# US 2019/0355982 A1 · Negative electrode of thin film battery and method for makingthesame and a thin film using the negative electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355982 A1
- Document ID: US20190355982A1
- Status: Published application
- Kind: A1
- Application number: 16/414,681
- Filed: 2019-05-16
- Published: 2019-11-21
- Earliest claimed: 2018-05-18
- Assignees: Securitag Assembly Group Co., Ltd.
- Applicants: Securitag Assembly Group Co., Ltd
- Inventors: Kuan-Jiuh Lin; Wen-Yin Ko; Man-Jyun Fang; Chia Ming Kuo; Wayyu Chen; Yu Ching Wang
- Web page: https://patentgrep.com/patent/US20190355982A1

## CPC

- H01G 11/30: characterised by their material
- H01M 4/366: {as layered products}
- H01G 11/46: Metal oxides
- H01G 11/50: specially adapted for lithium-ion capacitors, e.g. for lithium-doping or for intercalation
- H01M 4/0426: {Sputtering}
- H01M 4/0492: {Chemical attack of the support material}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0564: the electrolyte being constituted of organic materials only
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0065: Solid electrolytes
- Y02E 60/10: Energy storage using batteries
- Y02E 60/13: Energy storage using capacitors
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A negative electrode of a thin film battery and method for forming the same, wherein the negative electrode comprises a porous structural layer, a capacitor layer, and a lithium ion source layer. The porous structural layer is formed on a metal substrate, and a thickness of the porous structural layer is between 200 nm and 700 nm. The capacitor layer is formed on the porous structural layer, and a thickness is between 100 nm and 300 nm. The lithium ion source layer is formed on the capacitor layer. Since the porous structural layer is made of stable material, a problem of charging-discharging instability that is occurred due to damage of battery structure caused by the volume expansion of the capacitor layer during the charging-discharging process can be improved. In addition, the negative electrode can be combined with a positive electrode for forming a thin film battery.

## Claims

### Claim 1

A negative electrode of a thin film battery, comprising:
a metal substrate;
a porous structural layer, formed on the metal substrate, wherein the porous structural layer has a three-dimensional porous frame formed by titanium oxide or vanadium oxide;
a capacitor layer, formed on the porous structural layer, wherein a material for forming the capacitor layer is selected from a group consisting Ag, Al, Bi, C, Ge, Sb, Si, Sn and Zn, and the material is deposited on the three-dimensional porous frame for forming the capacitor layer; and;
a lithium ion source layer, formed on the capacitor layer, wherein a material for forming the lithium ion source layer is lithium source.

### Claim 2 (depends on 1)

The negative electrode of claim 1, wherein the porous structural layer comprises a plurality of nano scale void spaces, and a porosity of the porous structural layer is between 75%˜90%.

### Claim 3 (depends on 1)

The negative electrode of claim 1, wherein the porous structural layer includes a metal oxide formed by a chemical treatment on a metal layer formed on a surface of the metal substrate through a coating process.

### Claim 4 (depends on 1)

The negative electrode of claim 1, wherein a capacitor material of the capacitor layer is formed on the porous structural layer through a sputtering process.

### Claim 5 (depends on 1)

The negative electrode of claim 1, further comprising a solid-state organic electrolyte layer formed on the lithium ion source layer.

### Claim 6 (depends on 5)

The negative electrode of claim 5, further comprising an oxide layer formed on the solid-state organic electrolyte layer.

### Claim 7 (depends on 1)

The negative electrode of claim 1, wherein the lithium source is selected from a group consisting of LiClO4, LiCF3SO3, LiPF6, LiN(SO2CF3)2, Li2SO4, LiNO3, LiF, Li2CO3, and LiBF4.

### Claim 8

A method for forming a negative electrode of a thin film battery, comprising steps of:
providing a metal substrate;
forming a metal layer on the metal substrate, wherein the metal layer is titanium metal or vanadium metal;
transforming the metal layer into a porous structural layer having a three-dimensional porous frame formed by titanium oxide or vanadium oxide;
depositing a material selected from a group consisting Ag, Al, Bi, C, Ge, Sb, Si, Sn and Zn, on the three-dimensional porous frame to form a capacitor layer; and
forming a lithium ion source layer on the capacitor layer, wherein a material for forming the lithium ion source layer is lithium source.

### Claim 9 (depends on 8)

The method of claim 8, wherein the metal substrate is a metal roll for a roll-to-roll manufacturing process, and the steps of forming the structural layer, the porous structural layer, the capacitor layer, and the lithium ion source layer are completed through the roll-to-roll manufacturing process.

### Claim 10 (depends on 8)

The method of claim 8, wherein the porous structural layer comprises a plurality of nano scale void spaces, and a porosity of the porous structural layer is between 75%˜90%.

### Claim 11 (depends on 8)

The method of claim 8, wherein the step of providing the metal substrate further comprises a step of forming an adhesive layer for adhering the metal substrate to a carrier substrate.

### Claim 12 (depends on 11)

The method of claim 11, further comprising a step of removing the carrier substrate from the metal substrate.

### Claim 13 (depends on 8)

The method of claim 8, further comprising steps of:
forming a solid-state organic electrolyte layer on the lithium ion source layer; and
forming an oxide layer on the solid-state organic electrolyte layer.

### Claim 14 (depends on 8)

The method of claim 8, wherein the lithium source is selected from a group consisting LiClO4, LiCF3SO3, LiPF6, LiN(SO2CF3)2, Li2SO4, LiNO3, LiF, Li2CO3, and LiBF4.

### Claim 15

A thin film battery, comprising:
a positive electrode; and
a negative electrode, coupled to the positive electrode, the negative electrode comprising:
a first metal substrate;
a porous structural layer, formed on the first metal substrate, wherein the porous structural layer has a three-dimensional porous frame formed by titanium oxide or vanadium oxide;
a capacitor layer, formed on the porous structural layer, wherein a material for forming the capacitor layer is selected from a group consisting Ag, Al, Bi, C, Ge, Sb, Si, Sn and Zn, and the material is deposited on the three-dimensional porous frame for forming the capacitor layer; and
a lithium ion source layer, formed on the capacitor layer, wherein a material for forming the lithium ion source layer is lithium source.

### Claim 16 (depends on 15)

The thin film battery of claim 15, wherein the porous structural layer includes a metal oxide formed by a chemical treatment on a metal layer formed on a surface of the first metal substrate through a coating process.

### Claim 17 (depends on 15)

The thin film battery of claim 15, further comprising a solid-state organic electrolyte layer formed on the lithium ion source layer.

### Claim 18 (depends on 15)

The thin film battery of claim 15, wherein the lithium source is selected from a group consisting LiClO4, LiCF3SO3, LiPF6, LiN(SO2CF3)2, Li2SO4, LiNO3, LiF, Li2CO3, and LiBF4.

### Claim 19 (depends on 15)

The thin film battery of claim 15, wherein the positive electrode further comprises:
a solid-state organic electrolyte layer;
a lithium oxide layer, formed on the solid-state organic electrolyte layer; and
a second metal substrate, formed on the lithium oxide layer.