- Number: US 2019/0355980 A1
- Document ID: US20190355980A1
- Status: Published application
- Kind: A1
- Application number: 16/411,421
- Filed: 2019-05-14
- Published: 2019-11-21
- Earliest claimed: 2018-05-16
- Assignees: pH Matter, LLC
- Applicants: pH Matter, LLC
- Inventors: Christopher T. Holt; Mary C. Cramer; Paul H. Matter
- Web page: https://patentgrep.com/patent/US20190355980A1

## CPC

- H01M 4/366: {as layered products}
- H01M 4/483: {for non-aqueous cells (H01M4/485 takes precedence)}
- H01M 4/625: {Carbon or graphite}
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The instant invention includes a spherical porous secondary silicon-based particle and methods for producing the same. The spherical porous secondary silicon-based particle is comprised of agglomerated primary silicon-based nanoparticles. The secondary particle comprises a carbon coating that reduces the effective exposed surface area of the primary particles to the electrolyte, thus improving first cycle efficiency. The secondary particle further comprises porous regions that enable the silicon nanoparticles to expand during lithiation. Advantages include ease of castability with micron-sized spherical particles, ease of mixing spherical particles, ease of flow for spherical particles in various processing steps, and ease with obtaining higher loading, which translates to higher areal capacity and overall energy density of the cell. A readily scalable process for producing the particles using low-cost materials and low-cost processing methods is disclosed.

## Claims

### Claim 1

A spherical particle comprising:
primary SiO(2-x) nanoparticles, wherein x=0.1 to 2;
an internal void space; and
an external elemental carbon coating;
wherein the particle has a diameter of between and including 0.5 to 200 microns.

### Claim 2 (depends on 1)

The particle according to claim 1, wherein the internal void space further comprises 10% to 90% by volume of the particle.

### Claim 3 (depends on 1)

The particle according to claim 1, wherein the particle further comprises 2% to 90% carbon by mass.

### Claim 4 (depends on 1)

The particle according to claim 1, wherein the internal void space further comprises 30% to 70% by volume of the particle.

### Claim 5 (depends on 1)

The particle according to claim 1, wherein the spherical particle has a diameter of between and including 5 to 50 microns.

### Claim 6 (depends on 1)

The particle according to claim 1, wherein the primary SiO(2-x) nanoparticles have a diameter of between and including 10 to 1000 nanometers.

### Claim 7 (depends on 1)

The particle according to claim 1, wherein the primary SiO(2-x) nanoparticles have internal porosity.

### Claim 8 (depends on 1)

The particle according to claim 1, wherein the primary SiO(2-x) nanoparticles are a combination of both silicon metal and silicon oxide phases.

### Claim 9 (depends on 1)

The particle according to claim 1, wherein the particle further comprises 10% to 50% carbon by mass.

### Claim 10 (depends on 1)

The particle according to claim 1, wherein the elemental carbon coating is a coating selected from the group of coatings consisting of graphite, amorphous carbon, and graphene, and mixtures thereof.

### Claim 11 (depends on 1)

The particle according to claim 1, wherein the particle further comprises lithium metal or lithium salt.

### Claim 12 (depends on 1)

The particle according to claim 1, wherein the particle further comprises one or more additional metals that can alloy with lithium.

### Claim 13

A method for making a spherical particle of primary silicon nanoparticles, an internal void space, and an external carbon coating, comprising the steps of:
a. dispersing SiO(2-x) nano-particles, wherein X=0 to 2, in a solvent to form a liquid mixture;
b. spraying the liquid mixture to form spherical droplets;
c. drying the mixture to form spherical agglomerates of the nanoparticles; and
d. coating the agglomerates with carbon

### Claim 14 (depends on 13)

The method according to claim 13, wherein the method further comprises a step of adding a pore forming agent to the solvent and removing said pore forming agent prior to a final coating of the agglomerates with carbon.

### Claim 15 (depends on 13)

The method according to claim 13, wherein the method further comprises a step of adding a pore forming agent to the solvent, coating the agglomerates with an initial carbon coating, removing said pore forming agent, and forming a final coating of the agglomerates with carbon.

### Claim 16 (depends on 13)

The method according to claim 13, further comprising the step of chemically reducing the carbon-coated SiO(2-x) particles.

### Claim 17 (depends on 16)

The method according to claim 16, further comprising the step of chemically reducing the carbon-coated SiO(2-x) particles to SiO(2-y), where y is greater than x.