# US 2019/0376164 A1 · Austenitic alloy with high aluminum content and associated design process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0376164 A1
- Document ID: US20190376164A1
- Status: Published application
- Kind: A1
- Application number: 16/435,265
- Filed: 2019-06-07
- Published: 2019-12-12
- Earliest claimed: 2018-06-07
- Assignees: Manoir Pitres; Institut National des Sciences Appliquées Rouen Normandie; Universite De Rouen Normandie; Centre National De La Recherche Scientifique
- Applicants: Manoir Pitres; Université de Rouen Normandie; Centre National de la Recherche Scientifique; Institut National des Sciences Appliquées Rouen Normandie
- Inventors: Mathieu Couvrat; Antoine Facco; Cristelle Pareige
- Web page: https://patentgrep.com/patent/US20190376164A1

## CPC

- C22C 19/05: with chromium
- C22C 19/051: {and Mo or W}
- C22C 19/055: {with the maximum Cr content being at least 20% but less than 30%}
- C22C 38/44: with molybdenum or tungsten
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

An austenitic alloy based on nickel, chromium and iron, and having a high aluminum content, intended for use at a given operating temperature (Ts) between 900° C. and 1200° C., the alloy comprising the following elements, in weight percent: chromium between 20% and 32%, nickel between 30% and 60%, aluminum between 3.5% and 6%, carbon between 0.4% and 0.7%, titanium between 0.05% and 0.3%, niobium and/or tantalum between 0.6% and 2%, an element, composed of at least one rare earth and/or hafnium, between 0.002% and 0.1%, silicon between 0 and 0.5%, manganese between 0 and 0.5%, tungsten between 0 and 2%, and iron as the balance of the elements in the alloy. The alloy has less than 1% by volume of an intermetallic B2-NiAl phase and less than 1% by volume of an alpha prime phase rich in chromium, after subjecting the alloy to an operating temperature (Ts).

## Claims

### Claim 1

An austenitic alloy based on nickel, chromium and iron, and having a high aluminum content, for use at a given operating temperature (Ts) between 900° C. and 1200° C., the alloy comprising the following elements, in weight percent:
chromium between 20% and 32%,
nickel between 30% and 60%,
aluminum between 3.5% and 6%,
carbon between 0.4% and 0.7%,
titanium between 0.05% and 0.3%,
niobium and/or tantalum between 0.6% and 2%,
an element, composed of at least one rare earth and/or of hafnium, between 0.002% and 0.1%,
silicon between 0 and 0.5%,
manganese between 0 and 0.5%,
tungsten between 0 and 2%,
iron as a balance of the elements in the alloy;
and having less than 1% by volume of an intermetallic B2-NiAl phase and less than 1% by volume of an alpha prime chromium-rich phase, after subjecting the alloy to an operating temperature (Ts).

### Claim 2 (depends on 1)

The austenitic alloy of claim 1, wherein the mass percentages of aluminum XAl, nickel xNi, chromium xCr, titanium xTi, carbon xC, niobium xNb, tantalum xTa, silicon xSi and manganese xMn, satisfy the two following relationships (R3, R4):
−28.3xAl2+455.4xAl−0.32xNi2+15.3xNi−0.22xCr2+20.7xCr+121xSi+27xMn+16xTi+12xNb+16xTa−45xC−866≤Ts, (R3)
and
1.8xAl2+38.3xAl+0.42xNi2−51.2xNi+27.8xCr+34xSi+8xMn+89xTi+39xNb+22xTa−334xC+1572≤Ts, (R4)
where Ts represents the operating temperature.

### Claim 3 (depends on 2)

The austenitic alloy of claim 2, wherein the weight percentage of nickel xNi is defined by solving second degree equations (E3, E4) resulting from the relationships (R3, R4) linking the weight percentages of the alloy elements and the operating temperature Ts.

### Claim 4 (depends on 3)

The austenitic alloy of claim 3, wherein the weight percentage of nickel xNi is between a value (X), greater than 30%, consisting of the largest value between the solutions (X′, X″) of equations (E3, E4), and a value X plus ten (X+10).

### Claim 5 (depends on 4)

The austenitic alloy of claim 4, wherein the sum of the percentages of niobium and tantalum is greater than 0.6% and less than or equal to 2%.

