# US 2019/0355978 A1 · Method for preparing graphene/ternary material composite for use in lithium ion batteries and product thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355978 A1
- Document ID: US20190355978A1
- Status: Published application
- Kind: A1
- Application number: 16/474,209
- Filed: 2016-12-30
- Published: 2019-11-21
- Earliest claimed: 2016-12-30
- Assignees: Beijing Tunghsu Carbon Advanced Materials Technology Co., Ltd.; Tunghsu Group Co., Ltd.
- Applicants: Beijing Tunghsu Carbon Advanced Materials Technology Co., Ltd.; Tunghsu Group Co., Ltd.
- Inventors: Qing Li; Min Chen; Heran Li; Zhonghui Wang
- Web page: https://patentgrep.com/patent/US20190355978A1

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/364: {as mixtures}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a method for preparing a graphene/ternary material composite for use in lithium ion batteries, comprising the following preparation steps: (a) mixing a ternary material and a graphene oxide powder in an organic solvent to form a mixed dispersion; (b) adding a reducing agent to the mixed dispersion from step (a), and carrying out a reduction reaction at a reduction temperature of 80-160° C. while stirring, to obtain a reduction reaction mixture after a reduction time of 60-240 min; and (c) evaporating the solvent from the reduction reaction mixture from step (b) while stirring, and drying and then annealing the mixture at a low temperature in an inert atmosphere to obtain a graphene/ternary material composite having a three-dimensional network structure. Also provided is a graphene/ternary material composite prepared by using this method.

## Claims

### Claim 1

A method for preparing a graphene/ternary material composite for use in lithium ion batteries, comprising the steps of:
(a) mixing a ternary material with a graphene oxide powder in an organic solvent to form a mixed dispersion;
(b) adding a reducing agent to the mixed dispersion from step (a), and carrying out a reduction reaction at a reduction temperature of 80-160° C. while stirring, to obtain a reduction reaction mixture after a reduction time of 60-240 min; and
(c) evaporating the solvent from the reduction reaction mixture from step (b) while stirring, and drying and then annealing the mixture at a low temperature in an inert atmosphere to obtain a graphene/ternary material composite having a three-dimensional network structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the reducing agent is one or more selected from the group consisting of hydrazine reducing agents, weak acids, phenols, metal hydride reducing agents, strong bases, reducing sugars, alcohols, sodium dithionite, H2 and hydroiodic acid.

### Claim 3 (depends on 1)

The method of claim 1, wherein the reducing agent is one or more selected from the group consisting of hydrazine hydrate, dimethyl hydrazine, phenylhydrazine, p-methylsulfonyl hydrazide, ascorbic acid, pyrogallic acid, hydroquinone, tea polyphenol, sodium borohydride, lithium aluminum hydride, sodium hydroxide, potassium hydroxide, aqueous ammonia, glucose, fructose, sucrose, alcohols, sodium dithionite, H2 and hydroiodic acid.

### Claim 4 (depends on 1)

The method of claim 1, wherein step (a) further comprises the steps of:
(a1) adding the graphene oxide powder to the organic solvent to obtain a uniformly dispersed graphene oxide dispersion; and
(a2) adding the ternary material to the graphene oxide dispersion to form a mixed dispersion.

### Claim 5 (depends on 4)

The method of claim 4, wherein in step (a1), the uniformly dispersed graphene oxide dispersion is obtained by ultrasonic dispersion.

### Claim 6 (depends on 4)

The method of claim 4, wherein the graphene oxide dispersion obtained in step (a1) has a concentration of 0.1-5 g/L.

### Claim 7 (depends on 4)

The method of claim 4, wherein in step (a2), the ternary material is added to the graphene oxide dispersion in 2-6 portions.

### Claim 8 (depends on 4)

The method of claim 4, wherein in step (a2), the ternary material is sufficiently mixed with the graphene oxide by physical mixing to form a mixed dispersion, wherein the physical mixing is one or more selected from the group consisting of stirring, sonication, ball milling, and cell discruption.

### Claim 9 (depends on 1)

The method of claim 1, wherein the mass ratio of the ternary material to the graphene oxide is 1:20-1:200.

### Claim 10 (depends on 1)

The method of claim 1, wherein the mass ratio of the graphene oxide to the reducing agent is 1:1-1:100.

### Claim 11 (depends on 1)

The method of claim 1, wherein the organic solvent in step (a) is one or more selected from the group consisting of ethanol, N-methylpyrrolidone (NMP), N,N-dimethylformamide (DMF), methanol, propanol, isopropanol, n-butanol, ethylene glycol, glycerol, acetone, and n-propanol.

### Claim 12 (depends on 1)

The method of claim 1, wherein the reduction reaction mixture is purified before evaporating the solvent from the reduction reaction mixture from step (b) while stirring.

### Claim 13 (depends on 1)

The method of claim 1, wherein the annealing in step (c) is conducted at a temperature of 150-350° C.

### Claim 14 (depends on 1)

The method of claim 1, wherein the annealing in step (c) is conducted for 1-5 h.

### Claim 15 (depends on 1)

The method of claim 1, wherein the annealing at a low temperature in step (c) is carried out in a tube furnace.

### Claim 16 (depends on 1)

The method of claim 1, further comprising a pre-treatment prior to step (a), in which the pre-treatment comprises drying the ternary material and the graphene oxide powder at 120-200° C. for 1-3 h.

### Claim 17 (depends on 1)

The method of claim 1, wherein the ternary material is one or more selected from the group consisting of nickel-cobalt-manganese ternary materials, nickel-cobalt-aluminum ternary materials, and lithium-rich ternary materials.

### Claim 18 (depends on 1)

A graphene/ternary material composite for use in lithium ion batteries prepared by the method according to claim 1.