# US 2019/0375925 A1 · Insulating resin composition for dc power cable, crosslinked resin body, dc power cable, member for forming reinforcing insulating layer of dc power joint, and dc power cable joint

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0375925 A1
- Document ID: US20190375925A1
- Status: Published application
- Kind: A1
- Application number: 16/269,853
- Filed: 2017-07-26
- Published: 2019-12-12
- Earliest claimed: 2016-08-09
- Assignees: NUC Corporation; Furukawa Electric Co., Ltd.
- Applicants: NUC Corporation; Furukawa Electric Co., Ltd.
- Inventors: Hironori Mohri; Nobutaka Yuzawa; Takeshi Tachikawa; Anna Aso; Hiroki Mori; Naoto Shigemori; Saki Shigemori
- Web page: https://patentgrep.com/patent/US20190375925A1

## CPC

- C08K 5/13: Phenols; Phenolates
- C08L 23/06: Polyethylene
- C08K 5/14: Peroxides
- C08K 5/372: Sulfides {, e.g. R-(S)x-R'}
- C08L 51/06: grafted on to homopolymers or copolymers of aliphatic hydrocarbons containing only one carbon-to-carbon double bond
- H01B 3/441: {from alkenes}
- H01B 9/00: Power cables
- H01B 9/027: {composed of semi-conducting layers}
- H02G 15/18: protected by sleeves, e.g. for communication cable (two-part covers H02G15/10 {; preforms having internal stresses B29C61/00})
- C08L 2201/08: Stabilised against heat, light or radiation or oxydation
- C08L 2203/202: use in electrical wires or wirecoating
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2207/066: LDPE (radical process)
- C08L 2312/00: Crosslinking
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H02G: INSTALLATION OF ELECTRIC CABLES OR LINES, OR OF COMBINED OPTICAL AND ELECTRIC CABLES OR LINES

## Abstract

Provided is an insulating resin composition for a DC power cable, which insulating resin composition has excellent extrudability, is unlikely to experience sagging, has good scorch resistance, generates a smaller amount of secondary decomposition water, can form an insulating layer that stably exhibits good DC electrical properties, and has high extrusion stability. The insulating resin composition for a DC power cable according to the present invention includes (A) a low-density polyethylene having a complex viscosity η*100, which is measured at 130° C. and a frequency of 100 rad/s, of 600 to 1,300 Pa·s, wherein a ratio (η*0.1/η*100) of a complex viscosity η*0.1, which is measured at 130° C. and a frequency of 0.1 rad/s, to the complex viscosity η*100 is 4 or more; (B) a modified polyethylene; and (C) a stabilizer including a mixture of a hindered phenol antioxidant and a thioether antioxidant. The amount of carbonyl groups introduced into the resin composition through the component (B) is 7×10−6 to 1.3×10−5 mol/g relative to the total mass of the component (A), the component (B), and the component (C).

## Claims

### Claim 1

An insulating resin composition for a DC power cable, the resin composition comprising:
(A) 100 parts by mass of a low-density polyethylene having a complex viscosity η*100, which is measured at 130° C. and a frequency of 100 rad/s, of 600 to 1,300 Pa·s, wherein a ratio (η*0.1/η*100) of a complex viscosity η*0.1, which is measured at 130° C. and a frequency of 0.1 rad/s, to the complex viscosity η*100 is 4 or more;
(B) 5 to 12 parts by mass of a modified polyethylene obtained by grafting a polyethylene with at least one modifying monomer selected from unsaturated organic acids and derivatives thereof; and
(C) 0.01 to 0.8 parts by mass of a stabilizer including a mixture of 40% to 60% by weight of a hindered phenol antioxidant and 60% to 40% by weight of a thioether antioxidant,
wherein an amount of carbonyl groups introduced into the resin composition through the component (B) is 7×10−6 to 1.3×10−5 mol/g relative to a total mass of the component (A), the component (B), and the component (C).

### Claim 2 (depends on 1)

The resin composition for a DC power cable according to claim 1, wherein the component (B) is obtained by grafting a low-density polyethylene that satisfies the requirements for the component (A) with the modifying monomer.

### Claim 3 (depends on 1)

The insulating resin composition for a DC power cable according to claim 1, further comprising (D) 0.1 to 5 parts by mass of an organic peroxide.

### Claim 4 (depends on 3)

The insulating resin composition for a DC power cable according to claim 3,
wherein the component (D) has a melting point of 60° C. or lower, and
a decomposition time (half-life) at 130° C. of the component (D) is 1 to 5 hours.

### Claim 5 (depends on 1)

The insulating resin composition for a DC power cable according to claim 1, wherein the component (B) is a modified polyethylene obtained by grafting a polyethylene with at least one modifying monomer selected from unsaturated dicarboxylic acids, unsaturated dicarboxylic anhydrides, and unsaturated dicarboxylic acid derivatives.

### Claim 6 (depends on 1)

The insulating resin composition for a DC power cable according to claim 1, wherein the component (B) is a modified polyethylene obtained by grafting a polyethylene with maleic anhydride (MAH).

### Claim 7 (depends on 1)

A crosslinked resin body obtained by crosslinking the resin composition according to claim 1.

### Claim 8 (depends on 7)

The crosslinked resin body according to claim 7, wherein an amount of water generated by heating at 180° C. for 3 hours is 100 ppm or less.

### Claim 9 (depends on 7)

The crosslinked resin body according to claim 7, wherein an increase in electric field enhanced by internally accumulated charges is 25% or less, the increase in electric field being determined by space charge measurement.

### Claim 10 (depends on 7)

A DC power cable, wherein an inner semiconductive layer and an insulating layer made of the crosslinked resin body according to claim 7 are disposed in layers around a surface of a conductive member.

### Claim 11 (depends on 1)

A member for forming a reinforcing insulating layer of a DC power cable joint, the member comprising the resin composition according to claim 1, wherein the member is a tape-shaped repair member that, in connecting DC power cables together, is wound around a joint inner semiconductive layer covering exposed portions of conductive members of the DC power cables, the exposed portions including a joint between the conductive members, and is crosslinked to form a reinforcing insulating layer around the joint inner semiconductive layer.

### Claim 12 (depends on 7)

A DC power cable joint, wherein DC power cables are connected together, and a reinforcing insulating layer made of the crosslinked resin body according to claim 7 is formed around a joint inner semiconductive layer covering exposed portions of conductive members of the DC power cables, the exposed portions including a joint between the conductive members.