# US 2019/0368120 A1 · Compositions and methods for treating keratinous material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0368120 A1
- Document ID: US20190368120A1
- Status: Published application
- Kind: A1
- Application number: 16/220,393
- Filed: 2018-12-14
- Published: 2019-12-05
- Earliest claimed: 2014-04-19
- Assignees: Unshrinkit, Inc.
- Applicants: Unshrinkit, Inc.
- Inventors: Nathaniel Francis Barbera; Matthew Pendleton Kahn; Zack Nicholas Oakley; Aanchal Raj; Desiree Alexis Davis Stolar; Andrew Williams Watt; Mark Wayne Juckett; Evan Paul Boyst; Ian Alexander Von Wald
- Web page: https://patentgrep.com/patent/US20190368120A1

## CPC

- D06M 11/76: with carbon oxides or carbonates (D06M11/75 takes precedence; with percarbonic acids or their salts D06M11/50; with urea D06M13/432)
- D06M 11/52: with selenium, tellurium, polonium or their compounds; with sulfur, dithionites or compounds containing sulfur and halogens, with or without oxygen; by sulfohalogenation with chlorosulfonic acid; by sulfohalogenation with a mixture of sulfur dioxide and free halogens
- D06M 11/84: combined with mechanical treatment (combined with mechanical tension, e.g. mercerising D06M11/40)
- D06M 13/148: Polyalcohols, e.g. glycerol {or glucose}
- D06M 13/165: Ethers (D06M13/11 takes precedence)
- D06M 13/224: Esters of carboxylic acids; Esters of carbonic acid
- D06M 13/252: Mercaptans, thiophenols, sulfides or polysulfides, e.g. mercapto acetic acid; Sulfonium compounds
- D06M 13/285: Phosphines; Phosphine oxides; Phosphine sulfides; Phosphinic or phosphinous acids or derivatives thereof
- D06M 2101/12: Keratin fibres or silk
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS

## Abstract

Chemical compositions and techniques for treating wool (and other animal hair-based) fabrics, and in particular for unshrinking wool fabrics and garments.

## Claims

### Claim 1

A method for increasing the size of a shrunken material comprising keratinous material, the method comprising:
dissolving disulfide bonds in the shrunken material;
elongating the shrunken material; and
promoting reformation of disulfide bonds in the shrunken material.

### Claim 2 (depends on 1)

The method of claim 1, wherein dissolving disulfide bonds in the shrunken material comprises treating the shrunken material with an aqueous solution comprising a reducing agent.

### Claim 3 (depends on 2)

The method of claim 2, wherein elongating the shrunken material comprises physically stressing the material.

### Claim 4 (depends on 3)

The method of claim 3, wherein promoting reformation of disulfide bonds in the shrunken material comprises treating the shrunken material with a solvent to remove the reducing agent.

### Claim 5 (depends on 4)

The method of claim 4, further comprising drying the shrunken material without physically stressing the material during drying, drying occurring after treating the shrunken material with a solvent to remove the reducing agent.

### Claim 6 (depends on 2)

The method of claim 2, wherein the aqueous solution further comprises at least one of: a basic compound such as sodium bicarbonate, a binder to reduce odor, and a nonionic surfactant selected from the group consisting of ethoxylated alcohols, fatty acid esters, and alkylpolyglucoside families.

### Claim 7 (depends on 2)

The method of claim 2, wherein the reducing agent comprises a sulfite-based compound.

### Claim 8 (depends on 7)

The method of claim 7, wherein the reducing agent comprises one of potassium metabisulfite at a concentration from 0.15% to 0.45% weight per volume (w/v) and sodium metabisulfite at a concentration from 0.15% to 0.45% w/v.

### Claim 9 (depends on 2)

The method of claim 2, wherein the reducing agent is selected from the group consisting of: sodium metabisulfite, sodium sulfite, potassium sulfite, ammonium sulfite, sodium bisulfite, ammonium bisulfite, potassium metabisulfite, ammonium thioglycolate, tris (2-carboxyethyl) phosphine hydrochloride, 2-mercaptoethanol, and dithiothreitol.

