# US 2019/0355934 A1 · Film for preventing humidity from percolation and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355934 A1
- Document ID: US20190355934A1
- Status: Published application
- Kind: A1
- Application number: 16/476,253
- Filed: 2018-01-02
- Published: 2019-11-21
- Earliest claimed: 2017-01-05
- Assignees: Jusung Engineering Co., Ltd.
- Applicants: Jusung Engineering Co., Ltd.
- Inventors: Kyeong Min KIM; Bong Sik KIM; Sang Du LEE; Won Tae CHO
- Web page: https://patentgrep.com/patent/US20190355934A1

## CPC

- C23C 16/345: {Silicon nitride}
- C23C 16/401: {containing silicon}
- C23C 16/402: {Silicon dioxide}
- C23C 16/56: After-treatment
- H10K 59/873: {Encapsulations}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present inventive concept provides a moisture prevention film including: a first moisture prevention film; a second moisture prevention film formed on the first moisture prevention film; and a third moisture prevention film formed on the second moisture prevention film, wherein a concentration of oxygen (O) of the second moisture prevention film is higher than a concentration of oxygen of each of the first moisture prevention film and the third moisture prevention film, a method of manufacturing the moisture prevention film, and an organic light emitting device including the moisture prevention film.

## Claims

### Claim 1

A moisture prevention film comprising:
a first moisture prevention film;
a second moisture prevention film on the first moisture prevention film; and
a third moisture prevention film on the second moisture prevention film,
wherein a concentration of oxygen (O) of the second moisture prevention film is higher than a concentration of oxygen of each of the first moisture prevention film and the third moisture prevention film.

### Claim 2 (depends on 1)

The moisture prevention film of claim 1, wherein the second moisture prevention film is lower in concentration of nitrogen (N) than the first moisture prevention film and the third moisture prevention film.

### Claim 3 (depends on 1)

The moisture prevention film of claim 1, wherein a wet etch rate of the second moisture prevention film is higher than a wet etch rate of each of the first moisture prevention film and the third moisture prevention film.

### Claim 4 (depends on 3)

The moisture prevention film of claim 3, wherein the wet etch rate of the second moisture prevention film is 10 to 100 times higher than the wet etch rate of each of the first moisture prevention film and the third moisture prevention film.

### Claim 5 (depends on 1)

The moisture prevention film of claim 1, wherein a thickness of the second moisture prevention film is less than a thickness of each of the first moisture prevention film and the third moisture prevention film.

### Claim 6 (depends on 1)

The moisture prevention film of claim 1, wherein a crystallized layer is not formed between the first moisture prevention film and the second moisture prevention film.

### Claim 7 (depends on 1)

The moisture prevention film of claim 1, wherein a crystallized layer is not formed between the second moisture prevention film and the third moisture prevention film.

### Claim 8

An organic light emitting device comprising:
a substrate;
a light emitting part on the substrate; and
a moisture prevention film on the light emitting part,
wherein in the moisture prevention film, a concentration of oxygen (O) included in the moisture prevention film from a lower portion to an upper portion of the moisture prevention film increases gradually and then decreases, and a concentration of nitrogen (N) decreases gradually and then increases.

### Claim 9 (depends on 8)

The organic light emitting device of claim 8, wherein the moisture prevention film is formed of a single layer, and the concentration of the oxygen and the concentration of the nitrogen are gradually changed in the moisture prevention film.

### Claim 10

A method of manufacturing a moisture prevention film, the method comprising:
a first moisture prevention film forming process of forming a first moisture prevention film through a chemical vapor deposition process;
a second moisture prevention film forming process of forming a second moisture prevention film on the first moisture prevention film through an atomic layer deposition process; and
a third moisture prevention film forming process of forming a third moisture prevention film on the second moisture prevention film through a chemical vapor deposition process.

### Claim 11 (depends on 10)

The method of claim 10, wherein the first moisture prevention film to the third moisture prevention film are formed in one chamber.

### Claim 12 (depends on 10)

The method of claim 10, wherein the second moisture prevention film is formed through a reaction of a source gas including silicon (Si) with a second reactant gas including nitrous oxide (N2O).

### Claim 13 (depends on 10)

The method of claim 10, wherein the first moisture prevention film and the third moisture prevention film are each formed through a reaction of a source gas including silicon (Si) with a first reactant gas including ammonia (NH3) and nitrogen (N2).

### Claim 14 (depends on 10)

The method of claim 10, wherein a deposition rate of the second moisture prevention film is lower than a deposition rate of each of the first moisture prevention film and the third moisture prevention film.

### Claim 15 (depends on 14)

The method of claim 14, wherein the deposition rate of the second moisture prevention film is 4 to 10 times lower than the deposition rate of each of the first moisture prevention film and the third moisture prevention film.

### Claim 16 (depends on 10)

The method of claim 10, further comprising a seasoning process before only the first moisture prevention film forming process.

### Claim 17

A method of manufacturing a moisture prevention film, the method comprises;
a first process of forming a film through a reaction of a source gas including silicon with a first reactant gas including ammonia (NH3) and nitrogen (N2);
a second process of forming a film through a reaction of a source gas including silicon (Si) with a second reactant gas including nitrous oxide (N2O); and
a third process of forming a film through a reaction of the source gas including silicon with the first reactant gas including ammonia (NH3) and nitrogen (N2).