# US 2019/0355617 A1 · Atomic Layer Deposition For Low-K Trench Protection During Etch

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355617 A1
- Document ID: US20190355617A1
- Status: Published application
- Kind: A1
- Application number: 16/415,687
- Filed: 2019-05-17
- Published: 2019-11-21
- Earliest claimed: 2018-05-21
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: David O'Meara; Angelique Raley; Xinghua Sun; Yen-Tien Lu
- Web page: https://patentgrep.com/patent/US20190355617A1

## CPC

- H10P 50/73: {using masks for insulating materials}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10P 50/283: {by chemical means}
- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

An atomic layer deposition (ALD) technique is used to deposit one or more layers on hard mask layers and the sidewalls of low-K dielectric trench as part of the trench etch process. The ALD layer(s) can prevent the hard mask from being eroded during various hard mask open processes. Further, the ALD layer(s) may be utilized to prevent the low-K dielectric sidewall from being laterally etched during the low-K dielectric trench etch. Hence, better control of the trench profile and better critical dimension control may be provided.

## Claims

### Claim 1

A method of etching a substrate to form a trench, the method comprising:
providing a first patterned feature on the substrate;
providing a low-k dielectric layer on the substrate, the low-k dielectric layer underlying the first patterned feature;
etching a first portion of the low-k dielectric layer according a trench pattern formed by the first patterned feature;
after etching the first portion of the low-k dielectric layer, forming a first sidewall layer on exposed sidewall surfaces of the low-k dielectric layer, the forming the first sidewall layer being performed by an first atomic layer deposition process; and
after forming the first sidewall layer on exposed sidewall surfaces of the low-k dielectric layer, performing a second etching of the low-k dielectric layer according to the trench pattern, the first sidewall layer protecting sidewalls of the low-k dielectric layer during the second etching of the low-k dielectric layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein after the second etching of the low-k dielectric layer, forming a second sidewall layer on exposed sidewall surfaces of the low-k dielectric layer, the forming the second sidewall layer being performed by a second atomic layer deposition process.

### Claim 3 (depends on 2)

The method of claim 2, wherein after forming the second sidewall layer on exposed sidewall surfaces of the low-k dielectric layer, performing a third etching of the low-k dielectric layer according to the trench pattern, the second sidewall layer protecting sidewalls of the low-k dielectric layer during the third etching of the low-k dielectric layer.

### Claim 4 (depends on 3)

The method of claim 3, wherein after the third etching of the low-k dielectric layer, forming a third sidewall layer on exposed sidewall surfaces of the low-k dielectric layer, the forming the third sidewall layer being performed by a third atomic layer deposition process.

### Claim 5 (depends on 4)

The method of claim 4, wherein after forming the third sidewall layer on exposed sidewall surfaces of the low-k dielectric layer, performing a fourth etching of the low-k dielectric layer according to the trench pattern, the third sidewall layer protecting sidewalls of the low-k dielectric layer during the fourth etching of the low-k dielectric layer.

### Claim 6 (depends on 5)

The method of claim 5, further comprising forming a patterned feature sidewall layer on at least sidewalls of the patterned feature, the patterned feature sidewall layer being performed by an initial atomic layer deposition process, the patterned feature sidewall layer being performed before the etching a first portion of the low-k dielectric layer.

### Claim 7 (depends on 5)

The method of claim 5, wherein the first sidewall layer, the second sidewall layer and the third sidewall layer are formed of a same material.

### Claim 8 (depends on 7)

The method of claim 7, wherein the same material is silicon oxide or silicon nitride.

### Claim 9 (depends on 3)

The method of claim 3, further comprising forming a patterned feature sidewall layer on at least sidewalls of the patterned feature, the patterned feature sidewall layer being performed by an initial atomic layer deposition process, the patterned feature sidewall layer being performed before the etching a first portion of the low-k dielectric layer.

### Claim 10

A method of etching a substrate to form a trench, the method comprising:
providing a first patterned feature on the substrate;
providing a low-k dielectric layer on the substrate, the low-k dielectric layer underlying the first patterned feature;
providing an initial sidewall layer on at least sidewalls of the first patterned feature;
after providing the initial sidewall layer on at least sidewalls of the first patterned feature, etching a first portion of the low-k dielectric layer according a trench pattern formed by the first patterned feature; and
after etching the first portion of the low-k dielectric layer, performing a cyclic process of forming sidewall layers on exposed sidewall surfaces of the low-k dielectric layer by an atomic layer deposition process and then further etching the low-k dielectric layer until the trench is formed in the low-k dielectric layer, the forming sidewall layers on exposed sidewall surfaces protecting sidewalls of the low-k dielectric layer during the further etching of the low-k dielectric layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the initial sidewall layer on at least sidewalls of the first patterned feature and the sidewall layers on exposed sidewall surfaces of the low-k dielectric layer are formed of a same material.

### Claim 12 (depends on 10)

The method of claim 10, wherein the initial sidewall layer on at least sidewalls of the first patterned feature and the sidewall layers on exposed sidewall surfaces of the low-k dielectric layer are formed of silicon oxide or silicon nitride.

### Claim 13 (depends on 10)

The method of claim 10 wherein at least two cycles of the cyclic process occur.

### Claim 14 (depends on 13)

The method of claim 13, wherein the sidewalls formed during the cyclic process are all formed of a same material.

### Claim 15 (depends on 14)

The method of claim 14, wherein the same material is silicon oxide or silicon nitride.

### Claim 16

A method of etching a substrate to form a trench, the method comprising:
providing a hard mask layer on the substrate;
providing a first patterned feature on the substrate, the first patterned feature being located above the hard mask layer;
providing a low-k dielectric layer on the substrate, the low-k dielectric layer being located under the hard mask layer;
providing a first sidewall layer on at least sidewalls of the first patterned feature via a first atomic layer deposition process;
after providing the first sidewall layer on at least the sidewalls of the first patterned feature, etching the hard mask layer according to a trench pattern formed by the first patterned feature, the etching the hard mask layer replicating the trench pattern in the hard mask layer and exposing sidewalls of the hard mask layer;
providing a second sidewall layer on at least the sidewalls of the hard mask layer via a second atomic layer deposition process;
after providing the second sidewall layer on at least sidewalls of the hard mask layer, etching a portion of the low-k dielectric layer according to the trench pattern replicated in the hard mask layer; and
after etching the portion of the low-k dielectric layer, performing a cyclic process of forming sidewall layers on exposed sidewall surfaces of the low-k dielectric layer by additional atomic layer deposition processes and then further etching the low-k dielectric layer until the trench is formed in the low-k dielectric layer, the forming sidewall layers on exposed sidewall surfaces of the low-k dielectric layer protecting sidewalls of the low-k dielectric layer during the further etching of the low-k dielectric layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the trench aligns with a metallization layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein the sidewall layers on exposed sidewall surfaces of the low-k dielectric layer are all formed of a first material.

### Claim 19 (depends on 18)

The method of claim 18, wherein the first material is SiO2 or SiN.

### Claim 20 (depends on 19)

The method of claim 19, wherein the first sidewall layer and the second sidewall layer are both formed of the first material.

### Claim 21 (depends on 16)

The method of claim 16, wherein at least one of the first sidewall layer, the second sidewall layer, or the sidewall layers on exposed sidewall surfaces of the low-k dielectric layer are formed as a composite sidewall layer utilizing a first ALD method and a second ALD method, the first ALD method forming a lower composite sidewall layer and the second ALD method forming an upper composite sidewall layer over the lower composite sidewall layer, the first ALD method performed at a lower energy than the second ALD method.