# US 2019/0337851 A1 · Preparation of inured asphalt blown coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2019/0337851 A1
- Document ID: US20190337851A1
- Status: Published application
- Kind: A1
- Application number: 16/392,839
- Filed: 2019-04-24
- Published: 2019-11-07
- Earliest claimed: 2018-05-02
- Assignees: Building Materials Investment Corporation
- Inventors: Denis Muki Tibah
- Web page: https://patentgrep.com/patent/US20190337851A1

## CPC

- C04B 26/26: Bituminous materials, e.g. tar, pitch {(C08L95/00 takes precedence)}
- B32B 5/16: characterised by features of a layer formed of particles, e.g. chips, powder {or granules (layer formed of natural mineral particles B32B19/00; layer being formed of wood fibres, chips or particles B32B21/02)}
- B32B 9/005: {comprising one layer of ceramic material, e.g. porcelain, ceramic tile (layered products with at least two ceramic layers composed mainly of ceramic B32B18/00)}
- B32B 11/04: comprising such {bituminous or tarry} substance as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a glass layer B32B17/06)}
- B32B 11/08: of metal
- C04B 24/2611: {Polyalkenes}
- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- D06N 5/003: {coated with bitumen}
- E04D 1/20: of plastics; {of asphalt;} of fibrous materials
- F16L 9/14: Compound tubes, i.e. made of materials not wholly covered by any one of the preceding groups (F16L9/16 - F16L9/22 take precedence)
- B32B 2255/26: Polymeric coating
- B32B 2307/712: Weather resistant
- B32B 2419/06: Roofs, roof membranes
- B32B 2439/40: Closed containers
- B32B 2597/00: Tubular articles, e.g. hoses, pipes
- C04B 2111/00525: {for metallic surfaces}
- C04B 2111/00586: {Roofing materials}
- C04B 2111/00612: {as one or more layers of a layered structure}
- C04B 2111/00706: {around pipelines or the like}
- E04D 2001/005: {the roofing elements having a granulated surface}
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- D06N: WALL, FLOOR, OR LIKE COVERING MATERIALS, e.g. LINOLEUM, OILCLOTH, ARTIFICIAL LEATHER, ROOFING FELT, CONSISTING OF A FIBROUS WEB COATED WITH A LAYER OF MACROMOLECULAR MATERIAL; FLEXIBLE SHEET MATERIAL NOT OTHERWISE PROVIDED FOR
- E04D: ROOF COVERINGS; SKY-LIGHTS; GUTTERS; ROOF-WORKING TOOLS (coverings of outer walls by plaster or other porous material E04F13/00)
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention relates to a method for preparing a flexible and tough polymer modified asphalt composition which comprises sparging an oxygen containing gas through a liquid high-vinyl polybutadiene modified asphalt, wherein the liquid high-vinyl polybutadiene modified asphalt contains from about 0.25 weight percent to about 20 weight percent of the liquid high-vinyl polybutadiene, wherein the oxygen containing gas is sparged through the liquid high-vinyl polybutadiene modified asphalt at a temperature within the range of about 400° F. to about 550° F. for a period of time which is sufficient to increase the softening point of the asphalt to a value which is within the range of 185° F. to 250° F. and to attain a penetration value of at least 15 dmm to produce the polymer modified asphalt composition.

## Claims

### Claim 1

A liquid high-vinyl polybutadiene modified asphalt which is comprised of an asphalt and a liquid high-vinyl polybutadiene, wherein the liquid high-vinyl polybutadiene is present in the liquid high-vinyl polybutadiene modified asphalt at a level which is within the range of about 0.25 weight percent to about 20 weight percent, based upon the total weight of the liquid high-vinyl polybutadiene modified asphalt.

### Claim 2 (depends on 1)

The liquid high-vinyl polybutadiene modified asphalt as specified in claim 1 wherein the liquid high-vinyl polybutadiene has a number average molecular weight which is within the range of about 1000 to about 30,000.

### Claim 3 (depends on 1)

The liquid high-vinyl polybutadiene modified asphalt as specified in claim 1 wherein the liquid high-vinyl polybutadiene has a number average molecular weight which is within the range of about 1600 to about 3,000.

### Claim 4 (depends on 1)

The liquid high-vinyl polybutadiene modified asphalt as specified in claim 1 wherein the liquid high-vinyl polybutadiene has a vinyl microstructure content of at least 15%.

### Claim 5 (depends on 1)

The liquid high-vinyl polybutadiene modified asphalt as specified in claim 1 wherein the liquid high-vinyl polybutadiene has a vinyl microstructure content of at least 60%.

### Claim 6 (depends on 1)

The liquid high-vinyl polybutadiene modified asphalt as specified in claim 1 wherein the liquid high-vinyl polybutadiene has a vinyl microstructure content of at least 90%.

