# US 2019/0355900 A1 · Cryogenic oxidation of metal layer of magnetic-tunnel-junction (mtj) device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355900 A1
- Document ID: US20190355900A1
- Status: Published application
- Kind: A1
- Application number: 16/403,320
- Filed: 2019-05-03
- Published: 2019-11-21
- Earliest claimed: 2018-05-18
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., LTD.
- Inventors: WHAN KYUN KIM; EUN SUN NOH; JOON MYOUNG LEE; WOO CHANG LIM; JUN HO JEONG
- Web page: https://patentgrep.com/patent/US20190355900A1

## CPC

- H10B 61/22: {of the field-effect transistor [FET] type}
- H10N 50/01: Manufacture or treatment
- G11C 11/161: {details concerning the memory cell structure, e.g. the layers of the ferromagnetic memory cell}
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10D 86/421: {having a particular composition, shape or crystalline structure of the active layer}
- H10D 86/60: wherein the TFTs are in active matrices
- H10N 50/10: Magnetoresistive devices
- H10N 50/80: Constructional details
- H10N 50/85: Materials of the active region
- H10B: ELECTRONIC MEMORY DEVICES
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method is for manufacturing a magnetic-tunnel-junction (MTJ) device. The method includes forming a free magnetic layer over a substrate, forming a metal layer over the free magnetic layer, and oxidizing the metal layer by exposing the metal layer to an oxidation gas at a temperature of 250° K or less.

## Claims

### Claim 1

A method of manufacturing a magnetic-tunnel-junction (MTJ) device, the method comprising:
forming a free magnetic layer over a substrate;
forming a metal layer over the free magnetic layer; and
oxidizing the metal layer by exposing the metal layer to an oxidation gas at a temperature of 250° K or less.

### Claim 2 (depends on 1)

The method of claim 1, wherein the oxidation gas is a first oxidation gas and the temperature is a first temperature, and the method comprises:
further exposing the metal layer to a second oxidation gas at a second temperature that is higher than the first temperature.

### Claim 3 (depends on 2)

The method of claim 2, wherein at least one of the first and second oxidation gases is supplied from a shower head located at a distance between 10 and 30 nm, both inclusive, over a surface of the metal layer.

### Claim 4 (depends on 2)

The method of claim 2, wherein both of the first and second oxidation gases are supplied from a shower head located at a distance between 10 and 30 nm, both inclusive, over a surface of the metal layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the temperature is equal to or less than 230° K.

### Claim 6 (depends on 1)

The method of claim 1, wherein the temperature is equal to or less than 200° K.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second temperature is equal to or greater than 270° K.

### Claim 7 (depends on 2)

The method of claim 2, wherein the metal layer is exposed to the first oxidation gas at the first temperature for 50 to 100 seconds, both inclusive, and the metal layer is exposed to the second oxidation gas at the second temperature for 70 to 120 seconds, both inclusive.

### Claim 9 (depends on 2)

The method of claim 2, wherein the first oxidation gas and the second oxidation gas a same oxidation gas.

### Claim 10 (depends on 9)

The method of claim 9, wherein the metal layer is continuously exposed to the same oxidation gas as a temperature of the substrate transitions from the first temperature to the second temperature.

### Claim 11 (depends on 9)

The method of claim 9, wherein exposing the metal layer to the first oxidation gas at the first temperature is carried out in a same chamber as exposing the metal layer to the second oxidation gas at the second temperature.

### Claim 12 (depends on 1)

The method of claim 1, further comprising:
placing a wafer containing the MTJ device on an electrostatic chuck, the electromagnetic chuck in thermal contact with a cooling plate located below the electrostatic chuck; and
cooling the electrostatic chuck using the cooling plate so as to cool the wafer to the temperature.

### Claim 13 (depends on 2)

The method of claim 2, further comprising:
placing a wafer containing the MTJ device on an electrostatic chuck, the electromagnetic chuck in thermal contact with a cooling plate located below the electrostatic chuck;
cooling the electrostatic chuck using the cooling plate so as to cool the wafer to the first temperature; and
raising a temperature of the wafer to the second temperature.

### Claim 14 (depends on 13)

The method of claim 13, wherein raising the temperature of the wafer to the second temperature comprises lifting the wafer off a support surface of the electrostatic chuck.

### Claim 15 (depends on 13)

The method of claim 13, wherein raising the temperature of the wafer to the second temperature comprises using a lamp to heat the wafer.

### Claim 16 (depends on 1)

The method of claim 1, further comprising:
forming a lower electrode over the substrate;
forming a fixed magnetic layer over the lower electrode;
forming a tunnel barrier layer over the fixed magnetic layer,
wherein the free magnetic layer is formed over the tunnel barrier layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the fixed magnetic layer is formed from a seed layer deposited on the lower electrode.

### Claim 18 (depends on 16)

The method of claim 16, wherein the fixed magnetic layer is formed as a multilayer structure comprising plural fixed magnetic sublayers.

### Claim 19 (depends on 16)

The method of claim 16, further comprising forming an upper electrode over the metal layer after oxidation of the metal layer.

### Claim 20 (depends on 1)

The method of claim 1, wherein the metal layer is formed to include at least one of tantalum, zirconium, titanium, vanadium, yttrium, scandium, molybdenum, magnesium, and cobalt.

### Claim at position 21

21-30. (canceled)