# US 2019/0355538 A1 · Method for the fabrication of electron field emission devices including carbon nanotube electron field emission devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0355538 A1
- Document ID: US20190355538A1
- Status: Published application
- Kind: A1
- Application number: 16/527,533
- Filed: 2019-07-31
- Published: 2019-11-21
- Earliest claimed: 2011-05-23
- Assignees: Corporation for National Research Initiatives
- Applicants: Corporation for National Research Initiatives
- Inventors: Mehmet OZGUR; Paul SUNAL; Lance OH; Michael HUFF; Michael PEDERSEN
- Web page: https://patentgrep.com/patent/US20190355538A1

## CPC

- H01J 1/304: Field-emissive cathodes
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- B82Y 40/00: Manufacture or treatment of nanostructures
- H01J 9/025: {of field emission cathodes}
- H01J 2201/30469: Carbon nanotubes (CNTs)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

The present invention is directed to a method for the fabrication of electron field emitter devices, including carbon nanotube (CNT) field emission devices. The method of the present invention involves depositing one or more electrically conductive thin-film layers onto an electrically conductive substrate and performing lithography and etching on these thin film layers to pattern them into the desired shapes. The top-most layer may be of a material type that acts as a catalyst for the growth of single- or multiple-walled carbon nanotubes (CNTs). Subsequently, the substrate is etched to form a high-aspect ratio post or pillar structure onto which the previously patterned thin film layers are positioned. Carbon nanotubes may be grown on the catalyst material layer. The present invention also described methods by which the individual field emission devices may be singulated into individual die from a substrate.

## Claims

### Claim 1

A method of fabricating an electron field emission device using micro- and nano-fabrication techniques, the method comprising the steps of:
selecting a suitable first material substrate that is electrically conductive,
depositing onto this first material substrate a thin-film layer of second material layer that is electrically conductive;
patterning and etching said second material layer into a second predefined shape and dimensions; and
performing an etch into the first material substrate to a predefined depth to form a pillar or post shape structure to a predefined height.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first material substrate is composed of a semiconductor or metal material type.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first material substrate is silicon.

### Claim 4 (depends on 1)

The method of claim 1, wherein the second material layer is Titanium Nitride (TiN).

### Claim 5 (depends on 1)

The method of claim 1, wherein the second material layer is etched to predefined shapes and dimensions using ion milling, reactive ion etching, or wet etching technology.

### Claim 6 (depends on 5)

The method of claim 5, wherein the redeposited material of the second material layer after ion milling is removed using oblique angle ion milling for a short period of time.

### Claim 7 (depends on 1)

The method of claim 1, wherein the alignment marks are made to accurately register the layers of the field emitter device fabrication.

### Claim 8 (depends on 7)

The method of claim 7, for the alignment of subsequent layers, are patterned and etched in the surface of the first material substrate prior to deposition of the second material layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the fourth material layer is deposited onto the first material substrate prior to deposition of the second material layer and said fourth material layer is patterned and etched to define alignment marks for the alignment of subsequent layers, which are then patterned and etched in the surface of the first material substrate prior to deposition of the second material layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein the fourth material layer is composed of thin film material layer types including: dielectrics; metals; and polymers.

### Claim 11 (depends on 1)

The method of claim 1, wherein thickness of the second material layer is approximately 50 nanometers.

### Claim 12 (depends on 1)

The method of claim 1, wherein thickness of the second material layer is less than 10 nanometers.

### Claim 13 (depends on 1)

The method of claim 1, wherein thickness of the second material layer is between 10 and 100 nanometers.

### Claim 14 (depends on 1)

The method of claim 1, wherein thickness of the second material layer is more than 100 nanometers.

### Claim 15 (depends on 1)

The method of claim 1, wherein diameter of the predefined second material layer is between 300 and 500 nanometers.

### Claim 16 (depends on 1)

The method of claim 1, wherein diameter of the predefined second material layer is less than 300 nanometers.

### Claim 17 (depends on 1)

The method of claim 1, wherein diameter of the predefined second material layer is more than 500 nanometers.

### Claim 18 (depends on 1)

The method of claim 1, wherein the predefined pattern employs a single pillar or post for each field emitted device.

### Claim 19 (depends on 1)

The method of claim 1, wherein the predefined pattern employs an array of pillars or posts for each field emitted device.

### Claim 20 (depends on 1)

The method of claim 1, wherein the etch to form the pillar or post is performed resulting in a predefined height of the said pillar or post of 10 microns.

### Claim 21 (depends on 1)

The method of claim 1, wherein the etch to form the pillar or post is performed resulting in a predefined height of the said pillar or post of between 10 microns and 30 microns.

### Claim 22 (depends on 1)

The method of claim 1, wherein the etch to form the pillar or post is performed resulting in a predefined height of the said pillar or post of more than 30 microns.

### Claim 23 (depends on 1)

The method of claim 1, wherein the etch used to form the pillar or post is Deep Reactive Ion Etching (DRIE).

### Claim 24 (depends on 23)

The method of claim 23, wherein the etch used to form the pillar or post using Deep Reactive Ion Etching (DRIE) with the following recipe: 70 sccm O2, 7 sccm C4F8, 75 sccm SF6, RF power of 900 W, and platen power of 20 W.

### Claim 25 (depends on 1)

The method of claim 1, wherein a hard mask composed of Al2O3 is used for the pillar etch.

### Claim 26 (depends on 4)

The method of claim 4, wherein the second material layer is deposited using Chemical-Vapor Deposition (CVD) or Physical-Vapor Deposition (PVD) processes, reactive PVD processes, or Atomic Layer Deposition (ALD).

