# US 2019/0376156 A1 · Use of a duplex stainless steel object

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0376156 A1
- Document ID: US20190376156A1
- Status: Published application
- Kind: A1
- Application number: 16/470,743
- Filed: 2017-12-18
- Published: 2019-12-12
- Earliest claimed: 2016-12-21
- Assignees: Sandvik Intellectual Property AB
- Applicants: Sandvik Intellectual Property AB
- Inventors: Ulf KIVISÄKK
- Web page: https://patentgrep.com/patent/US20190376156A1

## CPC

- C21D 8/0273: {Final recrystallisation annealing}
- C21D 1/26: Methods of annealing
- C21D 6/004: {containing Cr and Ni}
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 9/08: for tubular bodies or pipes
- C21D 9/46: for sheet metals
- C21D 9/52: for wires; for strips {; for rods of unlimited length}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 2211/001: Austenite
- C21D 2211/005: Ferrite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present disclosure relates to the use of a solution-annealed object comprising a duplex stainless steel, having the following composition in weight % (wt %): C less than or equal to 0.03; Si less than or equal to 0.5; Mn less than or equal to 1.0; Ni 5.0 to 7.0; Cr 22.0 to 26.0; Mo 2.5 to 4.5; N 0.1 to 0.2; P less than or equal to 0.03; S less than or equal to 0.03; Cu less than or equal to 0.3; Al less than or equal to 0.10; the balance being Fe and inevitable impurities; wherein the duplex stainless steel fulfills the equation of Cr+50N≤35; and wherein the duplex stainless steel has a ferrite phase content in the range of from 40% to 60% by volume and an austenite phase content in the range of 40 to 60% by volume; in sea water applications.

## Claims

### Claim 1

A method of improving resistance to hydrogen induced stress corrosion of a solution-annealed object, the method comprising:
making the object from a duplex stainless steel consisting of a composition in weight % (wt %):
C
less than or equal to 0.03;
Si
less than or equal to 0.5;
Mn
less than or equal to 1.0;
Ni
5.0 to 7.0;
Cr
22.0 to 26.0;
Mo
2.5 to 4.5;
N
0.1 to 0.2;
P
less than or equal to 0.03;
S
less than or equal to 0.03;
Cu
less than or equal to 0.3;
Al
less than or equal to 0.10;
the balance being Fe and inevitable impurities;
wherein the duplex stainless steel fulfills the equation of Cr+50N≤35, and
wherein the duplex stainless steel has a ferrite phase content in the range of from 40% to 60% by volume and an austenite phase content in the range of 40 to 60% by volume, and
wherein the object is used in sea water applications.

### Claim 2 (depends on 1)

The method stool according to claim 1, wherein the content of Cr is of from 23.0 to 24.0 wt %.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the content of Ni is of from 6.0 to 7.0 wt %.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the content of N is of from 0.12 to 0.20 wt %.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the content of Mo is of from 2.8 to 4.0 wt %.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the content of Cu is less than or equal to 0.2 wt %.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the duplex stainless steel fulfills the equation of Cr+50N≤34.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the duplex stainless steel fulfills the equation of Cr+50N≤33.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the object is in the form of; a bar, a tube, a seamless or a welded tube, a constructive part, a plate, a sheet, a strip or a wire.

### Claim 10 (depends on 1)

The method according to claim 1, wherein making the object from a duplex stainless steel includes manufacturing by a process comprising the following steps:
a. melting;
b. casting;
c. hot working;
d. cold working;
e. solution annealing and wherein the solution annealing is performed at a temperature above the recristallisation temperature of said duplex stainless steel.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the solution annealing is performed in a temperature of from in the range of from 1030-1150° C.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the sea water application is as a cathode.