### Claim 7 (depends on 1)

The liquid high-vinyl polybutadiene modified asphalt as specified in claim 1 wherein the liquid high-vinyl polybutadiene is present in the liquid high-vinyl polybutadiene modified asphalt at a level which is within the range of about 0.5 weight percent to about 15 weight percent, based upon the total weight of the liquid high-vinyl polybutadiene modified asphalt.

### Claim 8 (depends on 1)

The liquid high-vinyl polybutadiene modified asphalt as specified in claim 1 wherein the liquid high-vinyl polybutadiene is present in the liquid high-vinyl polybutadiene modified asphalt at a level which is within the range of about 4 weight percent to about 8 weight percent, based upon the total weight of the liquid high-vinyl polybutadiene modified asphalt.

### Claim 9

A method for preparing a flexible and tough polymer modified asphalt composition which comprises sparging an oxygen containing gas through a liquid high-vinyl polybutadiene modified asphalt, wherein the liquid high-vinyl polybutadiene modified asphalt contains from about 0.25 weight percent to about 20 weight percent of the liquid high-vinyl polybutadiene, wherein the oxygen containing gas is sparged through the liquid high-vinyl polybutadiene modified asphalt at a temperature within the range of about 400° F. to about 550° F. for a period of time which is sufficient to increase the softening point of the asphalt to a value which is within the range of 185° F. to 250° F. and to attain a penetration value of at least 15 dmm to produce the flexible and tough polymer modified asphalt composition.

### Claim 10 (depends on 10)

The method as specified in claim 10 wherein the polymer modified asphalt composition has a softening point which is within the range of 190° F. to 220° F., and wherein the polymer modified asphalt composition has a penetration value which is within the range of 15 dmm to 25 dmm.

### Claim 11 (depends on 10)

The method as specified in claim 10 wherein the oxygen containing gas is sparged through the asphalt for a period of time which is within the range of 1 hour to 8 hours, wherein asphalt is further comprised of an air blowing catalyst.

### Claim 12 (depends on 9)

The method as specified in claim 9 wherein the asphalt would not be suitable for conversion into industrial asphalt by conventional techniques and/or wherein the time need to air blow the asphalt to attain industrial asphalt having required softness and penetration values as well as blow loss is reduced

### Claim 13 (depends on 1)

An asphalt roofing shingle which is comprised of a (1) base layer having an upper surface and a bottom surface, (2) an exposure layer which is situated above the upper surface of the base layer, and (3) a bottom layer which is situated under the bottom surface of the base layer, wherein the upper surface of the base layer is coated with the liquid high-vinyl polybutadiene modified asphalt specified in claim 1, wherein the liquid high-vinyl polybutadiene modified asphalt has a softening point which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm.

### Claim 14 (depends on 13)

The asphalt roofing shingle as specified in claim 13 wherein the weather resistant granules are selected from the group consisting of slate granules, schist granules, quartz granules, vitrified brick granules, stone granules, and ceramic granules.

### Claim 15 (depends on 13)

The asphalt roofing shingle as specified in claim 13 wherein bottom layer is comprised of material which is resistant to sticking and wherein the material which is resistant to sticking is selected from the group consisting of sand, talc and mica.

### Claim 16 (depends on 13)

The asphalt roofing shingle as specified in claim 13 wherein the asphalt roofing shingle is adapted for installation in cold weather environments.

### Claim 17 (depends on 1)

An asphalt roofing shingle which is comprised of a (1) base layer having an upper surface and an bottom surface, (2) an exposure layer which is situated above the upper surface of the base layer, and (3) a bottom layer which is situated under the bottom surface of the base layer, wherein the upper surface of the base layer is coated with the liquid high-vinyl polybutadiene modified asphalt composition of claim 1, wherein the liquid high-vinyl polybutadiene modified asphalt has a softening point which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm, and wherein the exposure layer is comprised of weather resistant granules which are adhered to the polymer modified asphalt composition.

### Claim 18 (depends on 1)

A metal pipe having a tube layer and a lumen, wherein the tube layer is coated with the polymer modified asphalt composition of claim 1, and wherein the liquid high-vinyl polybutadiene modified asphalt has a softening point which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm.

### Claim 19 (depends on 18)

The pipe of claim 18 wherein both the outer surface and the inner surface of the tube layer is coated with the liquid high-vinyl polybutadiene modified asphalt.

### Claim 20 (depends on 1)

A metal storage tank having an inner surface and an outer surface, wherein the inner surface of the storage tank is coated with the polymer modified asphalt composition of claim 1, and wherein the liquid high-vinyl polybutadiene modified asphalt has a softening point which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm.

### Claim 21

A method for preparing a polymer modified asphalt composition which comprises dispersing a liquid high-vinyl polybutadiene throughout a partially blown or fully blown asphalt, wherein the liquid high-vinyl polybutadiene is added at a level which is within the range of 0.25 weight percent to 20 weight percent, based upon the total weight of the polymer modified asphalt composition.

### Claim 22 (depends on 21)

The liquid high-vinyl polybutadiene modified asphalt of claim 21 which is further comprised of polyisobutylene.