# US 2019/0355579 A1 · Method to improve film stability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355579 A1
- Document ID: US20190355579A1
- Status: Published application
- Kind: A1
- Application number: 16/035,983
- Filed: 2018-07-16
- Published: 2019-11-21
- Earliest claimed: 2018-05-17
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Maximillian CLEMONS; Michel Ranjit FREI; Mahendra PAKALA; Mehul B. NAIK; Srinivas D. NEMANI; Ellie Y. YIEH
- Web page: https://patentgrep.com/patent/US20190355579A1

## CPC

- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6939: {characterised by the metal}
- H10N 70/023: {by chemical vapor deposition, e.g. MOCVD, ALD}
- H10N 70/041: {Modification of switching materials after formation, e.g. doping (shaping H10N70/061)}
- H10N 70/20: Multistable switching devices, e.g. memristors
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/6903: {containing silicon}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

Embodiments of the present disclosure generally relate to a film treatment process. In one embodiment, a transition metal oxide layer including a dopant is deposited on a substrate. After the doped transition metal oxide layer is deposited, a high pressure annealing process is performed on the doped transition metal oxide layer to densify the doped transition metal oxide without outgassing of the dopant. The high pressure annealing process is performed in an ambient environment including the dopant and at a pressure greater than 1 bar.

## Claims

### Claim 1

A method, comprising:
depositing a doped transition metal oxide layer on a substrate at a first temperature, the doped transition metal oxide layer comprising a dopant; and
annealing the doped transition metal oxide layer in a processing chamber at a chamber pressure greater than about 1 bar and in an ambient environment comprising the dopant.

### Claim 2 (depends on 1)

The method of claim 1, wherein the doped transition metal oxide layer is a carbon-doped nickel (II) oxide layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the doped transition metal oxide layer is annealed at a temperature ranging from about 200 degrees Celsius to about 500 degrees Celsius.

### Claim 4 (depends on 1)

The method of claim 1, wherein the chamber pressure ranges from about 2 bars to about 50 bars.

### Claim 5 (depends on 4)

The method of claim 4, wherein the chamber pressure ranges from about 10 bars to about 45 bars.

### Claim 6 (depends on 1)

The method of claim 1, wherein the annealing is performed at a second temperature greater than the first temperature.

### Claim 7 (depends on 6)

The method of claim 6, wherein the first temperature is about 350 degrees Celsius.

### Claim 8

A method, comprising:
depositing a doped transition metal oxide layer on a first electrode, the doped transition metal oxide layer comprising a dopant;
annealing the doped transition metal oxide layer in a processing chamber at a chamber pressure greater than about 1 bar and in an ambient environment comprising the dopant; and
depositing a metal layer over the doped transition metal oxide layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the dopant is carbon.

### Claim 10 (depends on 9)

The method of claim 9, wherein the ambient environment comprises CO2 gas.

### Claim 11 (depends on 10)

The method of claim 10, wherein the doped transition metal oxide layer comprises carbon-doped nickel (II) oxide layer.

### Claim 12 (depends on 8)

The method of claim 8, further comprising depositing a second electrode on the doped transition metal oxide layer, wherein the first electrode and the second electrode each comprise a metal that is different from the metal layer, and wherein the metal layer is deposited on the second electrode.

### Claim 13 (depends on 12)

The method of claim 12, wherein the metal layer comprises aluminum and the metal is iridium or platinum.

### Claim 14 (depends on 8)

The method of claim 8, wherein the chamber pressure ranges from about 2 bars to about 50 bars.

### Claim 15 (depends on 14)

The method of claim 14, wherein the chamber pressure ranges from about 10 bars to about 45 bars.

### Claim 16 (depends on 1)

The method of claim 1, wherein the annealing is performed at a temperature ranging from about 200 degrees Celsius to about 500 degrees Celsius.

### Claim 17

A method, comprising:
depositing a carbon-doped nickel (II) oxide layer on a substrate at a first temperature;
annealing the carbon-doped nickel (II) oxide layer in a processing chamber at a chamber pressure greater than about 1 bar and in a carbon-containing ambient environment; and
depositing a metal layer over the carbon-doped nickel (II) oxide layer at a second temperature greater than the first temperature.

### Claim 18 (depends on 17)

The method of claim 17, wherein the chamber pressure ranges from about 2 bars to about 50 bars.

### Claim 19 (depends on 17)

The method of claim 17, wherein the first temperature is about 350 degrees Celsius and the second temperature is about 400 degrees Celsius.

### Claim 20 (depends on 17)

The method of claim 17, wherein the annealing is performed at a temperature ranging from about 200 degrees Celsius to about 500 degrees Celsius.