# US 2019/0376363 A1 · Swellable Packers and Methods for Activating Swellable Packers in a Downhole Environment

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0376363 A1
- Document ID: US20190376363A1
- Status: Published application
- Kind: A1
- Application number: 16/480,092
- Filed: 2018-02-20
- Published: 2019-12-12
- Earliest claimed: 2017-03-16
- Assignees: Halliburton Energy Services, Inc.
- Applicants: Halliburton Energy Services, Inc.
- Inventors: Sunita Sameer Kadam; Vaishali Mishra; Rahul Chandrakant Patil; Mohamed A. Salam; Ravikant S. Belakshe; Siddharth Roy; Vilas Ramtenki
- Web page: https://patentgrep.com/patent/US20190376363A1

## CPC

- E21B 33/1208: {characterised by the construction of the sealing or packing means (E21B33/1277 takes precedence)}
- E21B 33/13: Methods or devices for cementing, for plugging holes, crevices or the like
- C09K 8/42: Compositions for cementing, e.g. for cementing casings into boreholes; Compositions for plugging, e.g. for killing wells (compositions for plastering C09K8/50)
- C09K 8/44: containing organic binders only
- E21B 29/02: by explosives or by thermal or chemical means {(freeing stuck objects by explosives E21B31/002)}
- E21B 33/12: Packers; Plugs (used for cementing E21B33/134, E21B33/16)
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

Methods for producing a swellable packer in a downhole environment are provided. A method includes introducing a treatment fluid containing a polymeric composition into a wellbore within the downhole environment and exposing the polymeric composition to an acid to produce a swollen polymeric material within the downhole environment. The polymeric composition contains a reaction product of at least one or more monomers, one or more comonomers, and one or more crosslinkers. The acid can be in situ formed from an acid precursor introduced into the downhole environment.

## Claims

### Claim 1

A method for producing a swellable packer in a downhole environment, comprising:
introducing a treatment fluid comprising a polymeric composition into a wellbore within the downhole environment, wherein the polymeric composition comprises a reaction product of at least:
a monomer having the chemical formula:
wherein:
each R1 is independently a C1-C10 alkyl,
R2 is a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group, and
m is an integral in a range from 1 to 5;
a comonomer having the chemical formula:
R3—CH═CH2,
wherein:
R3 is a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group; and
a crosslinker having the chemical formula:
wherein:
each R4 is independently a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group; and
n is an integral in a range from 1 to 5; and
exposing the polymeric composition to an acid to produce a swollen polymeric material within the downhole environment.

### Claim 2 (depends on 1)

The method of claim 1, wherein the downhole environment comprises a formation comprising a passageway, and wherein the swollen polymeric material is in contact with the formation within the passageway and forms a plug blocking fluid communication between the passageway and the wellbore.

### Claim 3 (depends on 2)

The method of claim 2, further comprising exposing the swollen polymer to an alkaline agent to reduce the swollenness of the swollen polymer and open the fluid communication between the passageway and the wellbore.

### Claim 4 (depends on 2)

The method of claim 2, further comprising exposing the swollen polymer to an oxidizing agent to break apart the swollen polymer into smaller pieces and open the fluid communication between the passageway and the wellbore.

### Claim 5 (depends on 1)

The method of claim 1, wherein the monomer has the chemical formula:
and
wherein:
each R1 is independently a C1-C5 alkyl, and
R2 is a C1-C5 alkyl, a phenyl, or an aryl.

### Claim 6 (depends on 5)

The method of claim 5, wherein each R1 and R2 is independently a C1-C3 alkyl, and wherein R3 is a phenyl, an aryl, or a C1-C10 alkyl.

### Claim 7 (depends on 1)

The method of claim 1, wherein the crosslinker has the chemical formula:
and
wherein each R4 is independently a C1-C5 alkyl, a phenyl, or an aryl.

### Claim 8 (depends on 1)

The method of claim 1, wherein the polymeric composition is produced by reacting together:
about 65 mol % to about 90 mol % of the monomer,
about 10 mol % to about 30 mol % of the comonomer, and
about 0.5 mol % to about 5 mol % of the crosslinker.

### Claim 9 (depends on 1)

The method of claim 1, wherein the polymeric composition is produced by reacting the monomer, the comonomer, the crosslinker, and a radical initiator.

