# US 2019/0355966 A1 · Methods of forming carbon-silicon composite material on a current collector

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355966 A1
- Document ID: US20190355966A1
- Status: Published application
- Kind: A1
- Application number: 16/430,306
- Filed: 2019-06-03
- Published: 2019-11-21
- Earliest claimed: 2017-03-28
- Assignees: Enevate Corporation
- Applicants: Enevate Corporation
- Inventors: Rahul R. Kamath; Benjamin Yong Park; Frederic C. Bonhomme
- Web page: https://patentgrep.com/patent/US20190355966A1

## CPC

- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/366: {as layered products}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/587: for inserting or intercalating light metals
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Methods of forming electrodes are described. In some embodiments, the method can include providing a current collector. The method can also include providing a first carbon precursor on the current collector and providing a mixture on the first carbon precursor. The mixture can include a second carbon precursor and silicon particles. The method can further include pyrolysing the second carbon precursor to convert the second carbon precursor into one or more types of carbon phases to form a composite material. The one or more types of carbon phases can be a substantially continuous phase with the silicon particles distributed throughout the composite material. The method can also include pyrolysing the first carbon precursor to adhere the composite material to the current collector.

## Claims

### Claim 1

A method of forming an electrode, the method comprising:
providing a current collector;
providing a first carbon precursor on the current collector;
providing a mixture on the first carbon precursor, the mixture comprising a second carbon precursor and silicon particles;
pyrolysing the second carbon precursor to convert the second carbon precursor into one or more types of carbon phases to form a composite material comprising the one or more types of carbon phases as a substantially continuous phase with the silicon particles distributed throughout the composite material; and
pyrolysing the first carbon precursor to adhere the composite material to the current collector.

### Claim 2 (depends on 1)

The method of claim 1, wherein pyrolysing the first carbon precursor causes the pyrolyzed carbon to diffuse into the current collector.

### Claim 3 (depends on 1)

The method of claim 1, wherein pyrolysing the first and second carbon precursors occur during the same heat treatment.

### Claim 4 (depends on 1)

The method of claim 1, wherein pyrolysing the first and second carbon precursors occur at a temperature in a range of about 350° C. to about 1350° C.

### Claim 5 (depends on 4)

The method of claim 4, wherein pyrolysing the first and second carbon precursors occur at a temperature in a range of about 350° C. to about 1275° C.

### Claim 6 (depends on 4)

The method of claim 4, wherein pyrolysing the first and second carbon precursors occur at a temperature in a range of about 700° C. to about 1350° C.

### Claim 7 (depends on 5)

The method of claim 5, wherein pyrolysing the first and second carbon precursors occur at a temperature in a range of about 700° C. to about 1275° C.

### Claim 8 (depends on 6)

The method of claim 6, wherein pyrolysing the first and second carbon precursors occur at a temperature in a range of about 900° C. to about 1350° C.

### Claim 9 (depends on 7)

The method of claim 7, wherein pyrolysing the first and second carbon precursors occur at a temperature in a range of about 900° C. to about 1275° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first carbon precursor has a 10% to 70% char yield.

### Claim 11 (depends on 1)

The method of claim 1, wherein the first carbon precursor comprises polyamic acid, phenol formaldehyde resin, polypyrrole, polyacrylonitrile, polyamideimide, polyimide, a polyimide precursor, or a combination thereof.

### Claim 12 (depends on 11)

The method of claim 11, wherein the polyimide precursor comprises pyromellitic dianhydride oxidianiline (PMDA-ODA), biphenyl tetracarboxylic acid dianhydride oxidianiline (BPDA-ODA), biphenyl tetracarboxylic acid dianhydride-p-phenylene diamine (BPDA-PDA), pyromellitic dianhydride-p-phenylene diamine (PMDA-PDA), or a combination thereof.

### Claim 13 (depends on 1)

The method of claim 1, wherein providing the first carbon precursor comprises coating the first carbon precursor on the current collector.

### Claim 14 (depends on 1)

The method of claim 1, further comprising drying the first carbon precursor prior to providing the mixture on the first carbon precursor.

### Claim 15 (depends on 1)

The method of claim 1, wherein the first carbon precursor on the current collector has a thickness in the range of about 1 μm to about 1 mm.

### Claim 16 (depends on 1)

The method of claim 1, wherein the first carbon precursor and the second carbon precursor are chemically the same.

### Claim 17 (depends on 1)

The method of claim 1, wherein the first carbon precursor is chemically different than the second carbon precursor.

### Claim 18 (depends on 1)

The method of claim 1, wherein providing the mixture comprises providing a slurry comprising the second carbon precursor and silicon particles.

### Claim 19 (depends on 1)

The method of claim 1, further comprising drying the mixture prior to pyrolysing the second carbon precursor.

### Claim 20 (depends on 1)

The method of claim 1, wherein the current collector comprises a transition element and/or an alloy comprising a transition element.

### Claim 21 (depends on 20)

The method of claim 20, wherein the transition element or the alloy comprises chromium, molybdenum, iron, vanadium, tungsten, tantalum, niobium, or a combination thereof.

### Claim 22 (depends on 21)

The method of claim 21, wherein the alloy comprises nickel and chromium.

### Claim 23 (depends on 21)

The method of claim 21, wherein the alloy comprises stainless steel.

### Claim 24 (depends on 22)

The method of claim 22, wherein the alloy comprises nichrome.

### Claim 25 (depends on 20)

The method of claim 20, wherein the current collector comprises a layer comprising the transition element and/or the alloy comprising the transition element on at least one side of the current collector, and the first carbon precursor is provided on the at least one side of the current collector.

### Claim 26 (depends on 1)

The method of claim 1, wherein the current collector comprises nickel and/or copper.

### Claim 27 (depends on 1)

The method of claim 1, wherein providing the mixture comprises providing the silicon particles such that the composite material comprises the silicon particles at about 60% to about 99% by weight.

### Claim 28 (depends on 1)

The method of claim 1, wherein the electrode is an anode.

### Claim 29 (depends on 1)

A method of forming an electrochemical device, the method comprising:
providing a first electrode, wherein providing the first electrode comprises providing the electrode formed by the method of claim 1;
providing a second electrode; and
providing electrolyte.

### Claim 30 (depends on 29)

The method of claim 29, wherein the first electrode is an anode and the second electrode is a cathode.

### Claim 31 (depends on 29)

The method of claim 29, wherein the electrochemical device is a battery.