# US 2019/0355856 A1 · Tunable earth abundant, non-toxic photovoltaic devices for low light and variable light level power applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355856 A1
- Document ID: US20190355856A1
- Status: Published application
- Kind: A1
- Application number: 15/979,802
- Filed: 2018-05-15
- Published: 2019-11-21
- Earliest claimed: 2018-05-15
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Priscilla D. Antunez; Douglas M. Bishop; Richard A. Haight; Yu Luo
- Web page: https://patentgrep.com/patent/US20190355856A1

## CPC

- H10F 71/1395: {for thin-film devices}
- H10F 77/128: {comprising only Group I-II-IV-VI kesterite materials, e.g. Cu2ZnSnSe4 or Cu2ZnSnS4}
- H02S 40/38: Energy storage means, e.g. batteries, structurally associated with PV modules
- H10F 10/16: Photovoltaic cells having only PN heterojunction potential barriers
- H10F 19/35: Structures for the connecting of adjacent photovoltaic cells, e.g. interconnections or insulating spacers
- H10F 19/902: {for series or parallel connection of photovoltaic cells}
- H10F 71/00: Manufacture or treatment of devices covered by this subclass (patterning processes to connect thin photovoltaic cells in integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/33; manufacture or treatment of encapsulations or containers for integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/80; manufacture or treatment of integrated devices, or assemblies of multiple devices, comprising at least one element in which radiation controls the flow of current H10F39/00)
- H10F 71/128: {Annealing}
- H10F 71/138: {Manufacture of transparent electrodes, e.g. transparent conductive oxides [TCO] or indium tin oxide [ITO] electrodes}
- H10F 77/244: {made of transparent conductive layers, e.g. transparent conductive oxide [TCO] layers}
- Y02E 10/50: Photovoltaic [PV] energy
- Y02E 70/30: Systems combining energy storage with energy generation of non-fossil origin
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H02S: GENERATION OF ELECTRIC POWER BY CONVERSION OF INFRARED RADIATION, VISIBLE LIGHT OR ULTRAVIOLET LIGHT, e.g. USING PHOTOVOLTAIC [PV] MODULES (obtaining electrical energy from radioactive sources G21H1/12; light sensitive inorganic semiconductor devices H10F; light sensitive organic semiconductor devices H10K30/00; thermoelectric devices H10N10/00; pyroelectric devices H10N15/00)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of fabricating a photovoltaic device includes performing fabrication operations to form the photovoltaic device. The fabrication operations include replacing a portion of selenium with sulfur in a copper zinc tin sulfur selenium alloy (CZTSSe) material arranged on a substrate to form a sulfur enriched CZTSSe material to alter a band gap of the CZTSSe material. The fabrication operations include removing surface secondary phases or degraded portions of the sulfur enriched CZTSSe material to form a single phase sulfur enriched CZTSSe material. The fabrication operations further include replacing the substrate in contact with the single phase sulfur enriched CZTSSe material with a different contact material to form an exfoliated sulfur enriched CZTSSe device.

## Claims

### Claim 1

A method of fabricating a photovoltaic device, the method comprising:
performing fabrication operations to form the photovoltaic device, wherein the fabrication operations include:
replacing a portion of selenium with sulfur in a copper zinc tin sulfur selenium alloy (CZTSSe) material arranged on a substrate to form a sulfur enriched CZTSSe material to alter a band gap of the CZTSSe material;
removing surface secondary phases or degraded portions of the sulfur enriched CZTSSe material to form a single phase sulfur enriched CZTSSe material; and
replacing the substrate in contact with the single phase sulfur enriched CZTSSe material with a different contact material to form an exfoliated sulfur enriched CZTSSe device.

### Claim 2 (depends on 1)

The method of claim 1 further comprising coupling a plurality of the exfoliated sulfur enriched CZTSSe devices in series and coupling the series with a battery to form a photovoltaic device.

### Claim 3 (depends on 1)

The method of claim 1 further comprising, prior to replacing the substrate, depositing a buffer layer and a top electrode on the single phase sulfur enriched CZTSSe material.

### Claim 4 (depends on 3)

The method of claim 3, wherein the buffer layer comprises an n-type material, and the top electrode comprises a transparent conductive material.

### Claim 5 (depends on 1)

The method of claim 1, wherein the different contact material comprises Au and MoO3.

### Claim 6 (depends on 1)

The method of claim 1, wherein replacing a portion of selenium with sulfur comprises annealing the CZTSSe material with elemental sulfur.

### Claim 7 (depends on 1)

The method of claim 1, wherein replacing the substrate comprises applying a mechanical impulse to remove the substrate and then depositing the different contact material.

### Claim 8

A method of fabricating a photovoltaic device, the method comprising:
performing fabrication operations to form the photovoltaic device, wherein the fabrication operations include:
replacing a portion of selenium with sulfur in a copper zinc tin sulfur selenium alloy (CZTSSe) material arranged on a substrate to form a sulfur enriched CZTSSe material to alter a band gap of the CZTSSe material;
annealing the sulfur enriched CZTSSe material in air;
removing surface secondary phases or degraded portions of the sulfur enriched CZTSSe material to form a single phase sulfur enriched CZTSSe material; and
exposing a surface of the single phase sulfur enriched CZTSSe material in contact with the substrate and depositing a contact material on the surface to form an exfoliated sulfur enriched CZTSSe device.

### Claim 9 (depends on 8)

The method of claim 8 further comprising coupling a plurality of the exfoliated sulfur enriched CZTSSe devices in series and coupling the series with a battery to form a photovoltaic device.

### Claim 10 (depends on 8)

The method of claim 8 further comprising, prior exposing the surface of the single phase sulfur enriched CZTSSe material, depositing a buffer layer and a top electrode on the single phase sulfur enriched CZTSSe material.

### Claim 11 (depends on 10)

The method of claim 10, wherein the buffer layer comprises an n-type material, and the top electrode comprises a transparent conductive material.

### Claim 12 (depends on 8)

The method of claim 8, wherein the contact material comprises Au and MoO3.

### Claim 13 (depends on 8)

The method of claim 8, wherein replacing a portion of selenium with sulfur comprises annealing the CZTSSe material with elemental sulfur.

### Claim 14 (depends on 8)

The method of claim 8, wherein replacing the substrate comprises applying a mechanical impulse to remove the substrate and then depositing the different contact material.

### Claim 15

A photovoltaic device comprising:
a battery; and
a plurality of light absorbing stacks coupled to one another in series and arranged on the battery, each light absorbing stack of the plurality comprising:
a sulfur enriched copper zinc tin sulfur selenium alloy (CZTSSe) material arranged on a first contact;
a buffer layer arranged on the sulfur enriched CZTSSe material; and
a transparent electrode arranged on the buffer layer.

### Claim 16 (depends on 15)

The photovoltaic device of claim 15, wherein the sulfur enriched CZTSSe material has a concentration ratio of [S]/[S]+[Se] of about 0.01 to 1.0.

### Claim 17 (depends on 15)

The photovoltaic device of claim 15, wherein the first contact comprises Au, MoO3, or a combination thereof.

### Claim 18 (depends on 15)

The photovoltaic device of claim 15, wherein the sulfur enriched CZTSSe material comprises a substantially single phase material at an interface with the buffer layer.

### Claim 19 (depends on 15)

The photovoltaic device of claim 15 further comprising an insulating layer arranged between the battery and the plurality of light absorbing stacks.

### Claim 20 (depends on 15)

The photovoltaic device of claim 15, the open circuit voltage of the photovoltaic device is in a range from about 300 to about 1000 mV.