### Claim 6 (depends on 5)

The austenitic alloy of claim 5, wherein the weight percentage of aluminum in the alloy is greater than 3.8% or even greater than 4%.

### Claim 7 (depends on 5)

The austenitic alloy of claim 5, wherein the weight percentage of aluminum in the alloy is greater than 3.8% or even greater than 4%.

### Claim 8 (depends on 6)

The austenitic alloy of claim 6, wherein the weight percentage of chromium in the alloy is less than 30%.

### Claim 9 (depends on 8)

The austenitic alloy of claim 8, wherein the weight percentage of chromium in the alloy is less than 28%.

### Claim 10 (depends on 7)

The austenitic alloy of claim 7, wherein the total weight percentage of rare earths and/or hafnium in the alloy is between 0.002% and 0.05%.

### Claim 11 (depends on 1)

The austenitic alloy of claim 1, wherein the sum of the percentages of niobium and tantalum is greater than 0.6% and less than or equal to 2%.

### Claim 12 (depends on 1)

The austenitic alloy of claim 1, wherein the weight percentage of aluminum in the alloy is greater than 3.8%.

### Claim 13 (depends on 1)

The austenitic alloy of claim 1, wherein the weight percentage of chromium in the alloy is less than 30% or even less than 28%.

### Claim 14 (depends on 13)

The austenitic alloy of claim 13, wherein the weight percentage of chromium in the alloy is less than 28%.

### Claim 15 (depends on 1)

The austenitic alloy of claim 1, wherein the total weight percentage of rare earths and/or hafnium in the alloy is between 0.002% and 0.05%.

### Claim 16

A method of forming an austenitic alloy based on nickel, chromium and iron, and having a high aluminum content, for use at a given operating temperature (Ts) between 900° C. and 1200° C., and comprising alloying the following elements, in weight percent:
chromium between 20% and 32%,
nickel between 30% and 60%,
aluminum between 3.5% and 6%,
carbon between 0.4% and 0.7%,
titanium between 0.05% and 0.3%,
niobium and/or tantalum between 0.6 and 2%,
an element, composed of at least one rare earth and/or of hafnium, between 0.002% and 0.1%,
silicon between 0 and 0.5%,
manganese between 0 and 0.5%,
tungsten between 0 and 2%,
iron to balance the elements in the alloy;
the method comprising selecting the respective weight percentages of aluminum XAl, nickel xNi, chromium xCr, titanium xTi, carbon xC, niobium xNb, tantalum XTa, silicon xSi and manganese xMn, so that the alloy has less than 1% by volume of an intermetallic B2-NiAl phase and less than 1% by volume of an alpha prime phase rich in chromium, after subjecting the alloy to an operating temperature (Ts).

### Claim 17 (depends on 16)

The method of claim 16, wherein the weight percentages of aluminum xAl, nickel xNi, chromium xCr, titanium xTi, carbon xC, niobium xNb, tantalum xTa, silicon xSi and manganese xMn satisfy the two following relationships (R3, R4):
−28.3xAl2+455.4xAl−0.32xNi2+15.3xNi−0.22xCr2+20.7xCr+121xSi+27xMn+16xTi+12xNb+16xTa−45xC−866≤Ts, (R3)
and
1.8xAl2+38.3xAl+0.42xNi2−51.2xNi+27.8xCr+34xSi+8xMn+89xTi+39xNb+22xTa−334xC+1572≤Ts, (R4)
where Ts represents the operating temperature.

### Claim 18 (depends on 17)

The method of claim 17, wherein the nickel weight percentage xNi is defined by solving the second degree equations (E3, E4) resulting from the relationships (R3, R4) linking the weight percentages of the alloy elements and the operating temperature Ts, and wherein the nickel weight percentage xNi is between a value (X), greater than 30%, consisting of the largest value between the solutions (X′, X″) of the equations (E3, E4), and a value increased by ten (X+10).

### Claim 19 (depends on 18)

The method of claim 18, wherein the weight percentage of aluminum in the alloy is greater than 3.8%.

### Claim 20 (depends on 16)

The method of claim 16, wherein the weight percentage of aluminum in the alloy is greater than 3.8%.