# US 2019/0375882 A1 · Toughened urethane acrylate compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0375882 A1
- Document ID: US20190375882A1
- Status: Published application
- Kind: A1
- Application number: 16/463,208
- Filed: 2017-09-07
- Published: 2019-12-12
- Earliest claimed: 2016-11-25
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Huifeng Qian; Rajat Duggal; Muhammad A. Shafi; Luigi Pellacani; Harshad M. Shah
- Web page: https://patentgrep.com/patent/US20190375882A1

## CPC

- C08G 18/7664: {containing alkylene polyphenyl groups}
- C08G 18/12: using two or more compounds having active hydrogen in the first polymerisation step
- C08G 18/246: {containing also tin-carbon bonds}
- C08G 18/4808: {Mixtures of two or more polyetherdiols}
- C08G 18/4829: {Polyethers containing at least three hydroxy groups (C08G18/4833 - C08G18/5096 take precedence)}
- C08G 18/6755: {Unsaturated carboxylic acids}
- C08G 18/7621: {being toluene diisocyanate including isomer mixtures}
- C09D 11/102: containing macromolecular compounds obtained by reactions other than those only involving unsaturated carbon-to-carbon bonds
- C09D 175/14: Polyurethanes having carbon-to-carbon unsaturated bonds
- C09D 175/16: having terminal carbon-to-carbon unsaturated bonds
- C09J 175/14: Polyurethanes having carbon-to-carbon unsaturated bonds
- C09J 175/16: having terminal carbon-to-carbon unsaturated bonds
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

In various embodiments, a resin composition includes a urethane (meth)acrylate, a reactive diluent, and a urethane (meth)acrylate toughener. The urethane (meth)acrylate toughener includes at least one additional polyol having a number average molecular weight Mn of greater than 1,000 g/mol. Cured articles made from the resin composition have an average fracture toughness (KIc) value from 1 MPa*m1/2 to 3 MPa*m1/2 when measured in accordance with ASTM D5045. Processes for making the resin composition as well as processes using the resin composition are also provided.

## Claims

### Claim 1

A resin composition comprising:
a urethane (meth)acrylate;
a reactive diluent; and
a urethane (meth)acrylate toughener comprising at least one additional polyol having a number average molecular weight Mn from 1,000 g/mol to 15,000 g/mol.

### Claim 2 (depends on 1)

The resin composition of claim 1, wherein the urethane (meth)acrylate is produced from the reaction of at least one polyisocyanate, at least one polyol, and a compound comprising a nucleophilic group and a (meth)acrylate group selected from the group consisting of hydroxyethyl acrylate, hydroxypropyl acrylate, hydroxyethyl methacrylate, hydroxyethyl acrylamide, hydroxypropyl acrylamide, and mixtures thereof.

### Claim 3 (depends on 1)

The resin composition of claim 1, further comprising a free radical-generating catalyst in an amount of from 0.1 wt % to 5 wt % based on a total weight of the resin composition.

### Claim 4 (depends on 1)

The resin composition of claim 1, wherein the at least one additional polyol is present in an amount of from 1.0 wt % to 20 wt % based on a total weight of the curable resin composition.

### Claim 5 (depends on 1)

The resin composition of claim 1, wherein the at least one additional polyol has a number average molecular weight Mn from 3,500 g/mol to 9,000 g/mol.

### Claim 6

A cured article comprising a composite, a coating, an adhesive, an ink, an encapsulation, or a casting prepared from a resin composition, the resin composition comprising:
a urethane (meth)acrylate;
a reactive diluent; and
a urethane (meth)acrylate toughener comprising at least one additional polyol having a number average molecular weight Mn from 1,000 g/mol to 15,000 g/mol.

### Claim 7 (depends on 6)

The cured article of claim 6, wherein the cured article has an average fracture toughness (KIC) value from 1 MPa*m1/2 to 3 MPa*m1/2 when measured in accordance with ASTM D5045.

### Claim at position 8

8-10. (canceled)

### Claim 11

A method of preparing a resin composition, comprising:
reacting a polyisocyanate, a polyol, and a compound containing both a nucleophilic group and a (meth)acrylate group to form urethane (meth)acrylate; and
mixing a reactive diluent and a urethane (meth)acrylate toughener with the urethane (meth)acrylate to form the resin composition, wherein
the urethane (meth)acrylate toughener comprises at least one additional polyol having a number average molecular weight Mn from 1,000 g/mol to 15,000 g/mol.

### Claim 12 (depends on 11)

The method of claim 11, wherein the method further comprises curing the resin composition at a temperature from 15° C. to 150° C.

### Claim 13 (depends on 11)

The method of claim 11, wherein the resin composition comprises an average fracture toughness (KIC) value from 1 MPa*m1/2 to 3 MPa*m1/2 when measured in accordance with ASTM D5045.

### Claim 14 (depends on 11)

The method of claim 11, wherein the resin composition comprises a viscosity of less than 10,000 cp.

### Claim 15 (depends on 11)

The method of claim 11, wherein the resin composition comprises a glass transition temperature, Tg, from 50° C. to 170° C.

### Claim 16 (depends on 1)

The resin composition of claim 1, further comprising an average fracture toughness (KIC) value from 1 MPa*m1/2 to 3 MPa*m1/2 when measured in accordance with ASTM D5045.

### Claim 17 (depends on 1)

The resin composition of claim 1, further comprising a viscosity of less than 10,000 cp.

### Claim 18 (depends on 1)

The resin composition of claim 1, further comprising a glass transition temperature, Tg, from 50° C. to 170° C.

### Claim 19 (depends on 6)

The cured article of claim 6, wherein the resin composition comprises a viscosity of less than 10,000 cp.

### Claim 20 (depends on 6)

The cured article of claim 6, wherein the resin composition comprises a glass transition temperature, Tg, from 50° C. to 170° C.