# US 2019/0355722 A1 · Very narrow aspect ratio trapping trench structure with smooth trench sidewalls

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355722 A1
- Document ID: US20190355722A1
- Status: Published application
- Kind: A1
- Application number: 16/526,320
- Filed: 2019-07-30
- Published: 2019-11-21
- Earliest claimed: 2017-05-01
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Karthik Balakrishnan; Kangguo Cheng; Pouya Hashemi; Alexander Reznicek
- Web page: https://patentgrep.com/patent/US20190355722A1

## CPC

- H10D 84/834: {comprising FinFETs}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10D 62/117: {Shapes of semiconductor bodies}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/276: {Lateral overgrowth}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3416: {Nitrides}
- H10P 14/3466: {Crystal orientation}
- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- H10D 84/0151: {Manufacturing their isolation regions}
- H10D 84/8316: {the IGFETs characterised by having gate sidewall spacers specially adapted for integration}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

After forming a plurality of semiconductor fins that are separated from one another by trenches on a substrate, the semiconductor fins are fully or partially oxidized to provide semiconductor oxide portions. The volume expansion caused by the oxidation of the semiconductor fins reduces widths of the trenches, thereby providing narrowed trenches for formation of epitaxial semiconductor fins using aspect ratio trapping techniques.

## Claims

### Claim 1

A method of forming a semiconductor structure comprising:
forming a plurality of semiconductor fins on a substrate, wherein the plurality of semiconductor fins are separated from one another by first trenches having a first width;
oxidizing at least a portion of each of the plurality of semiconductor fins to provide a semiconductor oxide portion, wherein the semiconductor oxide portions are separated from one another by second trenches having a second width less than the first width; and
forming an epitaxial semiconductor layer within each second trench.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming the epitaxial semiconductor layer comprises epitaxially growing a semiconductor material from a surface of the substrate exposed by each second trench.

### Claim 3 (depends on 1)

The method of claim 1, further comprising, prior to the oxidizing, forming a bottom spacer layer on the substrate to laterally surround bottom portions of the semiconductor fins.

### Claim 4 (depends on 3)

The method of claim 3, further comprising etching the bottom spacer layer to provide an opening beneath each second trench and provide a bottom spacer laterally surrounding each opening, wherein sidewalls of each bottom spacer are offset from sidewalls of each second trench, and each epitaxial semiconductor layer is formed by epitaxially growing the semiconductor material from a surface of the substrate exposed by each opening.

### Claim 5 (depends on 4)

The method of claim 4, wherein the etching comprises a directional etching process.

### Claim 6 (depends on 4)

The method of claim 4, wherein the etching process comprises an anisotropic etch followed by an isotropic etch.

### Claim 7 (depends on 6)

The method of claim 6, wherein the anisotropic etch and the isotropic etch collectively provide an aspect ratio trench (ART) having a narrow trench portion and a wider bottom portion.

### Claim 8 (depends on 1)

The method of claim 1, wherein an entirety of each semiconductor fin is oxidized, wherein the second trenches are separated by one another solely by the semiconductor oxide portions.

### Claim 9 (depends on 1)

The method of claim 1, wherein an outer portion of each semiconductor fin is oxidized to provide the semiconductor oxide portion around a remaining portion of each semiconductor fin.

### Claim 10 (depends on 9)

The method of claim 9, further comprising recessing the remaining portion of each semiconductor fin to provide a semiconductor fin base portion.

### Claim 11 (depends on 10)

The method of claim 10, further comprising forming a dielectric fill portion atop each semiconductor fin base portion.

### Claim 12 (depends on 1)

The method of claim 1, wherein each epitaxial semiconductor layer has a wider bottom portion and a narrower upper portion.

### Claim 13 (depends on 12)

The method of claim 12, wherein defects are trapped alone sidewalls of the bottom portion of each epitaxial semiconductor material.

### Claim 14 (depends on 1)

The method of claim 1, wherein each epitaxial semiconductor layer has a topmost surface that has a chevron shape.

### Claim 15 (depends on 14)

The method of claim 14, further comprising removing the chevron shape from each epitaxial semiconductor layer to provide an uppermost surface that is entirely planar.

### Claim 16 (depends on 1)

The method of claim 1, wherein the oxidizing is performed at a temperature from 600° C. to 1200° C.

### Claim 17

A method of forming a semiconductor structure, the method comprising
forming a plurality of semiconductor fins on a substrate, wherein the plurality of semiconductor fins are separated from one another by first trenches having a first width;
forming a bottom spacer layer around a bottom portion of each semiconductor fin;
fully oxidizing each of the plurality of semiconductor fins to provide a semiconductor oxide portion, wherein the semiconductor oxide portions are separated from one another by second trenches having a second width less than the first width;
etching the bottom spacer layer to form an opening underneath the second trench provided by the oxidizing;
forming a faceted opening within the substrate and beneath each opening;
forming an epitaxial semiconductor layer within each second trench and each opening; and
recessing each semiconductor oxide portion to exposed an upper portion of each epitaxial semiconductor layer.

### Claim 18 (depends on 17)

The method of claim 17, wherein each epitaxial semiconductor layer has a topmost surface that has a chevron shape, and the chevron shape is removed from each epitaxial semiconductor layer prior to recessing each semiconductor oxide portion.

### Claim 19

A method of forming a semiconductor structure, the method comprising
forming a plurality of semiconductor fins on a substrate, wherein the plurality of semiconductor fins are separated from one another by first trenches having a first width;
forming a bottom spacer layer around a bottom portion of each semiconductor fin;
partially oxidizing each of the plurality of semiconductor fins to provide a semiconductor oxide portion, wherein the semiconductor oxide portions are separated from one another by second trenches having a second width less than the first width;
etching the bottom spacer layer to form an opening underneath the second trench provided by the oxidizing;
forming a faceted opening within the substrate and beneath each opening;
forming an epitaxial semiconductor layer within each second trench and each opening; and
recessing each semiconductor oxide portion to exposed an upper portion of each epitaxial semiconductor layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein each epitaxial semiconductor layer has a topmost surface that has a chevron shape, and the chevron shape is removed from each epitaxial semiconductor layer prior to recessing each semiconductor oxide portion.