# US 2019/0369325 A1 · High chlorine content low attenuation optical fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0369325 A1
- Document ID: US20190369325A1
- Status: Published application
- Kind: A1
- Application number: 16/543,967
- Filed: 2019-08-19
- Published: 2019-12-05
- Earliest claimed: 2014-07-10
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: George Edward Berkey; Dana Craig Bookbinder; Ming-Jun Li; Pushkar Tandon
- Web page: https://patentgrep.com/patent/US20190369325A1

## CPC

- G02B 6/02014: {Effective area greater than 60 square microns in the C band, i.e. 1530-1565 nm}
- C03B 37/01453: {for doping the preform with flourine}
- C03B 37/01815: {Reactant deposition burners or deposition heating means}
- C03B 37/0183: {for plasma within a tube substrate}
- C03B 37/01853: {Thermal after-treatment of preforms, e.g. dehydrating, consolidating, sintering}
- C03B 37/01869: {Collapsing}
- C03C 13/046: {Multicomponent glass compositions}
- G02B 6/03627: {arranged - +}
- C03B 37/01205: {starting from tubes, rods, fibres or filaments (C03B37/014 takes precedence)}
- C03B 37/01211: {by inserting one or more rods or tubes into a tube}
- C03B 37/01262: {Depositing additional preform material as liquids or solutions, e.g. solution doping of preform tubes or rods}
- C03B 37/01282: {by pressing or sintering, e.g. hot-pressing}
- C03B 37/01413: {Reactant delivery systems (C03B37/01807 takes precedence; devices therefor in general B01D1/00, B01J4/00)}
- C03B 37/01433: {for delivering and depositing additional reactants as liquids or solutions, e.g. for solution doping of the porous glass preform}
- C03B 37/01446: {Thermal after-treatment of preforms, e.g. dehydrating, consolidating, sintering (C03B37/01853 takes precedence)}
- C03B 37/018: by glass deposition on a glass substrate, e.g. by {inside-, modified-, plasma- or plasma modified-} chemical vapour deposition {[ICVD, MCVD, PCVD, PMCVD], i.e. by thin layer coating on the inside or outside of a glass tube or on a glass rod} (C03B37/016 takes precedence; surface treatment of glass by coating with glass C03C17/02)
- C03B 37/01838: {for delivering and depositing additional reactants as liquids or solutions, e.g. for solution doping of the deposited glass}
- C03B 2201/08: doped with boron or fluorine or other refractive index decreasing dopant
- C03B 2201/12: doped with fluorine (C03B2201/14 takes precedence)
- C03B 2201/20: doped with non-metals other than boron or fluorine
- C03B 2201/24: doped with nitrogen, e.g. silicon oxy-nitride glasses
- C03B 2203/22: Radial profile of refractive index, composition or softening point
- C03B 2203/23: Double or multiple optical cladding profiles
- C03B 2203/24: Single mode [SM or monomode]
- C03B 2205/42: Drawing at high speed, i.e. > 10 m/s
- C03B 2207/30: For glass precursor of non-standard type, e.g. solid SiH3F
- C03C 13/045: {Silica-containing oxide glass compositions}
- C03C 25/1061: {Inorganic coatings}
- C03C 2201/11: containing chlorine
- C03C 2201/12: containing fluorine (C03C2201/14 takes precedence)
- C03C 2203/54: in a dopant containing atmosphere
- C03C 2213/00: Glass fibres or filaments
- G02B 6/02019: {Effective area greater than 90 square microns in the C band, i.e. 1530-1565 nm}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

An optical fiber having a core comprising silica and greater than 1.5 wt % chlorine and less than 0.5 wt % F, said core having a refractive index Δ1MAX, and an inner cladding region having refractive index Δ2MIN surrounding the core, where Δ1MAX>Δ2MIN.

## Claims

### Claim 1

A method for making an optical fiber preform, the method comprising:
exposing a silica soot core preform having a surface area greater than 10 m2/gm to an atmosphere comprising a chlorine-containing compound at temperatures higher than 1300° C. to form a chlorine doped soot core preform; and
sintering the soot core preform to form a core portion of the optical fiber preform such that the chlorine concentration in said core portion is greater than or equal to 1.5 wt % chlorine.

### Claim 2 (depends on 1)

The method of claim 1, further comprising forming a cladding layer over said core portion of said fiber preform, said cladding layer comprising fluorine, wherein the molar ratio of the chlorine in the core portion to the fluorine in the first inner cladding layer is ≥1.

### Claim 3 (depends on 1)

The method of claim 1, wherein the soot preform comprises greater than 0.5 wt % silicon monoxide (SiO).

### Claim 4 (depends on 1)

The method of claim 1, wherein the surface area of the silica soot preform is greater than 25 m2/gm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the surface area of the silica soot preform is greater than 50 m2/gm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the chlorine doping and sintering of the silica soot preform is done in an atmosphere containing SiCl4 having partial pressure of greater than 0.5 atm.

### Claim 7 (depends on 6)

The method of claim 6, wherein the chlorine doping and sintering of the silica soot preform is done in an atmosphere containing SiCl4 having partial pressure of greater than 1 atm.

### Claim 8 (depends on 2)

The method of claim 2, wherein the chlorine weight % in core portion of the optical fiber preform is greater than 1.5 wt % and fluorine weight % in cladding portion of optical fiber preform is less than 0.6 wt %.

### Claim 9 (depends on 1)

The method of claim 1, wherein said step of exposing the silica soot preform having to an atmosphere comprising a chlorine-containing compound comprises a first chlorine doping step comprising exposing the preform to an atmosphere comprising SiCl4, and subsequent to said first exposing step, exposing the preform to atmosphere comprising water or oxygen, and thereafter performing a second chlorine doping step in an atmosphere comprising SiCl4 at temperatures higher than 1300° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein said step of exposing the silica soot preform having to an atmosphere comprising a chlorine-containing compound comprises a first chlorine doping step comprising exposing the preform to an atmosphere comprising 1) a mixture of SiCl4 and water or 2) a mixture of SiCl4 and oxygen, and said method further comprises chlorine doping the preform in a second chlorine doping step in an atmosphere comprising SiCl4 at temperatures higher than 1300° C.

### Claim 11

A method for making a single mode optical fiber, the method comprising:
depositing, via a PCVD (plasma chemical vapor deposition) process, a core glass layer inside a glass tube which is comprised of SiO2, the glass layer comprising chlorine doped silica having greater than 3 wt % Cl; and
collapsing the tube to eliminate the open centerline and thereby forming an optical fiber preform.

### Claim 12 (depends on 11)

The method of claim 11 wherein the method further comprises forming at least one cladding layer on the outside of said tube, said cladding layer comprising fluorine doped silica.

### Claim 13 (depends on 12)

The method of claim 12 wherein the molar ratio of the chlorine in the core portion to the fluorine in the cladding layer is ≥1.

### Claim 14 (depends on 11)

The method of claim 11 wherein the silica glass tube comprises fluorine doped silica.