# US 2019/0355933 A1 · Display panel and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355933 A1
- Document ID: US20190355933A1
- Status: Published application
- Kind: A1
- Application number: 16/092,006
- Filed: 2018-08-09
- Published: 2019-11-21
- Earliest claimed: 2018-05-21
- Assignees: Wuhan China Star Optoelectronics Semiconductor Display Technology Co., Ltd.
- Applicants: Wuhan China Star Optoelectronics Semiconductor Display Technology Co., Ltd.
- Inventors: Tianfu GUO
- Web page: https://patentgrep.com/patent/US20190355933A1

## CPC

- H10K 71/00: Manufacture or treatment specially adapted for the organic devices covered by this subclass
- H10K 59/1213: {the pixel elements being TFTs}
- H10K 59/8731: {multilayered coatings having a repetitive structure, e.g. having multiple organic-inorganic bilayers}
- H10K 59/1201: {Manufacture or treatment}
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

The present disclosure provides a display panel and a method for manufacturing the same. The method includes forming a base layer, a thin film transistor (TFT) device layer, an organic light-emitting diode (OLED) device layer, and a first inorganic material in turn on a substrate; modifying a surface of the first inorganic material to increase flowability of an organic buffer layer that is to be formed on a surface of the first inorganic layer; and forming the organic buffer layer and a second inorganic layer in turn on the first inorganic layer. According to the present disclosure, flowability of the organic material formed on the inorganic material layer is increased.

## Claims

### Claim 1

A method for manufacturing a display panel, comprising:
a step A of forming a base layer on a substrate;
a step B of forming a thin film transistor (TFT) device layer on the base layer;
a step C of forming an organic light-emitting diode (OLED) device layer on the TFT device layer;
a step D of forming a first inorganic material on the OLED device layer;
a step E of modifying a surface of the first inorganic material to form a first inorganic layer, wherein the first inorganic layer is configured to prevent water outside of the display panel from contacting the OLED device layer, and to increase flowability of an organic buffer layer that is to be formed on a surface of the first inorganic layer;
a step F of forming the organic buffer layer on the first inorganic layer; and
a step G of forming a second inorganic layer on the organic buffer layer;
wherein the step E includes:
a step e1 of injecting a trimethyl aluminum gas towards the surface of the first inorganic material to have hydroxyl functional groups on the surface of the first inorganic material react with the trimethyl aluminum gas, so as to form aluminum containing hydrocarbon functional groups on the surface of the first inorganic material; and
a step e2 of injecting a hydroxyl functional group containing alkyl alcohol gas towards the surface of the first inorganic material to transfer hydroxyl functional groups of the aluminum containing hydrocarbon functional groups on the surface of the first inorganic material into alkoxy chains;
wherein the organic buffer layer covers a plurality of foreign matter particulate on the first inorganic layer, and is configured to planarize the surface of the first inorganic layer having a device disposed underneath, and to release stress generated from the first inorganic layer; and
wherein a contact angle of the organic buffer layer with the modified surface of the first inorganic layer is less than 5 degrees.

### Claim 2 (depends on 1)

The method for manufacturing the display panel according to claim 1, wherein the first inorganic layer includes a material selected from a group consisting of silicon nitride, silicon oxynitride, silicon oxycarbide, and any combinations thereof; and
wherein the organic buffer layer includes resin.

### Claim 3

A method for manufacturing a display panel, comprising:
a step A of forming a base layer on a substrate;
a step B of forming a thin film transistor (TFT) device layer on the base layer;
a step C of forming an organic light-emitting diode (OLED) device layer on the TFT device layer;
a step D of forming a first inorganic material on the OLED device layer;
a step E of modifying a surface of the first inorganic material to form a first inorganic layer, wherein the first inorganic layer is configured to prevent water outside of the display panel from contacting the OLED device layer, and to increase flowability of an organic buffer layer that is to be formed on a surface of the first inorganic layer;
a step F of forming the organic buffer layer on the first inorganic layer; and
a step G of forming a second inorganic layer on the organic buffer layer.

### Claim 4 (depends on 3)

The method for manufacturing the display panel according to claim 3, wherein the step E includes:
a step e1 of injecting a trimethyl aluminum gas towards the surface of the first inorganic material to have hydroxyl functional groups on the surface of the first inorganic material react with the trimethyl aluminum gas, so as to form aluminum containing hydrocarbon functional groups on the surface of the first inorganic material; and
a step e2 of injecting a hydroxyl functional group containing alkyl alcohol gas towards the surface of the first inorganic material where aluminum containing hydrocarbon functional groups are formed, so as to transfer hydroxyl functional groups of the aluminum containing hydrocarbon functional groups on the surface of the first inorganic material into alkoxy chains.

### Claim 5 (depends on 4)

The method for manufacturing the display panel according to claim 4, wherein the hydroxyl functional group containing alkyl alcohol gas is selected from a group consisting of an ethanol gas, a methanol gas, and any combinations thereof.

### Claim 6 (depends on 4)

The method for manufacturing the display panel according to claim 4, wherein the step e1 includes:
injecting the trimethyl aluminum gas towards the surface of the first inorganic material at a first flow rate for a first duration, such that a force corresponding to a flow of the trimethyl aluminum gas is applied to the surface of the first inorganic material to have hydroxyl functional groups on the surface of the first inorganic material react with the trimethyl aluminum gas, and aluminum containing hydrocarbon functional groups are formed on the surface of the first inorganic material.

