# US 2019/0355988 A1 · Cathode material and lithium ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355988 A1
- Document ID: US20190355988A1
- Status: Published application
- Kind: A1
- Application number: 16/158,639
- Filed: 2018-10-12
- Published: 2019-11-21
- Earliest claimed: 2018-05-18
- Assignees: Ningde Amperex Technology Limited
- Applicants: Ningde Amperex Technology Limited
- Inventors: Ye LANG; Gang PENG; Leimin XU; Yousong CHENG
- Web page: https://patentgrep.com/patent/US20190355988A1

## CPC

- C01G 51/42: containing alkali metals, e.g. LiCoO2
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/366: {as layered products}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/32: spinel-type (AB2O4)
- C01P 2002/52: containing elements as dopants
- C01P 2004/03: obtained by SEM
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/12: Surface area
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application relates to a cathode material and a lithium ion battery. Particularly, the cathode material includes a matrix and a coating layer, wherein the matrix includes lithium cobalt oxide bulk-doped with metal element M, and the coating layer has a spinel phase structure doped with metal element Me. The spinel phase structure can form three-dimensional lithium ion channels, thereby increasing a diffusion path of lithium ions, and introducing more electrochemical reaction active sites. Therefore, when the lithium ion battery with the cathode material is discharged at a current of about 6 C at about −10° C., a capacity retention rate is up to about 99% or above as compared with that when the current is about 0.5 C. At the same time, the lithium ion battery also has high temperature stability, and has excellent cycle performance in high-temperature heavy-current charge-discharge environments.

## Claims

### Claim 1

A cathode material, comprising:
a matrix, wherein the matrix comprises lithium cobalt bulk-doped with metal element M; and
a coating layer, arranged on a surface of the matrix,
wherein M comprises at least one of Mg, Ti, Zr or Al,
wherein the coating layer has a spinel phase structure doped with metal element Me, and Me comprises at least one of Ni, Mn, Al, Mg, Ti, Zr, Y, Mo, W, Na, Cu, Cr, Zn or Fe, and
wherein the coating layer comprises Me, O, Li and Co elements.

### Claim 2 (depends on 1)

The cathode material according to claim 1, wherein an active specific surface area that the cathode material can perform a lithium ion deintercalation reaction is greater than or equal to about 3.6 cm2/g.

### Claim 3 (depends on 1)

The cathode material according to claim 1, wherein Me at least comprises two metal elements.

### Claim 4 (depends on 1)

The cathode material according to claim 1, wherein M and Me are not completely identical.

### Claim 5 (depends on 1)

The cathode material according to claim 1, wherein the mole percentage of each of Me relative to that of Co is about 0.1%-2%.

### Claim 6 (depends on 1)

The cathode material according to claim 1, wherein the mole percent of each of M relative to that of Co is about 0.1%-1%.

### Claim 7 (depends on 1)

The cathode material according to claim 1, wherein the cathode material has a median particle diameter D50 about 3-11 μm.

### Claim 8

A method for preparing a cathode material, comprising:
providing a precursor of lithium cobalt oxide;
mixing the precursor with a compound of lithium and a compound of metal element M, and sintering the mixture in an air atmosphere at about 900-1000° C. for about 6-12 hours to form lithium cobalt oxide bulk-doped with metal element M; and
mixing the lithium cobalt oxide with a compound of metal element Me, sintering the mixture in an air atmosphere at about 850-950° C. for about 6-12 hours, naturally cooling, and then annealing the mixture in an oxygen-containing atmosphere to obtain a lithium cobalt oxide cathode material surface-doped with metal element Me and having a spinel phase structure on the surface, wherein the annealing temperature is about 600-900° C., and the annealing time is about 1-8 hours,
wherein M comprises at least one of Mg, Ti, Zr or Al, and
wherein Me comprises at least one of Ni, Mn, Al, Mg, Ti, Zr, Y, Mo, W, Na, Cu, Cr, Zn or Fe.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the volume percentage of oxygen in the oxygen-containing atmosphere is less than about 10%.

### Claim 10 (depends on 8)

The method according to claim 8, wherein the annealing temperature is about 700-860° C.

### Claim 11 (depends on 8)

The method according to claim 8, wherein the annealing time is about 2-6 hours.

### Claim 12

A method for preparing a cathode material, comprising:
mixing a cobalt source, a lithium source, a precipitant and a salt of metal element M in an aqueous solution, and precipitating to form a precursor of lithium cobalt oxide bulk-doped with metal element M;
sintering the precursor in an air atmosphere at about 900-1000° C. for about 6-12 hours to form lithium cobalt oxide bulk-doped with metal element M; and
mixing the lithium cobalt oxide with a compound of metal element Me, sintering the mixture in an air atmosphere at about 850-950° C. for about 6-12 hours, naturally cooling the mixture, and then annealing the mixture in an oxygen-containing atmosphere to obtain a lithium cobalt oxide cathode material surface-doped with metal element Me and having a spinel phase structure on the surface, wherein the annealing temperature is about 600-900° C., and the annealing time is about 1-8 hours;
wherein M comprises at least one of Mg, Ti, Zr or Al, and
wherein Me comprises at least one of Ni, Mn, Al, Mg, Ti, Zr, Y, Mo, W, Na, Cu, Cr, Zn or Fe.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the volume percentage of oxygen in the oxygen-containing atmosphere is less than about 10%.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the annealing temperature is about 700-860° C.

### Claim 15 (depends on 12)

The method according to claim 12, wherein the annealing time is about 2-6 hours.

### Claim 16 (depends on 12)

The method according to claim 12, wherein the lithium source comprises one of lithium acetate, lithium nitrate or lithium.

### Claim 17 (depends on 12)

The method according to claim 12, wherein the cobalt source comprises one of cobalt oxalate, cobalt acetate, cobalt carbonate, cobalt sulfate or cobalt chloride.

### Claim 18 (depends on 12)

The method according to claim 12, wherein the precipitant comprises one of lithium hydroxide, sodium hydroxide or ammonia.