# US 2019/0375688 A1 · Sintering control method of ceramic manufacturing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0375688 A1
- Document ID: US20190375688A1
- Status: Published application
- Kind: A1
- Application number: 16/436,677
- Filed: 2019-06-10
- Published: 2019-12-12
- Earliest claimed: 2018-06-12
- Assignees: RegenBone Biomedical Inc.
- Applicants: RegenBone Biomedical Inc.
- Inventors: Tzong-Li LIN; Chih-Yang LIN; Lung-Yi CHEN; Chia-Jie CHEN
- Web page: https://patentgrep.com/patent/US20190375688A1

## CPC

- C04B 38/068: {Carbonaceous materials, e.g. coal, carbon, graphite, hydrocarbons}
- B28B 1/001: {Rapid manufacturing of 3D objects by additive depositing, agglomerating or laminating of material (selective deposition modelling of metallic powder B22F10/00; rapid manufacturing of 3D objects in general and in particular of plastics B29C64/00)}
- B28B 11/243: {Setting, e.g. drying, dehydrating or firing ceramic articles (B28B11/242 takes precedence)}
- B29C 64/153: using layers of powder being selectively joined, e.g. by selective laser sintering or melting
- B33Y 10/00: Processes of additive manufacturing
- B33Y 70/10: Composites of different types of material, e.g. mixtures of ceramics and polymers or mixtures of metals and biomaterials
- C04B 35/111: Fine ceramics
- C04B 35/16: based on silicates other than clay {(zircon C04B35/48)}
- C04B 35/18: rich in aluminium oxide
- C04B 35/195: Alkaline earth aluminosilicates, e.g. cordierite {or anorthite}
- C04B 35/478: based on aluminium titanates
- C04B 35/5607: {based on refractory metal carbides}
- C04B 35/5611: {based on titanium carbides}
- C04B 35/563: based on boron carbide
- C04B 35/565: based on silicon carbide
- C04B 35/58014: {based on titanium nitrides, e.g. TiAlON}
- C04B 35/583: based on boron nitride
- C04B 35/584: based on silicon nitride
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 38/00: Porous mortars, concrete, artificial stone or ceramic ware; Preparation thereof (treating slag with gases or gas generating material C04B5/06 {; expanded graphite C04B35/536})
- C04B 2111/00836: {for medical or dental applications}
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3232: Titanium oxides or titanates, e.g. rutile or anatase
- C04B 2235/3234: Titanates, not containing zirconia
- C04B 2235/3241: Chromium oxides, chromates, or oxide-forming salts thereof
- C04B 2235/3244: Zirconium oxides, zirconates, hafnium oxides, hafnates, or oxide-forming salts thereof
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/3427: Silicates other than clay, e.g. water glass
- C04B 2235/3463: Alumino-silicates other than clay, e.g. mullite
- C04B 2235/3481: Alkaline earth metal alumino-silicates other than clay, e.g. cordierite, beryl, micas such as margarite, plagioclase feldspars such as anorthite, zeolites such as chabazite
- C04B 2235/3821: Boron carbides
- C04B 2235/3839: Refractory metal carbides
- C04B 2235/3843: Titanium carbides
- C04B 2235/3847: Tungsten carbides
- C04B 2235/386: Boron nitrides
- C04B 2235/3873: Silicon nitrides, e.g. silicon carbonitride, silicon oxynitride
- C04B 2235/3886: Refractory metal nitrides, e.g. vanadium nitride, tungsten nitride
- C04B 2235/5248: Carbon, e.g. graphite
- C04B 2235/5288: Carbon nanotubes
- C04B 2235/6026: Computer aided shaping, e.g. rapid prototyping
- C04B 2235/656: characterised by specific heating conditions during heat treatment
- C04B 2235/6583: Oxygen containing atmosphere, e.g. with changing oxygen pressures
- C04B 2235/6584: at an oxygen percentage below that of air
- C04B 2235/661: Multi-step sintering
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING

## Abstract

The present invention provides a sintering control method of ceramic manufacturing. The method includes the following steps: S1: preparing a pore-forming agent containing a porogen; S2: mixing the pore-forming agent with a ceramic slurry and forming a greenpart; S3: sintering the greenpart at a first temperature in an oxygen-free environment to form a semi-finished object; and S4: sintering the semi-finished object at a second temperature in an oxygen-containing environment to form a ceramic article. Wherein, the first temperature is higher than the second temperature. While the porogen is a carbon-based material, the second temperature is from 300° C. to 600° C., and the porosity of the ceramic article may reach 30% to 70%. By this method, the property of the ceramic article (including mechanical strength, porosity, pore shape and size) can be designed according to requirement and controlled for quality assurance.

## Claims

### Claim 1

A sintering control method of ceramic manufacturing, comprising the following steps:
S1: preparing a pore-forming agent containing a porogen;
S2: mixing the pore-forming agent with a ceramic slurry and forming a greenpart;
S3: sintering the greenpart at a first temperature in an oxygen-free environment to form a semi-finished object; and
S4: sintering the semi-finished object at a second temperature in an oxygen-containing environment to form a ceramic article.
wherein, the second temperature is lower than the first temperature.

### Claim 2 (depends on 1)

The method of claim 1, wherein the porogen in the step S1 is a carbon-based material, an ore, a salt, a natural fiber or a high molecular polymer, and the carbon-based material is a carbon fiber, a carbon nanotube, a graphene or an expanded graphite.

### Claim 3 (depends on 2)

The method of claim 2, wherein the shape of the carbon-based material in the step S1 is spherical, plate, irregular, strip or cube.

### Claim 4 (depends on 1)

The method of claim 1, wherein the particle size of the porogen in the step S1 is from 50 nm to 400 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the step S2 further comprises the following steps:
S21: mixing the pore-forming agent with a ceramic slurry according to a predetermined ratio for forming a mixed raw material; and
S22: printing the mixed raw material by additive manufacturing for forming the greenpart.

### Claim 6 (depends on 5)

The method of claim 5, wherein the pore-forming agent in the step S21 accounts for the predetermined ratio of the mixed raw material from 10 wt % to 50 wt %.

### Claim 7 (depends on 1)

The method of claim 1, wherein the step S3 further comprises the following steps:
S31: injecting a stabilizing gas into a predetermined environment for establishing the oxygen-free environment; and
S32: sintering the greenpart at the first temperature in the oxygen-free environment for forming the semi-finished object.

### Claim 8 (depends on 7)

The method of claim 7, wherein the stabilizing gas in the step S31 is nitrogen gas, and the first temperature in the step S32 is higher than 600° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the step S4 further comprises the following steps:
S41: injecting air into a predetermined environment for establishing the oxygen-containing environment; and
S42: sintering the semi-finished object from 1 to 10 hours at the second temperature in the oxygen-containing environment for forming the ceramic article, wherein the second temperature is between 300° C. and 600° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the porosity of the ceramic article in the step S4 is from 30% to 70%.