# US 2019/0355985 A1 · Method for preparing silicon-carbon-graphene composite, composite prepared according thereto, and secondary battery to which same is applied

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355985 A1
- Document ID: US20190355985A1
- Status: Published application
- Kind: A1
- Application number: 16/483,932
- Filed: 2017-05-23
- Published: 2019-11-21
- Earliest claimed: 2017-02-09
- Assignees: Korea Institute of Geoscience and Mineral Resources
- Applicants: Korea Institute of Geoscience and Mineral Resources
- Inventors: Hee-Dong JANG; Han-Kwon CHANG; Dae-Sup Kil; Ji-Hyuk Choi; Sun-Kyung Kim
- Web page: https://patentgrep.com/patent/US20190355985A1

## CPC

- H01M 4/366: {as layered products}
- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- C01B 32/182: Graphene
- C01B 33/021: Preparation (chemical coating from the vapour phase C23C16/00)
- C01B 33/037: Purification (by zone-melting C30B13/00)
- C04B 35/528: obtained from carbonaceous particles with or without other non-organic components
- C04B 35/6261: {Milling}
- C04B 35/62655: {Drying, e.g. freeze-drying, spray-drying, microwave or supercritical drying}
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- C01P 2006/40: Electric properties
- C04B 2235/422: Carbon
- C04B 2235/428: Silicon
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/606: Drying
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An embodiment of the present invention provides a method for preparing a silicon-carbon-graphene composite, comprising the steps of: (step 1) adding a carbon precursor solution to silicon and performing wet grinding so as to prepare a suspension: (step 2) forming a silicon-carbon composite by spray drying the suspension; and (step 3) spray drying and heat treating a solution comprising the silicon-carbon composite and graphene oxide.

## Claims

### Claim 1

A manufacturing method of a silicon-carbon-graphene composite, comprising,
adding a carbon precursor solution to silicon and performing wet pulverization to prepare a suspension in step 1;
forming a silicon-carbon composite by spray-drying the suspension in step 2; and
spray-drying and heat-treating a mixed solution of the silicon-carbon composite and a graphene oxide in step 3.

### Claim 2 (depends on 1)

The method of claim 1, wherein the silicon of said step 1 is obtained by, acid-leaching a waste silicon sludge and selectively separating and recovering silicon in step 0.

### Claim 3 (depends on 2)

The method of claim 2, wherein said step 0 further comprises,
drying after the acid-leaching, and after preforming ultrasonic treatment on a solution comprising the waste silicon sludge that was subject to drying, the silicon is selectively separated and recovered by centrifugal separation.

### Claim 4 (depends on 3)

The method of claim 3, wherein the ultrasonic treatment of said step 0 is performed for 1 hour to 10 hours,
and the centrifugal separation of said step 0 is performed at a rotation speed of 100 rpm to 1000 rpm for 1 minute to 60 minutes.

### Claim 5 (depends on 1)

The method of claim 1, wherein the carbon precursor of said step 1 comprises one or more selected from the group consisting of monosaccharides, disaccharides, polysaccharides, polyvinylpyrrolidone (PVP), polyethylene glycol (PEG), and polyvinyl alcohol (PVA).

### Claim 6 (depends on 1)

The method of claim 1, wherein a mixing ratio of the silicon and the carbon precursor is 1:0.1 to 1:2.

### Claim 7 (depends on 1)

The method of claim 1 wherein, the wet pulverization of said step 1 is performed such that an average particle size of the silicon is 0.1 μm to 1 μm.

### Claim 8 (depends on 1)

The method of claim 1 wherein, the wet pulverization of said step 1 is performed by one or more methods selected from the group consisting of a bead mill, a basket mill, an attrition mill, and a ball mill.

### Claim 9 (depends on 1)

The method of claim 1 wherein, the spraying of said step 2 is performed by ultrasonic spraying at an ultrasonic frequency of from 1.0 Mhz to 2.5 Mhz.

### Claim 10 (depends on 1)

The method of claim 1 wherein, the drying described in step 2 is performed by passing a sprayed material through a tubular heating furnace via a carrier gas.

### Claim 11 (depends on 1)

The method of claim 1 wherein, the solution of said step 3 has a graphene oxide concentration of 0.05 wt % to 0.2 wt %,
and the solution of said step 3 has a silicon-carbon composite concentration of 0.1 wt % to 3 wt %.

### Claim 12 (depends on 1)

The method of claim 1 wherein, the spray-drying of said step 3 is performed by,
spraying a mixed solution of the silicon-carbon composite and graphene oxide in a form of aerosol droplets through a two-fluid nozzle in step 3a;
drying and heat-treating the sprayed droplets by passing the sprayed droplets through a tubular heating furnace via a carrier gas in step 3b.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the heat-treatment temperature described in said step 3 is 500° C. to 1000° C.

### Claim 14

A manufacturing method of a silicon-carbon-graphene composite, comprising.
acid-leaching a waste silicon sludge, and selectively separating and recovering silicon by ultrasonic treatment and centrifugal separation in step 0;
adding a carbon precursor solution to the recovered silicon and performing wet pulverization to prepare a suspension in step 1;
forming a silicon-carbon composite by ultrasonically spray-drying the suspension in step 2;
spraying a mixed solution of the silicon-carbon composite and graphene oxide in a form of aerosol droplets through a two-fluid nozzle in step 3a; and
drying and heat-treating the sprayed droplets by passing the sprayed droplets through a tubular heating furnace via a carrier gas in step 3b.

### Claim 15

A silicon-carbon-graphene composite comprising, a silicon-carbon composite comprising a carbon layer formed around silicon particles; and
a graphene layer formed around an agglomerate comprising a plurality of the silicon-carbon composites,
wherein the silicon-carbon-graphene composite has an average particle size of 0.5 μm to 20 μm, and the graphene layer is formed by agglomeration of a plurality of crumpled graphene sheets.

### Claim 16 (depends on 15)

A secondary battery comprising,
an anode; a cathode comprising the silicon-carbon-graphene composite of claim 15;
a separator formed between the anode and the cathode; and an electrolyte.