# US 2019/0376175 A1 · Hard decorative member and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0376175 A1
- Document ID: US20190376175A1
- Status: Published application
- Kind: A1
- Application number: 16/435,685
- Filed: 2019-06-10
- Published: 2019-12-12
- Earliest claimed: 2018-06-11
- Assignees: Citizen Watch Co., Ltd.
- Applicants: Citizen Watch Co., Ltd.
- Inventors: Rikuto YOSHIDA
- Web page: https://patentgrep.com/patent/US20190376175A1

## CPC

- C23C 14/18: on other inorganic substrates
- C22C 5/02: Alloys based on gold
- C22C 14/00: Alloys based on titanium
- C23C 14/0015: {characterized by the colour of the layer}
- C23C 14/024: {Deposition of sublayers, e.g. to promote adhesion of the coating (C23C14/027 takes precedence)}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/16: on metallic substrates or on substrates of boron or silicon
- C23C 14/30: by electron bombardment
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A hard decorative member of the invention includes a gold alloy layer that is formed as a film by a dry plating method on a base material made of titanium or composed of a base and titanium formed on a surface of the base. The hard decorative member includes an undercoat layer that is formed on the base material and includes titanium carbon nitride, an adhesion layer that is formed on the undercoat layer and includes titanium carbon nitride, gold, copper and palladium, and a gold alloy layer that is formed on the adhesion layer and includes gold, copper and palladium. The gold alloy layer contains 70.3 to 75.2% by weight of gold, 20.7 to 25.6% by weight of copper, and 3.7 to 4.3% by weight of palladium.

## Claims

### Claim 1

A hard decorative member that includes a gold alloy layer formed as a film by a dry plating method on a base material made of titanium or composed of a base and titanium formed on a surface of the base, the hard decorative member comprising:
an undercoat layer that is formed on the base material and includes titanium carbon nitride;
an adhesion layer that is formed on the undercoat layer and includes titanium carbon nitride, gold, copper and palladium; and
a gold alloy layer that is formed on the adhesion layer and includes gold, copper, and palladium, wherein
the gold alloy layer contains 70.3 to 75.2% by weight of gold, 20.7 to 25.6% by weight of copper and 3.7 to 4.3% by weight of palladium.

### Claim 2 (depends on 1)

The hard decorative member according to claim 1, wherein
the gold alloy layer has a Vickers hardness of from 700 to 800 in a layer structure composed of the undercoat layer, the adhesion layer and the gold alloy layer.

### Claim 3 (depends on 1)

The hard decorative member according to claim 1, wherein
a color evaluation according to an L*a*b* color specification system of the gold alloy layer satisfies that 84.6≤L*≤85.4, 5.9≤a*≤6.1 and 10.3≤b*≤10.6.

### Claim 4 (depends on 1)

The hard decorative member according to claim 1, wherein
the undercoat layer has a Vickers hardness of from 2100 to 2400.

### Claim 5 (depends on 1)

The hard decorative member according to claim 1, wherein
the undercoat layer contains 65.3 to 69.5% by weight of titanium, 4.9 to 5.9% by weight of carbon and 25.6 to 29.9% by weight of nitrogen.

### Claim 6 (depends on 1)

The hard decorative member according to claim 1, wherein
a color evaluation according to an L*a*b* color specification system of the undercoat layer satisfies that 70.6≤L*≤73.0, 5.0≤a*≤7.1 and 11.7≤b*≤15.2.

### Claim 7

A method for manufacturing a hard decorative member, comprising:
an undercoat layer-forming step of forming an undercoat layer including titanium carbon nitride on a base material made of titanium or composed of a base and titanium formed on a surface of the base;
an adhesion layer-forming step of forming an adhesion layer on the undercoat layer, the adhesion layer including titanium carbon nitride, gold, copper and palladium; and
a gold alloy layer-forming step of forming a gold alloy layer on the adhesion layer, the gold alloy layer containing 70.3 to 75.2% by weight of gold, 20.7 to 25.6% by weight of copper and 3.7 to 4.3% by weight of palladium.

### Claim 8 (depends on 7)

The method for manufacturing a hard decorative member according to claim 7, wherein
at the undercoat layer-forming step, the undercoat layer containing 65.3 to 69.5% by weight of titanium, 4.9 to 5.9% by weight of carbon and 25.6 to 29.9% by weight of nitrogen is formed.

### Claim 9 (depends on 7)

The method for manufacturing a hard decorative member according to claim 7, wherein
at the undercoat layer-forming step, titanium is vaporized while argon gas, nitrogen gas and methane gas are introduced into a chamber of a vacuum device, and a cathode voltage is applied to the base material.

### Claim 10 (depends on 7)

The method for manufacturing a hard decorative member according to claim 7, wherein
at the adhesion layer-forming step, titanium and a gold alloy including gold, copper and palladium are vaporized while argon gas, nitrogen gas and methane gas are introduced into a chamber of a vacuum device, and a cathode voltage is applied to the base material.

### Claim 11 (depends on 7)

The method for manufacturing a hard decorative member according to claim 7, wherein
at the gold alloy layer-forming step, a gold alloy including gold, copper and palladium is vaporized while argon gas is introduced into a chamber of a vacuum device, and a cathode voltage is applied to the base material.