### Claim 27 (depends on 26)

The method of claim 26, wherein the second material layer is deposited using reactive sputtering, sputtering, evaporation, or reactive evaporation.

### Claim 28 (depends on 3)

The method of claim 3, wherein the said first material substrate composed of silicon is highly doped to make it electrically conductive.

### Claim 29 (depends on 28)

The method of claim 28, wherein doping level of the silicon greater than 1×1019 dopants/cm3.

### Claim 30 (depends on 27)

The method of claim 27, wherein the second material layer is deposited using the recipe composed of: 3 milli-Torr pressure of Ar/N2 at 50 standard cubic centimeters per minute operating at a sputtering power of 2000 Watts and a 350 kHz frequency with a 1.1 microsecond pulse power duration.

### Claim 31 (depends on 4)

The method of claim 4, wherein the percentage of Titanium to Nitrogen in the deposited TiN film layer be approximately 50% to 50%.

### Claim 32 (depends on 4)

The method of claim 4, wherein the second material layer composed of Titanium-Nitride has a smooth surface.

### Claim 33 (depends on 27)

The method of claim 27, wherein the second material layer composed of Titanium Nitride is annealed after the second material layer deposition.

### Claim 34 (depends on 33)

The method of claim 33, wherein the second material layer composed of Titanium Nitride is annealed immediately after the second material layer deposition.

### Claim 35 (depends on 33)

The method of claim 33, wherein the second material layer composed of Titanium Nitride is in-situ annealed after the second material layer deposition.

### Claim 36 (depends on 33)

The method of claim 33, wherein the second material layer composed of Titanium Nitride is annealed using rapid thermal anneal (RTA).

### Claim 37 (depends on 36)

The method of claim 36, wherein the second material layer composed of Titanium Nitride is annealed using rapid thermal anneal (RTA) with a background non-reactive gas comprising Nitrogen or Argon and at a temperature of approximately 800 C for 30 seconds.

### Claim 38 (depends on 5)

The method of claim 5, wherein the second material layer is etched to predefined shapes composed of circles.

### Claim 39 (depends on 1)

The method of claim 1, wherein the substrate is separated into individual die by depositing a layer of photoresist or polymer on the surface of the first material substrate after the pillar etch has been complete and before the carbon nanotube growth has been performed, subsequently dicing the substrate into a plurality of individual dies, and then removing said polymer using a wet chemical immersion.

### Claim 40 (depends on 39)

The method of claim 39, wherein the layer of photoresist or polymer deposited on the surface of the first material substrate has a thickness sufficient to encase the pillars or posts on the substrate.

### Claim 41 (depends on 1)

The method of claim 1, wherein the substrate is separated into individual die by etching cleaving trenches into the backside of the first material substrate before performing the pillar or post etch, performing the reminder of the field emitter device fabrication up to point before the carbon nanotube growth, and then cleaving the substrates into a plurality of individual dies.

### Claim 42 (depends on 1)

The method of claim 1, wherein the substrate is separated into individual dies by etching cavities into a second substrate of a depth greater than the height of the pillars or posts fabricated on the surface of the first material substrate, placing a double-sided thermal tape onto the second substrate that has been etched with said predetermined cavities, bonding the second and first material substrates together to enclose the pillars or posts in a sealed cavity, dicing the substrate into a plurality of individual dies and then removing the cavity die from the device die thereby exposing the pillar or post device structures.

### Claim 43 (depends on 42)

The method of claim 42 wherein the thermal tape is patterned prior to placing onto the cavity substrate.

### Claim 44 (depends on 43)

The method of claim 43, wherein alignment marks are formed into the backside of the cavity or device substrate prior to them being bonded to one another so as to facilitate locating the exact locations of the dicing lines prior to performing the dicing of the substrate.

### Claim 45 (depends on 1)

The method of claim 1, die separation of the field emitter substrate is performed using a laser machine tool to cut the substrate into a plurality of individual dies.

### Claim 46 (depends on 45)

The method of claim 45, wherein a protective coating comprises a photoresist or polymer layer and is deposited on the substrate surface prior to the laser dicing operation in order to protect the surface from re-deposited material and then removing said protective coating using an appropriate means of removing said protective coating material comprising a solvent immersion after the substrate has been diced into a plurality of individual dies.

### Claim 47 (depends on 10)

The method of claim 10, wherein dielectrics are oxides, nitrides or oxy-nitrides.

### Claim 48 (depends on 10)

The method of claim 10, wherein the metals are aluminum or platinum.

### Claim 49 (depends on 10)

The method of claim 10, wherein the polymers are photoresist or polyimide.

### Claim 50

A method of fabricating high-aspect ratio pillar or post structures having sloping sidewalls using Deep Reactive Ion Etching (DRIE) technology comprising the steps of:
selecting a first material substrate that is electrically conductive,
depositing onto the first material substrate a thin-film layer of second material layer,
patterning and etching said second material layer into a first predefined shape and dimensions, and
performing an etch into the first material substrate to a predefined depth to form a pillar or post shape structure.

### Claim 51 (depends on 50)

The method of claim 50, wherein the pillar or post structures are etched using a continuous etch recipe with O2, C4F8, and SF6 gasses, wherein the etch recipe matches the undercut requirements of lateral etch underneath the mask for a predefined design using a recipe wherein O2 flow is set within a range of between 30-100 sccm, C4F8 and SF6 flow rates are 5-20 sccm, and 75 sccm, respectively, and coil and platen powers are 800 W-2000 W and 10 W-40 W, respectively.