### Claim 10 (depends on 4)

The method of claim 4, wherein the solvent comprises water at a temperature from about 0° C. to about 10° C.

### Claim 11 (depends on 2)

The method of claim 2, further comprising preparing the aqueous solution, wherein preparing comprises providing a concentrated solution having the reducing agent and diluting the concentrated solution with an effective amount of water.

### Claim 12 (depends on 3)

The method of claim 3, wherein physically stressing the material comprises stretching the shrunken material to a length to or beyond a desired size for a time period from about 10 seconds to about 60 seconds.

### Claim 13 (depends on 2)

The method of claim 2, wherein treating the shrunken material in the aqueous solution occurs for a time period from about 10 minutes to about 60 minutes.

### Claim 14 (depends on 1)

The method of claim 1, wherein the shrunken material comprises a garment having woolen fibers.

### Claim 15 (depends on 1)

The method of claim 1, wherein dissolving disulfide bonds in the shrunken material comprises dissolving disulfide bonds formed in keratinous protein molecules, the keratinous protein molecules having a curled orientation and a substantially rough texture, wherein elongating the shrunken material comprises reorienting protein molecules into a straightened orientation, and wherein promoting reformation of disulfide bonds comprises promoting reformation of disulfide bonds in keratinous protein molecules having the straightened orientation to maintain the straightened orientation and produce a substantially scaled texture.

### Claim 16

A kit for increasing the size of a shrunken garment comprising wool fibers, the kit comprising:
a concentrated solution comprising a reducing agent capable of cleaving disulfide bonds in the wool fibers; and
instructions for use.

### Claim 17 (depends on 16)

The kit of claim 16, wherein the instructions for use comprise instructions to:
place into a washing machine the shrunken garment;
introduce to the washing machine the concentrated solution;
operate the washing machine on a gentle or delicate cycle that may include a soak cycle;
remove the shrunken garment from the washing machine;
physically stretch the shrunken garment to a length to or beyond a desired size; and
allow the shrunken garment to dry.

### Claim 18 (depends on 16)

The kit of claim 16, wherein the instructions for use comprise instructions to:
place into a bin the shrunken garment;
introduce to the bin the concentrated solution;
introduce to the bin water to form an aqueous solution with the concentrated solution;
soak the shrunken garment in the aqueous solution;
rinse the shrunken garment;
physically stretch the shrunken garment to a length to or beyond a desired size; and
allow the shrunken garment to dry.

### Claim 19 (depends on 16)

The kit of claim 16, wherein the concentrated solution further comprises at least one of a basic compound such as sodium bicarbonate for odor control, a surfactant, and a binder.

### Claim 20 (depends on 16)

The kit of claim 16, wherein the reducing agent is a sulfite-based reducing agent.

### Claim 21 (depends on 16)

The kit of claim 16, wherein the reducing agent is selected from the group consisting of: sodium metabisulfite, sodium sulfite, potassium sulfite, ammonium sulfite, sodium bisulfite, ammonium bisulfite, potassium metabisulfite, ammonium thioglycolate, tris (2-carboxyethyl) phosphine hydrochloride, 2-mercaptoethanol, and dithiothreitol.

### Claim 22

A method for unshrinking a garment comprising wool fiber, the method comprising:
introducing the garment to an aqueous solution comprising a reducing agent;
rinsing the garment to remove residual reducing agent from the garment;
physically stretching the garment; and
allowing the material to dry without further physical stress.

### Claim 23 (depends on 22)

The method of claim 22, wherein rinsing the garment to remove residual reducing agent occurs prior to physically stretching the garment.

### Claim 24 (depends on 22)

The method of claim 22, wherein the reducing agent is a sulfite-based reducing agent.

### Claim 25 (depends on 22)

The method of claim 22, wherein the reducing agent is selected from the group consisting of: sodium metabisulfite, sodium sulfite, potassium sulfite, ammonium sulfite, sodium bisulfite, ammonium bisulfite, potassium metabisulfite, ammonium thioglycolate, tris (2-carboxyethyl) phosphine hydrochloride, 2-mercaptoethanol, and dithiothreitol.