### Claim 7 (depends on 4)

The method for manufacturing the display panel according to claim 4, wherein the step e2 includes:
injecting the hydroxyl functional group containing alkyl alcohol gas towards the surface of the first inorganic material where aluminum containing hydrocarbon functional groups are formed at a second flow rate for a second duration, such that a force corresponding to a flow of the hydroxyl functional group containing alkyl alcohol gas is applied to the surface of the first inorganic material to have hydroxyl functional groups of the aluminum containing hydrocarbon functional groups react with the hydroxyl functional group containing alkyl alcohol gas, and hydroxyl functional groups of the aluminum containing hydrocarbon functional groups on the surface of the first inorganic material are transferred into alkoxy chains.

### Claim 8 (depends on 3)

The method for manufacturing the display panel according to claim 3, wherein the first inorganic layer includes a material selected from a group consisting of silicon nitride, silicon oxynitride, silicon oxycarbide, and any combinations thereof; and
wherein the organic buffer layer includes resin.

### Claim 9 (depends on 3)

The method for manufacturing the display panel according to claim 3, wherein the organic buffer layer covers a plurality of foreign matter particulate on the first inorganic layer, and is configured to planarize the surface of the first inorganic layer having a device disposed underneath, and to release stress generated from the first inorganic layer.

### Claim 10 (depends on 3)

The method for manufacturing the display panel according to claim 3, wherein a contact angle of the organic buffer layer with the modified surface of the first inorganic layer is less than 5 degrees.

### Claim 11

A display panel, comprising:
a substrate;
a base layer disposed on the substrate;
a thin film transistor (TFT) device layer disposed on the base layer;
an organic light-emitting diode (OLED) device layer disposed on the TFT device layer;
a first inorganic layer disposed on the OLED device layer, wherein the first inorganic layer is formed by forming a first inorganic material on the OLED device layer and modifying a surface of the first inorganic material, and wherein the first inorganic layer is configured to isolate the OLED device layer from water outside of the display panel, and to increase flowability of an organic buffer layer that is to be disposed on a surface of the first inorganic layer;
the organic buffer layer disposed on the first inorganic layer; and
a second inorganic layer disposed on the organic buffer layer.

### Claim 12 (depends on 11)

The display panel according to claim 11, wherein the first inorganic layer is formed by:
injecting a trimethyl aluminum gas towards the surface of the first inorganic material to have hydroxyl functional groups on the surface of the first inorganic material react with the trimethyl aluminum gas, so as to form aluminum containing hydrocarbon functional groups on the surface of the first inorganic material; and
injecting a hydroxyl functional group containing alkyl alcohol gas towards the surface of the first inorganic material where aluminum containing hydrocarbon functional groups are formed, so as to transfer hydroxyl functional groups of the aluminum containing hydrocarbon functional groups on the surface of the first inorganic material into alkoxy chains.

### Claim 13 (depends on 12)

The display panel according to claim 12, wherein the hydroxyl functional group containing alkyl alcohol gas is selected from a group consisting of an ethanol gas, a methanol gas, and any combinations thereof.

### Claim 14 (depends on 12)

The display panel according to claim 12, wherein the aluminum containing hydrocarbon functional groups is formed on the surface of the first inorganic material by injecting the trimethyl aluminum gas towards the surface of the first inorganic material at a first flow rate for a first duration, such that a force corresponding to a flow of the trimethyl aluminum gas is applied to the surface of the first inorganic material to have hydroxyl functional groups on the surface of the first inorganic material react with the trimethyl aluminum gas.

### Claim 15 (depends on 12)

The display panel according to claim 12, wherein the alkoxy chains is formed by injecting the hydroxyl functional group containing alkyl alcohol gas towards the surface of the first inorganic material where aluminum containing hydrocarbon functional groups are formed at a second flow rate for a second duration, such that a force corresponding to a flow of the hydroxyl functional group containing alkyl alcohol gas is applied to the surface of the first inorganic material to have hydroxyl functional groups of the aluminum containing hydrocarbon functional groups react with the hydroxyl functional group containing alkyl alcohol gas.

### Claim 16 (depends on 11)

The display panel according to claim 11, wherein the second inorganic layer includes a first bending portion at a side edge of the second inorganic layer, and the first bending portion encapsulates a side of a combined structure of the first inorganic layer and the organic buffer layer; and
the first inorganic layer includes a second bending portion at a side edge of the first inorganic layer, and the second bending portion encapsulates a side of the OLED device layer.

### Claim 17 (depends on 16)

The display panel according to claim 16, wherein the organic buffer layer includes a third bending portion at a side edge of the organic buffer layer, and the third bending portion encapsulates the second bending portion of the first inorganic layer.

### Claim 18 (depends on 11)

The display panel according to claim 11, wherein the organic buffer layer covers a plurality of foreign matter particulate on the first inorganic layer, and is configured to planarize the surface of the first inorganic layer having a device disposed underneath, and to release stress generated from the first inorganic layer.

### Claim 19 (depends on 11)

The display panel according to claim 11, wherein the first inorganic layer includes a material selected from a group consisting of silicon nitride, silicon oxynitride, silicon oxycarbide, and any combinations thereof; and
wherein the organic buffer layer includes resin.

### Claim 20 (depends on 11)

The display panel according to claim 11, wherein a contact angle of the organic buffer layer with the modified surface of the first inorganic layer is less than 5 degrees.