### Claim 10 (depends on 1)

The method of claim 1, wherein the acid comprises an organic acid, and wherein the polymeric composition is exposed to the organic acid produce the swollen polymeric material.

### Claim 11 (depends on 10)

The method of claim 10, wherein the organic acid is generated in situ the downhole environment and in the presence of the polymeric composition.

### Claim 12

A method for producing a swellable packer in a downhole environment, comprising:
introducing a treatment fluid comprising a polymeric composition and an acid precursor into a wellbore within the downhole environment, wherein the polymeric composition comprises a reaction product of at least:
a monomer having the chemical formula:
wherein:
each R1 is independently a C1-C10 alkyl,
R2 is a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group, and
m is an integral in a range from 1 to 5;
a comonomer having the chemical formula:
R3—CH═CH2,
wherein:
R3 is a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group; and
a crosslinker having the chemical formula:
wherein:
each R4 is independently a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group; and
n is an integral in a range from 1 to 5; and
forming an acid from the acid precursor within the downhole environment; and
exposing the polymeric composition to the acid to produce a swollen polymeric material within the downhole environment.

### Claim 13 (depends on 12)

The method of claim 12, wherein the downhole environment comprises a formation comprising a passageway, and wherein the swollen polymeric material is in contact with the formation within the passageway and forms a plug blocking fluid communication between the passageway and the wellbore.

### Claim 14 (depends on 13)

The method of claim 13, further comprising exposing the swollen polymer to an alkaline agent to reduce the swollenness of the swollen polymer and open the fluid communication between the passageway and the wellbore.

### Claim 15 (depends on 13)

The method of claim 13, further comprising exposing the swollen polymer to an oxidizing agent to break apart the swollen polymer into smaller pieces and open the fluid communication between the passageway and the wellbore.

### Claim 16 (depends on 12)

The method of claim 12, wherein the acid precursor comprises:
a substituted or unsubstituted (C1-C20)hydrocarbyl ester of a substituted or unsubstituted (C1-C20)alkanoic acid;
a homo- or hetero-anhydride of a substituted or unsubstituted (C1-C20)alkanoic acid; or
a combination thereof.

### Claim 17 (depends on 12)

The method of claim 12, wherein the acid precursor comprises:
a (C1-C5)alkyl ester of a substituted or unsubstituted (C1-C5)alkanoic acid;
a (C1-C5)alkyl ester or anhydride of a mono- or poly-hydroxy substituted (C1-C5)alkanoic acid; or
a combination thereof.

### Claim 18 (depends on 12)

The method of claim 12, wherein the acid precursor comprises a substituted or unsubstituted (C1-C20)hydrocarbyl ester or anhydride of at least one of formic acid, acetic acid, lactic acid, glycolic acid, propionic acid, or any combination thereof.

### Claim 19 (depends on 12)

The method of claim 12, wherein the acid precursor comprises at least one of diethylene glycol diformate, ethylene glycol monoformate, ethyl lactate, ethyl formate, methyl formate, glycerin diacetate, methyl lactate, or any combination thereof.

### Claim 20

A method for producing a swellable packer in a downhole environment, comprising:
introducing a treatment fluid comprising a polymeric composition and an acid precursor into a wellbore within the downhole environment, wherein the polymeric composition comprises a reaction product of at least:
a monomer having the chemical formula:
wherein:
each R1 is independently a C1-C10 alkyl,
R2 is a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group, and
m is an integral in a range from 1 to 5;
a comonomer having the chemical formula:
R3—CH═CH2,
wherein:
R3 is a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group; and
a crosslinker having the chemical formula:
wherein:
each R4 is independently a substituted or unsubstituted linear, branched, cyclic, heterocyclic, or aromatic hydrocarbyl group; and
n is an integral in a range from 1 to 5; and
forming an acid from the acid precursor within the downhole environment;
exposing the polymeric composition to the acid to produce a swollen polymeric material within the downhole environment;
forming a plug comprising the swollen polymeric material, wherein the downhole environment comprises a formation comprising a passageway, wherein the plug is in contact with the formation within the passageway and blocks fluid communication between the passageway and the wellbore;
perform a drilling or production process in the wellbore; and subsequently