An electrochemical electrode for use in a biosensor. The electrode comprises a substrate, a palladium metal layer manufactured on the substrate, and a palladium oxide-containing layer manufactured on the palladium metal layer. The palladium metal layer has a thickness of no more than 90 nm, and the palladium oxide-containing layer has a thickness of no more than 40 nm.

## Claims

### Claim 1

An electrochemical electrode for use in a biosensor, said electrode comprising:
(a) a substrate;
(b) a palladium metal layer manufactured on said substrate, wherein said palladium metal layer has a thickness of no more than 90 nm; and
(c) a palladium oxide-containing layer manufactured on said palladium metal layer, wherein said palladium oxide-containing layer has a thickness of no more than 40 nm.

### Claim 2 (depends on 1)

The electrochemical electrode of claim 1, wherein the biosensor is a medical sensor.

### Claim 3 (depends on 2)

The electrochemical electrode of claim 2, wherein the medical sensor is a blood glucose sensor.

### Claim 4 (depends on 1)

The electrochemical electrode of claim 1, wherein said electrode has a thickness of at least 5 nm and/or not more than 110 nm.

### Claim 5 (depends on 1)

The electrochemical electrode of claim 1, wherein said palladium metal layer has a thickness of at least 4 nm and/or not more than 80 nm.

### Claim 6 (depends on 1)

The electrochemical electrode of claim 1, wherein said palladium oxide-containing layer has a thickness of at least 0.5 nm and/or not more than 30 nm.

### Claim 7 (depends on 1)

The electrochemical electrode of claim 1, wherein said palladium metal layer is sputter coated on said substrate.

### Claim 8 (depends on 1)

The electrochemical electrode of claim 1, wherein said palladium oxide-containing layer is sputter coated on said palladium metal layer.

### Claim 9 (depends on 1)

The electrochemical electrode of claim 1, wherein said palladium metal layer is sputter coated on said substrate and said palladium oxide-containing layer is sputter coated on said palladium metal layer.

### Claim 10 (depends on 1)

The electrochemical electrode of claim 1, wherein said palladium metal layer is sputter coated on the substrate in a first atmosphere consisting essentially of an inert gas;
wherein the palladium oxide-containing layer is sputtered on the palladium metal layer in a second atmosphere comprising a mixture of the inert gas and an oxidant; and
wherein the oxidant makes up between 0.5 and 50% of the second atmosphere by partial pressure.

### Claim 11 (depends on 10)

The electrochemical electrode of claim 10, wherein the inert gas is argon.

### Claim 12 (depends on 10)

The electrochemical electrode of claim 10, wherein the oxidant is selected from one or more of the following: oxygen, ozone, and water.

### Claim 13 (depends on 10)

The electrochemical electrode of claim 10, wherein the oxidant is oxygen, and wherein oxygen makes up between 1 and 20% of the second atmosphere by partial pressure.

### Claim 14 (depends on 10)

The electrochemical electrode of claim 10, wherein a ratio of the sputtering power used during said sputtering of the palladium metal layer and said sputtering of the palladium oxide-containing layer is about 4:1.

### Claim 15 (depends on 1)

The electrochemical electrode of claim 1, wherein said palladium oxide-containing layer has a thickness that is not more than 40% of said palladium metal layer.

### Claim 16 (depends on 1)

The electrochemical electrode of claim 1, wherein said substrate comprises a polymeric film.

### Claim 17 (depends on 1)

The electrochemical electrode of claim 1, wherein said substrate comprises a polyester or polycarbonate.

### Claim 18 (depends on 1)

The electrochemical electrode of claim 1,
wherein said electrode is configured to receive a particular fractional surface coverage (fractional coverage A) of Mercaptoethanesulphonate (MESA), as determined by the Type 1 MESA Coverage Test, on an outer surface of said electrode upon said electrode being coated in MESA, via a MESA Coating Procedure, within 10 days of said palladium metal layer and said palladium oxide-containing layer being formed,
wherein said electrode is configured to receive a separate fractional surface coverage (fractional coverage B) of MESA, as determined by the Type 1 MESA Coverage Test, on the outer surface of said electrode upon said electrode being coated in MESA, via the MESA Coating Procedure, after 90 days of said palladium metal layer and said palladium oxide-containing layer being formed,
wherein the fractional coverage A deviates by no more than 30% from the fractional coverage B.

### Claim 19 (depends on 18)

The electrochemical electrode of claim 18, wherein the fractional coverage A deviates by no more than 20% from the fractional coverage B.